# US 2013/0157466 A1 · Silicon nitride films for semiconductor device applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157466 A1
- Document ID: US20130157466A1
- Status: Published application
- Kind: A1
- Application number: 13/766,696
- Filed: 2013-02-13
- Published: 2013-06-20
- Earliest claimed: 2010-03-25
- Inventors: Keith Fox; Dong Niu; Joseph L. Womack; Mandyam Sriram; George Andrew Antonelli; Bart J. van Schravendijk; Jennifer O'Loughlin
- Web page: https://patentgrep.com/patent/US20130157466A1

## CPC

- H10P 50/642: {Chemical etching}
- C23C 16/24: Deposition of silicon only
- C23C 16/345: {Silicon nitride}
- C23C 16/402: {Silicon dioxide}
- C23C 16/4401: {Means for minimising impurities, e.g. dust, moisture or residual gas, in the reaction chamber}
- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/509: using internal electrodes
- C23C 16/54: Apparatus specially adapted for continuous coating
- H01J 37/32082: {Radio frequency generated discharge (H01J37/32357, H01J37/32366, H01J37/32394 and H01J37/32403 take precedence)}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 50/283: {by chemical means}
- H10P 72/0462: {characterised by the construction of the processing chambers, e.g. modular processing chambers}
- H10P 72/0466: {characterised by the construction of the load-lock chamber}
- H10P 72/0468: {comprising a chamber adapted to a particular process}
- H01J 2237/3321: CVD [Chemical Vapor Deposition]
- H10D 1/68: Capacitors having no potential barriers
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The embodiments herein relate to plasma-enhanced chemical vapor deposition methods and apparatus for depositing silicon nitride on a substrate. The disclosed methods provide silicon nitride films having wet etch rates (e.g., in dilute hydrofluoric acid or hot phosphoric acid) suitable for certain applications such as vertical memory devices. Further, the methods provide silicon nitride films having defined levels of internal stress suitable for the applications in question. These silicon nitride film characteristics can be set or tuned by controlling, for example, the composition and flow rates of the precursors, as well as the RF power supplied to the plasma and the pressure in the reactor. In certain embodiments, a boron-containing precursor is added.

## Claims

### Claim 1

A method for forming a silicon nitride film on a substrate in a plasma-enhanced chemical vapor deposition apparatus, the method comprising:
flowing a silicon-containing reactant, a nitrogen-containing reactant, and a boron-containing reactant through the plasma-enhanced chemical vapor deposition apparatus containing the substrate, wherein the flowing is conducted such that the ratio of flow rates of the silicon-containing reactant to the nitrogen-containing reactant is about 0.02 or less;
generating or maintaining a plasma in the plasma-enhanced chemical vapor deposition apparatus; and
depositing the silicon nitride film on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the silicon-containing reactant is selected from the group consisting of silane, disilane, trisilane or an alkyl silane.

### Claim 3 (depends on 1)

The method of claim 1, wherein the nitrogen-containing reactant is selected from the group consisting of ammonia, hydrazine or nitrogen.

### Claim 4 (depends on 1)

The method of claim 1, wherein the boron-containing reactant is selected from the group consisting of diborane and trimethyl borate.

### Claim 5 (depends on 4)

The method of claim 4, wherein the flowing is conducted by flowing diborane at a rate of about 4 to 15 sccm.

### Claim 6 (depends on 4)

The method of claim 4, wherein the silicon-containing reactant is silane and the boron-containing reactant is diborane, and wherein the flowing is conducted such that the ratio of flow rates of the silane to diborane is about 3 to 20.

### Claim 7 (depends on 6)

The method of claim 6, further comprising flowing diborane to the apparatus in an inert gas carrier.

### Claim 8 (depends on 1)

The method of claim 1, wherein the flowing is conducted with the addition of a flowing inert gas.

### Claim 9 (depends on 8)

The method of claim 8, wherein the inert gas is nitrogen.

