# US 2013/0157864 A1 · Low temperature resistor for superconductor circuits

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157864 A1
- Document ID: US20130157864A1
- Status: Published application
- Kind: A1
- Application number: 13/330,270
- Filed: 2011-12-19
- Published: 2013-06-20
- Earliest claimed: 2011-12-19
- Assignees: Northrup Grumman Systems Corporation
- Inventors: John J. Talvacchio; Erica C. Folk; Sean R. McLaughlin; David J. Phillips
- Web page: https://patentgrep.com/patent/US20130157864A1

## CPC

- H10N 69/00: Integrated devices, or assemblies of multiple devices, comprising at least one superconducting element covered by group H10N60/00
- H01C 7/006: {Thin film resistors}
- H01C 13/00: Resistors not provided for elsewhere
- H10N 60/00: Superconducting devices (integrated devices or assemblies of multiple devices H10N69/00)
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H01C: RESISTORS

## Abstract

A integrated circuit and methods for fabricating the circuit are provided. The circuit integrates at least one circuit element formed from a material that is superconducting at temperatures less than one hundred milliKelvin and at least one resistor connected to the circuit element. The resistor is formed from an alloy of transition metals that is resistive at temperatures less than one hundred milliKelvin.

## Claims

### Claim 1

An integrated circuit comprising:
a circuit element formed from a material that is superconducting at temperatures less than one hundred milliKelvin; and
a resistor connected to the circuit element, the resistor being formed from an alloy of transition metals that is resistive at temperatures less than one hundred milliKelvin.

### Claim 2 (depends on 1)

The integrated circuit of claim 1, an atomic ratio of the transition metals comprising the alloy being selected such that a ratio of the number of valance electrons to atoms within the alloy is between about 5.35 and about 5.95.

### Claim 3 (depends on 1)

The integrated circuit of claim 1, wherein the transition metals comprising the alloy are selected as at least two of titanium, vanadium, zirconium, niobium, molybdenum, hafnium, tungsten, tantalum, and rhenium.

### Claim 4 (depends on 3)

The integrated circuit of claim 3, wherein the alloy is an alloy of titanium and tungsten.

### Claim 5 (depends on 4)

The integrated circuit of claim 4, wherein the alloy comprises an atomic ratio of approximately five atoms of tungsten to each atom of titanium.

### Claim 6 (depends on 4)

The integrated circuit of claim 4, wherein the resistor is implemented as a thin film of the alloy.

### Claim 7

A method for creating a superconducting circuit comprising:
depositing a first layer of material that is superconducting at temperatures less than one hundred milliKelvin on an insulating substrate; and
depositing a second layer of material comprising an alloy of transition metals, the alloy comprising at least two of titanium, vanadium, zirconium, niobium, molybdenum, hafnium, tungsten, tantalum, and rhenium, that remains resistive at temperatures less than one hundred milliKelvin, the second layer of material being in contact with the first layer of material.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first layer of material is deposited prior to the second layer of material.

### Claim 9 (depends on 7)

The method of claim 7, wherein the second layer of material is deposited prior to the first layer of material.

### Claim 10 (depends on 7)

The method of claim 7, an atomic ratio of the transition metals comprising the alloy being selected such that a ratio of the number of valance electrons to atoms within the alloy is between about 5.35 and about 5.95.

### Claim 11 (depends on 7)

The method of claim 7, wherein the alloy of transition metals is an alloy of titanium and tungsten having an atomic ratio of approximately five atoms of tungsten to each atom of titanium.

### Claim 12 (depends on 7)

The method of claim 7, further comprising depositing the second layer of material via a sputtering process performed at room temperature in argon gas.

### Claim 13 (depends on 7)

The method of claim 7, further comprising etching the second layer of material via a reactive ion etching process with fluorine-based gases.

### Claim 14 (depends on 7)

The method of claim 7, further comprising depositing a layer of an insulator material over the first and second layers of material.

### Claim 15 (depends on 7)

The method of claim 7, wherein the insulating substrate is a silicon wafer.

### Claim 16

An integrated circuit comprising:
a circuit element formed from a superconducting material; and
a resistor connected to the circuit element, the resistor being formed from an alloy of transition metals having an atomic ratio selected such that a ratio of the number of valance electrons to atoms within the alloy is between about 5.35 and about 5.95.

### Claim 17 (depends on 16)

The integrated circuit of claim 16, wherein the transition metals comprising the alloy are selected as at least two of titanium, vanadium, zirconium, niobium, molybdenum, hafnium, tungsten, tantalum, and rhenium.

### Claim 18 (depends on 17)

The integrated circuit of claim 17, wherein the alloy is an alloy of titanium and tungsten.

### Claim 19 (depends on 18)

The integrated circuit of claim 18, wherein the alloy comprises an atomic ratio of approximately five atoms of tungsten to each atom of titanium.

### Claim 20 (depends on 16)

The integrated circuit of claim 16, wherein the integrated circuit is configured for operation at temperatures less than one hundred milliKelvin, such that the integrated material has substantially no resistance at temperatures less than one hundred milliKelvin and the alloy of transition metals is resistive at temperatures less than one hundred milliKelvin.