# US 2013/0157551 A1 · Polishing cloth and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157551 A1
- Document ID: US20130157551A1
- Status: Published application
- Kind: A1
- Application number: 13/819,104
- Filed: 2011-08-18
- Published: 2013-06-20
- Earliest claimed: 2010-08-31
- Assignees: Toray Industries, Inc.
- Inventors: Masanori Endo; Hajime Nishimura; Satoshi Yanagisawa; Yukihiro Matsuzaki
- Web page: https://patentgrep.com/patent/US20130157551A1

## CPC

- B24D 11/00: Constructional features of flexible abrasive materials; Special features in the manufacture of such materials
- G11B 5/8404: {manufacturing base layers}
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)

## Abstract

A high performance polishing cloth having a densified surface state with ultrafine fiber bundles uniformly dispersed therein and having excellent smoothness is provided. The polishing cloth comprises a nonwoven fabric formed by entangling the ultrafine fiber bundles formed by bundling ultrafine fibers with an average single fiber diameter of 0.05 to 2.0 μm and a polymeric elastic material, wherein the average size of the surface fiber-napped portions constituted by the aforementioned ultrafine fiber bundles of the aforementioned nonwoven fabric in the width direction of the ultrafine fiber bundles is 50 to 180 μM.

## Claims

### Claim 1

A polishing cloth mainly comprising a nonwoven fabric formed by entangling the ultrafine fiber bundles including ultrafine fibers with an average single fiber diameter of 0.05 to 2.0 μm and a polymeric elastic material, wherein the average size of the surface fiber-napped portions constituted by the aforementioned ultrafine fiber bundles of the aforementioned nonwoven fabric in the width direction of the ultrafine fiber bundles is 50 to 180 μm.

### Claim 2 (depends on 1)

A polishing cloth, according to claim 1, wherein the average size of the surface fiber-napped portions in the width direction of the ultrafine fiber bundles is 50 to 120 μm.

### Claim 3 (depends on 1, 2)

A polishing cloth, according to claim 1 or 2, wherein the surface roughness of the polishing cloth is 5 to 18 μm.

### Claim 4 (depends on 1)

A polishing cloth, according to claim 1, wherein the CV of the ultrafine fiber is 1 to 30%.

### Claim 5

A method for producing a polishing cloth comprising at least the following steps (1) through (5) in combination, wherein the number of islands-in-sea type composite fibers convertible into ultrafine fibers, which can be brought in by needle punching of the following step (2), is 3 to 6 fibers/1 barb:
(1) producing islands-in-sea type composite fibers convertible into ultrafine fibers with an average single fiber diameter of 0.05 to 2.0 μm;
(2) laminating fiber webs by a card and a crosslapper using said islands-in-sea type composite fibers, and obtaining a nonwoven fabric by needle punching;
(3) giving a polymeric elastic material to said nonwoven fabric by 10 to 200 mass % based on the mass of the ultrafine fibers obtained by converting the composite fibers;
(4) buffing at least one surface; and
(5) converting said islands-in-sea type composite fibers into ultrafine fibers.

### Claim 6 (depends on 5)

A method for producing a polishing cloth, according to claim 5, wherein the number of islands-in-sea type composite fibers brought in by needle punching is 3 to 4 fibers/1 barb.