### Claim 10 (depends on 1)

The method of claim 1, wherein the generating and maintaining the plasma is conducted using low frequency and high frequency power and wherein the low frequency power is provided at about 0 to 300 Watts per 300 mm wafer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the low frequency power is provided at or below about 75 Watts per 300 mm wafer.

### Claim 12 (depends on 10)

The method of claim 10, wherein the high frequency power is provided at about 100 to 750 Watts per 300 mm wafer.

### Claim 13 (depends on 1)

The method of claim 1, wherein the pressure in the apparatus is maintained between about 0.5 and 8 Torr while depositing the silicon nitride film on the substrate.

### Claim 14 (depends on 1)

The method of claim 1, wherein the depositing deposits the silicon nitride film on the substrate to a thickness of between about 10 and 100 nm.

### Claim 15 (depends on 1)

The method of claim 1, wherein the silicon nitride film etches at a rate of at least about 20 Ångstroms per minute when exposed to aqueous hydrofluoric acid provided in a volume ratio of 100 units of water to 1 unit standard 50% hydrofluoric acid at 20° C.

### Claim 16 (depends on 1)

The method of claim 1, further comprising:
selecting an amount of internal stress for the silicon nitride film; and
selecting process parameters for depositing the silicon nitride film with the amount of internal stress.

### Claim 17 (depends on 1)

The method of claim 1, wherein the depositing is conducted under conditions that produce the silicon nitride film with tensile internal stress.

### Claim 18 (depends on 17)

The method of claim 17, wherein tensile internal stress is between about 400 and 600 MPa.

### Claim 19 (depends on 1)

The method of claim 1, wherein the silicon nitride film comprises between about 1 and 15 atomic percent boron.

### Claim 20 (depends on 1)

The method of claim 1, wherein the silicon nitride film has an average roughness of less than about 6 Å as measured on the substrate.

### Claim 21 (depends on 20)

The method of claim 20, wherein the silicon nitride film has an average roughness of less than about 4.5 Å as measured on the substrate.

### Claim 22 (depends on 1)

The method of claim 1, further comprising heating the substrate with deposited silicon nitride film to a temperature of at least about 400° C.

### Claim 23 (depends on 1)

The method of claim 1, further comprising forming a stack comprising alternating layers of an oxide and the deposited silicon nitride film.

### Claim 24 (depends on 23)

The method of claim 23, wherein the stack contains at least about 10 layers of the silicon nitride film.

### Claim 25 (depends on 24)

The method of claim 24, wherein the stack contains at least about 50 layers of the silicon nitride film.

### Claim 26 (depends on 23)

The method of claim 23, further comprising wet etching silicon nitride layers from the stack to form a fishbone shaped structure having recesses.

### Claim 27 (depends on 26)

The method of claim 26, further comprising forming a vertical memory device using the fishbone shaped structure.

### Claim 28 (depends on 26)

The method of claim 26, further comprising forming capacitors at least partially in the recesses formed by wet etching silicon nitride.

### Claim 29

A method for forming a film stack including a silicon nitride film and a second film on a substrate, the silicon nitride film having a different material composition from the second film, the method comprising:
(a) depositing the silicon nitride film on the substrate by plasma-enhanced chemical vapor deposition while flowing a silicon-containing reactant, a nitrogen-containing reactant, and a boron-containing reactant through the plasma-enhanced chemical vapor deposition apparatus containing the substrate, wherein the silicon nitride film has a thickness of between about 10 and 100 nm;
(b) depositing the second film on the silicon nitride film, wherein the second film has a thickness of between about 10 and 100 nm; and
(c) repeating (a) and (b) at least twice to form the film stack.

### Claim 30 (depends on 29)

The method of claim 29, wherein depositing the silicon nitride film is conducted such that the ratio of flow rates of the silicon-containing reactant to the nitrogen-containing reactant is about 0.02 or less.

### Claim 31 (depends on 29)

The method of claim 29, wherein the second film is a silicon oxide film.

### Claim 32 (depends on 31)

The method of claim 31, wherein the silicon oxide film is formed by a thermal process.

