# US 2013/0157842 A1 · Unsupported and supported promoted ruthenium sulfide catalyst with high catalytic activity for hydrocarbon hydrotreatments and its method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157842 A1
- Document ID: US20130157842A1
- Status: Published application
- Kind: A1
- Application number: 13/444,534
- Filed: 2012-04-11
- Published: 2013-06-20
- Earliest claimed: 2011-12-14
- Assignees: Centro de Investigacion en Materiales Avanzados, S.C.
- Inventors: Carlos Elias Ornelas Gutierrez; Lorena Alvarez Contreras; Jose Rurik Farias Mancilla; Alfredo Aguilar Elguezabal
- Web page: https://patentgrep.com/patent/US20130157842A1

## CPC

- B01J 27/045: Platinum group metals
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 37/0201: {Impregnation}
- B01J 37/031: {Precipitation}
- B01J 37/18: with gases containing free hydrogen
- B01J 37/20: Sulfiding
- C10G 45/10: containing platinum group metals or compounds thereof
- B01J 2235/15: X-ray diffraction
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

The present invention relates to synthesis method of a family of ruthenium sulfide catalysts promoted with an added additional metal, unsupported (M/RuS2) and supported (M/RuS2/support). The obtained catalysts exhibit a high catalytic activity in hydrotreating or hydroprocessing (HDT) of hydrocarbons, mainly hydrodesulfuration, hydrodenitrogenation, and hydrodeoxigenation. The impact of the present invention for application in the commercial context, lies in the high catalytic activity of the obtained catalysts, which is far superior to the existing commercial catalysts, as well as the simplicity of the synthesis method, which will affect the quality of the products obtained in the oil industry, allowing to meet the environmental standards imposed by current legislations.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A synthesis method for a ruthenium sulfide (RuS2) promoted with an additional metal to obtain a family of ruthenium precursory complex to obtain ruthenium sulfide catalysts comprising the steps of:
a) dissolving hydrated ruthenium chloride in a solution of R1COR2, R2-OH, C4H8O (THF), C4H8O2, CH2Cl2 (DCM), C2H3N (MeCN), C3H7ON (DMF), C2H6SO (DMSO) or a combination thereof;
wherein:
R1 is equal to OH or a lineal chain or branched radical C1 to C8,
R2 is equal to H, a lineal chain or branched radical C1 to C8, with relation 0.01 to 40 ml of solvent per gram of salt preferably dissolved in methanol, ethanol or acetone;
b) dissolving ammonium chloride in solution of R1COR2, R2-OH, C4H8O (THF), C4H8O2, CH2Cl2 (DCM), C2H3N (MeCN), C3H7ON (DMF), C2H6SO (DMSO) or a combination thereof;
wherein:
R1 is equal to OH, a lineal chain or branched radical C1 to C8,
R2 is equal to H or to a lineal chain or branched radical C1 to C8, with relation 0.01 to 40 ml of solvent per gram of salt preferably dissolved in water, methanol, ethanol, acetone or one combination thereof;
c) dissolving an inorganic salt of transition metals of groups VIB or VIIIB with a ratio of the transition metal to the ruthenium from 0.01 to 3, in solution of R1COR2, R2-OH, C4H8O (THF), C4H8O2, CH2Cl2 (DCM), C2H3N (MeCN), C3H7ON (DMF), C2H6SO (DMSO) or a combination thereof,
wherein:
R1 is equal to OH or to a lineal or branched radical C1 to C8 and
R2 is equal to H or to a radical of straight-chain or branched C1 to C8, with relation 0.01 to 40 ml of solvent per gram of salt, preferably dissolved in water, methanol, ethanol, acetone, or a combination;
d) adding the solution of b) in a molar relation of 1:1 to 10:1 of NH4Cl to the ruthenium chloride solution to the solution of a), keeping in mechanical agitation between 100 to 700 rpm during the addition and up to 30 minutes after the addition has finished;
e) adding NH4OH or HCl in proportion of 0.01 to 2 ml per gram of ruthenium chloride;
f) adding to the solution of step d) or e) a R3COR4 or R3COOR5 compound,
wherein:
R3 is a linear chain or branched radical C1 to C8,
R4 is equal to H or a linear chain or branched radical C1 to C8 and include 1 or 2 oxygen atoms or 1 nitrogen atom,
R5 is equal to a hydrogen radical or a linear chain or branched radical C1 to C10;
g) leaving to the solution of f) in mechanical agitation for 30 minutes between 100-700 rpm and resting time from 0.1 to 3 hours to allow crystallization; a family of promoted ruthenium complex compounds very soluble in water and sparingly soluble in acetone is produced and precipitated, the family of ruthenium complex compounds have decomposition temperatures above 200° C. and total decomposition to metallic charge (MW/Ru) in inert atmosphere to temperatures lower than 485° C., filtering and washing with acetone the precipitate;
h) incorporating the ruthenium complex to a support by using a method selected from an incipient impregnating method or a wet impregnating method,
wherein a support bed includes: TiO2, zeolitic, and mesostructured supports selected from MCM-41, SBA-15, alumina, silice, mixed oxides, or a combination thereof; doped or not doped, including the nanometric form of the same;
wherein the support bed is impregnated with a solution of the precursory complex in weight relation 1-90% of dissolved metallic charge in the minimum amount of solvent,
wherein during the impregnation, the solution of the ruthenium complex compounds is dripped over the catalyst until filling all porosity, by incipient impregnation or moistening the catalyst, wet impregnation;
i) decomposing and activating the ruthenium precursor complex at temperatures between 350° C. to 550° C. with a heating rate from 2 to 50° C. per minute; under pressure of 1 atm, in a reducing atmosphere of a gas mixture formed by H2S/G where G may be H2, N2, Ar or He; in H25 concentrations from 2 to 99%.

