# US 2013/0157465 A1 · Methods for stripping photoresist and/or cleaning metal regions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157465 A1
- Document ID: US20130157465A1
- Status: Published application
- Kind: A1
- Application number: 13/759,958
- Filed: 2013-02-05
- Published: 2013-06-20
- Earliest claimed: 2007-04-04
- Assignees: Novellus Systems, Inc.
- Inventors: David Chen; Haruhiro Harry Goto; Martina Martina; Frank Greer; Shamsuddin Alokozai
- Web page: https://patentgrep.com/patent/US20130157465A1

## CPC

- H10P 70/273: {the processing being a delineation of conductive layers, e.g. by RIE}
- H10P 50/287: {by chemical means}
- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10P 70/277: {the processing being a planarisation of conductive layers}
- H10P 72/0421: {for drying etching}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods are provided for cleaning metal regions overlying semiconductor substrates. A method for removing material from a metal region comprises heating the metal region, forming a plasma from a gas comprising hydrogen and carbon dioxide, and exposing the metal region to the plasma.

## Claims

### Claim 1

A method for removing material from a metal region overlying a semiconductor substrate, the method comprising:
forming a plasma from a gas comprising hydrogen and carbon dioxide; and
exposing the metal region to the plasma to thereby remove material from the metal region of the semiconductor substrate.

### Claim 2 (depends on 1)

The method of claim 1, further comprising heating the metal region to a temperature in a range of about 200° C. to about 450° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein the temperature is in a range of about 270° C. and 350° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the plasma is formed from gas comprising hydrogen and about 0.1% to about 10% carbon dioxide.

### Claim 5 (depends on 4)

The method of claim 4, wherein the plasma is formed gas comprising hydrogen and about 0.1% to about 1% carbon dioxide.

### Claim 6 (depends on 1)

The method of claim 1, wherein the plasma is a remote plasma.

### Claim 7 (depends on 1)

The method of claim 1, wherein the plasma is an in situ plasma.

### Claim 8 (depends on 1)

The method of claim 1, wherein the metal region is a metal silicide region.

### Claim 9 (depends on 8)

The method of claim 8, the metal silicide region is a nickel silicide region.

### Claim 10 (depends on 1)

The method of claim 1, wherein the metal region comprises a metal interconnect.

### Claim 11 (depends on 1)

The method of claim 1, wherein exposing the metal region to the plasma comprises exposing the metal region to the plasma and an inert gas.

### Claim 12 (depends on 11)

The method of claim 11, further comprising introducing the inert gas upstream from the metal region, wherein the inert gas has a flow rate in a range of about 0.15 and 25 times a flow rate of the hydrogen.

### Claim 13 (depends on 1)

The method of claim 1, wherein a polymeric material is removed.

### Claim 14

A method for cleaning a metal region overlying a semiconductor substrate, the method:
exciting a gas, wherein the gas comprises hydrogen and carbon dioxide; and
subjecting the metal region to the excited gas to thereby clean the metal region of the semiconductor substrate.

### Claim 15 (depends on 14)

The method of claim 14, wherein the gas comprises about 0.1% by volume to about 10% by volume carbon dioxide.

### Claim 16 (depends on 14)

The method of claim 14, wherein exciting the gas comprises exciting the gas upstream from a chamber in which the semiconductor substrate is disposed.

### Claim 17 (depends on 16)

The method of claim 16, further comprising introducing an inert gas upstream from the semiconductor substrate, and wherein subjecting the metal region to the excited gas comprises subjecting the metal region to the excited gas and the inert gas.

### Claim 18 (depends on 14)

The method of claim 14, wherein exciting the gas comprises exciting the gas in a chamber in which the semiconductor substrate is disposed.

### Claim 19

A method for fabricating a semiconductor structure including a metal region, the method comprising:
heating the metal region;
exciting a gas to form a plasma, wherein the gas comprises hydrogen and carbon dioxide;
subjecting the metal region to a plasma to thereby remove material from the metal region; and
forming an insulating layer overlying the metal region.

### Claim 20 (depends on 19)

The method of claim 19, wherein the gas comprises about 0.1% by volume to about 10% by volume carbon dioxide.