### Claim 33 (depends on 31)

The method of claim 31, wherein (c) comprises repeating (a) and (b) at least 10 times to form the film stack.

### Claim 34 (depends on 33)

The method of claim 33, further comprising wet etching the silicon nitride film from the stack to form a fishbone shaped structure having recesses.

### Claim 35 (depends on 34)

The method of claim 34, further comprising forming a vertical memory device using the fishbone shaped structure.

### Claim 36 (depends on 34)

The method of claim 34, further comprising forming capacitors at least partially in the recesses formed by wet etching silicon nitride.

### Claim 37 (depends on 29)

The method of claim 29, further comprising:
applying photoresist to the substrate;
exposing the photoresist to light;
patterning the resist with a pattern and transferring the pattern to the substrate; and
selectively removing the photoresist from the substrate.

### Claim 38

A plasma-enhanced chemical vapor deposition apparatus configured to deposit a film stack on a substrate, the apparatus comprising:
a process station;
a first reactant feed for supplying a silicon-containing reactant to the process station;
a second reactant feed for supplying a co-reactant to the process station;
a plasma source; and
a controller configured to control the apparatus to maintain a plasma and process gas flow conditions, the controller comprising instructions for
(a) depositing a silicon nitride film on the substrate by plasma-enhanced chemical vapor deposition while flowing the silicon-containing reactant, a nitrogen-containing reactant, and a boron-containing reactant through the plasma-enhanced chemical vapor deposition apparatus containing the substrate, wherein the silicon nitride film has a thickness of between about 10 and 100 nm; and
(b) depositing the second film on the silicon nitride film, wherein the second film has a thickness of between about 10 and 100 nm.

### Claim 39 (depends on 38)

The apparatus of claim 38, wherein the controller further comprises instructions for (c) repeating (a) and (b) at least twice to form the film stack.

### Claim 40 (depends on 39)

The apparatus of claim 39, wherein the instructions for (c) comprise instructions for repeating (a) and (b) at least 10 times to form the film stack.

### Claim 41 (depends on 38)

The apparatus of claim 38, wherein the plasma source is a capacitively-coupled plasma source.

### Claim 42 (depends on 38)

The apparatus of claim 38, wherein the controller instructions for depositing the silicon nitride film on the substrate comprise instructions for providing a ratio of flow rates of the silicon-containing reactant to the nitrogen-containing reactant is about 0.02 or less.

### Claim 43 (depends on 38)

The apparatus of claim 38, wherein the second film is a silicon oxide film.

### Claim 44 (depends on 43)

The apparatus of claim 43, wherein the controller instructions for depositing the silicon oxide film on the substrate comprise instructions for forming the silicon oxide film by a thermal process.

### Claim 45 (depends on 38)

The apparatus of claim 38, wherein the boron-containing reactant is diborane and the controller is configured to flow the diborane into the process station at a rate of about 4 to 15 sccm.

### Claim 46 (depends on 38)

The apparatus of claim 38, wherein the boron-containing reactant is diborane, wherein the silicon-containing reactant is silane, and wherein controller is configured to flow the silane and diborane at a ratio of flow rates of the silane to diborane of about 3 to 20.

### Claim 47 (depends on 38)

The apparatus of claim 38, wherein the controller further comprises instructions for generating and maintaining a plasma using the plasma source.

### Claim 48 (depends on 47)

The apparatus of claim 47, wherein the instructions for generating and maintaining a plasma comprise instructions for generating low frequency and high frequency power and with the low frequency power provided at or below about 150 Watts per 300 mm wafer.

### Claim 49 (depends on 48)

The apparatus of claim 48, wherein instructions for generating low frequency and high frequency power comprise instructions for generating the high frequency power at about 100 to 750 Watts per 300 mm wafer.

### Claim 50 (depends on 38)

The apparatus of claim 38, wherein the controller further comprises instructions for maintaining a pressure of between about 0.5 and 8 Torr in the process station while depositing the silicon nitride film on the substrate.

### Claim 51 (depends on 38)

A system, comprising the apparatus of claim 38 and a stepper tool.