### Claim 16 (depends on 15)

The synthesis method according to claim 15, wherein the promoter is incorporated by an impregnation method to the unsupported or supported ruthenium sulfide catalyst by dripping of the solution of step c) over the catalyst until filling all the porous or wetting the catalyst, wherein after the impregnation, the catalyst is activated again following step i).

### Claim 17 (depends on 15)

The synthesis method according to claim 15, wherein the promoter is incorporated by using a method of co-synthesis 1, the method of co-synthesis 1 includes forming a bimetallic complex precursor and activating the bimetallic complex precursor by adding the solution of step c) to the solution of step a) keeping mechanical agitation between 100 to 700 rpm during the addition and follows by the step d) replacing the solution of step a) with the mixture of the solution of step c) and the solution of step a).

### Claim 18 (depends on 15)

The synthesis method according to claim 15, wherein the promoter is incorporated by using a method of co-synthesis 2, the method of co-synthesis 2 includes forming a bimetallic complex precursor and activating the bimetallic complex precursor by adding the solution of step c) to the solution of step b) keeping mechanical agitation between 100 to 700 rpm during the addition and follows by the step d) replacing the solution of step b) with the mixture of the solutions of step c) and the solution of step b).

### Claim 19 (depends on 15)

The synthesis method according to claim 15, wherein the promoter is incorporated by using a method of co-synthesis 3, the method of co-synthesis 3 includes forming a bimetallic complex precursor and activating the bimetallic complex precursor by adding the solution of step c) to the ruthenium complex precursor forming in step g), wherein the ruthenium complex precursor formed in the step g) is dissolved in a solvent R1COR2, R2-OH, C4H8OR (THF), C4H8O2, CH2Cl2 (DMC), C2H3N (MeCN), C3H7ON (DMF), C2H6SO (DMSO) or a combination thereof;
wherein:
R1 is equal to OH, or to a radical of lineal or branched chain C1 to C8 and
R2 is equal to H, or to a radical of lineal or branched chain C1 to C8, with relation 0.01 to 40 ml of solvent per gram of salt, preferably dissolved in water, methanol, ethanol, acetone, or a combination thereof;
wherein the bimetallic complex follows the procedure of the step h) to supported catalysts and the step i) for unsupported or supported catalyst.

### Claim 20 (depends on 15)

The synthesis method according to claim 15, wherein the step g) is carried out according to the following equation:
MClY+RuCl3+NH4Cl→MW/RuNX+H4xCl3+ZH2S→MW/RuS2

### Claim 21 (depends on 16)

The synthesis method according to claim 16, wherein the method is carried out according to the following equation:

### Claim 22 (depends on 17)

The synthesis method according to claim 17, wherein the method is carried out according to the following equation:
(MClY+RuCl3)+NH4Cl→MW/RuNXH4xCl3+Z+H2S→MW/RuS2

### Claim 23 (depends on 18)

The synthesis method according to claim 18, wherein the method is carried out according to the following equation:
RuCl3+(MClY+NH4Cl)→MW/RuNXH4xCl3+Z+H2S→MW/RuS2

### Claim 24 (depends on 19)

The synthesis method according to claim 19, wherein the method is carried out according to the following equation:

### Claim 25 (depends on 15)

The synthesis method according to claim 15, wherein the family of ruthenium precursory complexes have the formula:
MW/RuNXH4xCl3+Z
wherein:
M is one or more transitional metals of group VIB or VIIIB,
X and Z have values from 0 to 10 and
W has values from 0.01 to 3 or value of 0 for promotion by impregnation.

### Claim 26 (depends on 15)

The synthesis method according to claim 15, wherein the method provides unsupported promoted catalysts having an active component MW/RuS2 and supported catalyst having as an active ingredient MW/RuS2.

### Claim 27 (depends on 15)

The synthesis method according to claim 15, wherein the unsupported catalysts include a surface area of 40 to 250 m2/g and a high number of active sites.

### Claim 28 (depends on 15)

The synthesis method according to claim 15, wherein the ruthenium sulfide precursor is decomposed and activated by the step i).

### Claim 29 (depends on 15)

The synthesis method according to claim 15, wherein the catalyst is incorporated to the support after the step h) by an impregnation method.

### Claim 30 (depends on 15)

The synthesis method according to claim 15, wherein, the catalysts are used in reactions of hydrotreating, hydroprocessing (HDT) of hydrocarbons, hydrodesulfuration, hydrodenitrogenation, or hydrodeoxigenation.

### Claim 31 (depends on 15)

A family of ruthenium sulfide catalyst obtained by the method of claim 15, including unsupported and supported catalysts.

### Claim 32 (depends on 31)

The family of ruthenium sulfide catalyst according to claim 31, wherein the catalysts are used in reactions of hydrotreating or hydroprocessing (HDT) of hydrocarbons, hydrodesulfuration, hydrodenitrogenation, or hydrodeoxigenation.