# US 2013/0158143 A1 · Thermoplastic resin foam, method of producing the same, and light reflecting material using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0158143 A1
- Document ID: US20130158143A1
- Status: Published application
- Kind: A1
- Application number: 13/768,480
- Filed: 2013-02-15
- Published: 2013-06-20
- Earliest claimed: 2010-08-17
- Assignees: Furukawa Electric Co., Ltd.
- Inventors: Hideyuki IKEDA; Kojiro INAMORI
- Web page: https://patentgrep.com/patent/US20130158143A1

## CPC

- C08K 5/20: Carboxylic acid amides
- C08J 9/0028: {containing nitrogen}
- C08J 9/12: by a physical blowing agent
- C08K 5/0083: {Nucleating agents promoting the crystallisation of the polymer matrix}
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A thermoplastic resin foam, having a bubble with an average bubble diameter of 10 μm or less in the inside thereof, in which wherein the thermoplastic resin foam is prepared by using and foaming a thermoplastic resin composition containing 0.25 to 2.5 part(s) by mass of a melt-type crystallization nucleating agent (B), with respect to 100 parts by mass of an amorphous thermoplastic resin (A).

## Claims

### Claim 1

A thermoplastic resin foam, comprising a bubble with an average bubble diameter of 10 μm or less in the inside thereof,
wherein the thermoplastic resin foam is prepared by using and foaming a thermoplastic resin composition containing 0.25 to 2.5 part(s) by mass of a melt-type crystallization nucleating agent (B), with respect to 100 parts by mass of an amorphous thermoplastic resin (A).

### Claim 2 (depends on 1)

The thermoplastic resin foam according to claim 1,
wherein the melt-type crystallization nucleating agent (B) is a compound represented by the following formula (1):
R1—(CONHR2)a Formula (1)
wherein R1 represents a saturated or unsaturated aliphatic polycarboxylic acid residue having 2 to 30 carbon atoms, a saturated or unsaturated alicyclic polycarboxylic acid residue having 4 to 28 carbon atoms, or an aromatic polycarboxylic acid residue having 6 to 28 carbon atoms; R2 represents an alkyl group having 1 to 18 carbon atom(s), an alkenyl group having 2 to 18 carbon atoms, a cycloalkyl group or a cycloalkenyl group having 3 to 12 carbon atoms, a phenyl group, a naphthyl group, or an anthryl group; and a represents an integer from 2 to 6.

### Claim 3 (depends on 1)

The thermoplastic resin foam according to claim 1,
wherein the melt-type crystallization nucleating agent (B) is at least one selected from the group consisting of trimesic acid tris(t-butylamide), trimesic acid tricyclohexylamide, trimesic acid tri(2-methylcyclohexylamide), trimesic acid tri(4-methylcyclohexylamide), 1,4-cyclohexane dicarboxylic acid dianilide, 1,4-cyclohexanoic acid dicarboxylic acid dicyclohexylamide, 1,4-cyclohexanoic acid dicarboxylic acid dibenzylamide, 2,6-naphthalene dicarboxylic acid dicyclohexylamide, 1,2,3,4-butane tetracarboxylic acid tetracyclohexylamide and 1,2,3,4-buatne tetracarboxylic acid tetraanilide.

### Claim 4 (depends on 1)

The thermoplastic resin foam according to claim 1, wherein the thermoplastic resin foam satisfies V-0, V-1 or V-2 in the UL-94 vertical burning test.

### Claim 5 (depends on 1)

The thermoplastic resin foam according to claim 1, wherein the amorphous thermoplastic resin (A) is polycarbonate.

### Claim 6 (depends on 1)

A light reflecting material according to claim 1, being molded by using the amorphous thermoplastic resin foam.

### Claim 7

A method of producing a thermoplastic resin foam, comprising the steps of:
preparing a thermoplastic resin composition by melt-dispersing 0.25 to 2.5 part(s) by mass of a melt-type crystallization nucleating agent, with respect to 100 parts by mass of an amorphous thermoplastic resin;
depositing the melt-type crystallization nucleating agent by solidifying the composition followed by impregnating an inert gas to the composition under pressure; and
foaming the composition impregnated with the inert gas by heating at a temperature of a glass transition temperature of the amorphous thermoplastic resin or more under a released pressure.