# US 2013/0157835 A1 · Boron carbide-containing ceramic bonded body and method for producing the bonded body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157835 A1
- Document ID: US20130157835A1
- Status: Published application
- Kind: A1
- Application number: 13/819,651
- Filed: 2011-08-30
- Published: 2013-06-20
- Earliest claimed: 2010-08-31
- Assignees: Mino Ceramic Co., Ltd.
- Inventors: Kiyoto Sekine; Takeshi Kumazawa; Hideki Kita; Hideki Hyuga
- Web page: https://patentgrep.com/patent/US20130157835A1

## CPC

- B23K 1/19: taking account of the properties of the materials to be soldered
- C04B 35/563: based on boron carbide
- C04B 37/005: {consisting of glass or ceramic material}
- C04B 37/006: {consisting of metals or metal salts}
- C04B 2237/064: based on alumina or aluminates
- C04B 2237/068: based on refractory oxides, e.g. zirconia
- C04B 2237/121: based on aluminium
- C04B 2237/122: based on refractory metals
- C04B 2237/124: based on copper
- C04B 2237/125: based on noble metals, e.g. silver
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A bonded, boron carbide-containing ceramic body includes ceramic members. These ceramic members each contain boron carbide at 2 mass % or higher, and are integrated together via a bonding layer bonded with a bonding material containing at least one metal selected from the group consisting of aluminum, copper, gold and zirconium or integrated together via a bonding layer formed from one of aluminum metal and an aluminum compound and a titanium compound as bonding materials, wherein a bonded part has a strength of 100 MPa or higher. According to this technology, the boron carbide-containing ceramic members can be bonded together with a high strength of 100 MPa or more by a simple process, and further, the bonding is feasible with excellent chemical resistance at the bonded part as needed.

## Claims

### Claim 1

A bonded, boron carbide-containing ceramic body comprising ceramic members each containing boron carbide at 60 mass % or higher and integrated together via a bonding layer bonded with a bonding material containing at least one metal selected from the group consisting of aluminum, copper, gold and zirconium or integrated together via a bonding layer formed from one of aluminum metal and an aluminum compound and a titanium compound as bonding materials, wherein a bonded part has a strength of 100 MPa or higher.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The bonded, boron carbide-containing ceramic body according to claim 1, wherein the bonding layer has a thickness of 1 to 1,000 μm.

### Claim 4 (depends on 1)

A process for producing the bonded, boron carbide-containing ceramic body according to claim 1, comprising, upon bonding together ceramic members each containing boron carbide at 60 mass % or higher, interposing a bonding material, which is selected from a foil, paste or vapor deposition layer comprised of a metal of aluminum, copper, gold or zirconium or an alloy of the metal as a base, between parts of the ceramic members, said parts being to be bonded together, such that the bonding material has a thickness in a range of not greater than 1,000 μm, and while holding the ceramic members and bonding material as they are, heating both the ceramic members at least at the parts to be bonded together at a temperature of 600° C. or higher but 1,600° C. or lower in air, under vacuum conditions or in an inert atmosphere.

### Claim 5 (depends on 1)

A process for producing the bonded, boron carbide-containing ceramic body according to claim 1, comprising, upon bonding together ceramic members each containing boron carbide at 60 mass % or higher, applying a slurry-form or paste-form titanium compound in a form of a sheet to parts of the ceramic members, said parts being to be bonded together, to interpose the sheet with a thickness in a range of not greater than 1,000 μm, holding the ceramic members in close contact with the sheet being interposed therebetween, arranging a bonding material containing a powder of aluminum metal or a powder of an aluminum compound over the parts to be bonded together, and conducting heating at a temperature of 600° C. or higher but lower than 1,200° C. under vacuum conditions or in an inert atmosphere such that the aluminum or aluminum compound is allowed to infiltrate into the parts to be bonded together.

### Claim 6 (depends on 3)

A process for producing the bonded, boron carbide-containing ceramic body according to claim 3, comprising, upon bonding together ceramic members each containing boron carbide at 60 mass % or higher, interposing a bonding material, which is selected from a foil, paste or vapor deposition layer comprised of a metal of aluminum, copper, gold or zirconium or an alloy of the metal as a base, between parts of the ceramic members, said parts being to be bonded together, such that the bonding material has a thickness in a range of not greater than 1,000 μm, and while holding the ceramic members and bonding material as they are, heating both the ceramic members at least at the parts to be bonded together at a temperature of 600° C. or higher but 1,600° C. or lower in air, under vacuum conditions or in an inert atmosphere.

### Claim 7 (depends on 3)

A process for producing the bonded, boron carbide-containing ceramic body according to claim 3, comprising, upon bonding together ceramic members each containing boron carbide at 60 mass % or higher, applying a slurry-form or paste-form titanium compound in a form of a sheet to parts of the ceramic members, said parts being to be bonded together, to interpose the sheet with a thickness in a range of not greater than 1,000 μm, holding the ceramic members in close contact with the sheet being interposed therebetween, arranging a bonding material containing a powder of aluminum metal or a powder of an aluminum compound over the parts to be bonded together, and conducting heating at a temperature of 600° C. or higher but lower than 1,200° C. under vacuum conditions or in an inert atmosphere such that the aluminum or aluminum compound is allowed to infiltrate into the parts to be bonded together.