# US 2013/0157460 A1 · Methods for annealing a metal contact layer to form a metal silicidation layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157460 A1
- Document ID: US20130157460A1
- Status: Published application
- Kind: A1
- Application number: 13/714,588
- Filed: 2012-12-14
- Published: 2013-06-20
- Earliest claimed: 2011-12-16
- Assignees: Applied Materials, Inc.
- Inventors: Xinyu Fu; Wei Tang; Kavita Shah; Srinivas Gandikota; San H. Yu; Avgerinos Gelatos
- Web page: https://patentgrep.com/patent/US20130157460A1

## CPC

- H10D 64/01: Manufacture or treatment
- H10D 64/0131: {the additional conductive layer comprising a silicide layer formed by the silicidation reaction between the layer of silicon with a metal layer which is not formed by metal implantation}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods for annealing a contact metal layer for a metal silicidation process are provided in the present invention. In one embodiment, a method for annealing a contact metal layer for a silicidation process in a semiconductor device includes providing a substrate having a contact metal layer disposed thereon in a thermal annealing processing chamber, providing a heat energy to the contact metal layer in the thermal processing chamber, supplying a gas mixture including a nitrogen gas and a hydrogen gas while providing the heat energy to the contact layer in the thermal processing chamber, wherein the nitrogen gas and the hydrogen gas is supplied at a ratio between about 1:10 and about 1:1, and forming a metal silicide layer on the substrate.

## Claims

### Claim 1

A method for annealing a contact metal layer for a metal silicidation process in a semiconductor device, comprising:
providing a substrate having a contact metal layer disposed thereon in a thermal annealing processing chamber;
providing a heat energy to the contact metal layer in the thermal processing chamber;
supplying a gas mixture including a nitrogen gas and a hydrogen gas while providing the heat energy to the contact layer in the thermal processing chamber, wherein the nitrogen gas and the hydrogen gas is supplied at a ratio between about 1:10 and about 1:1; and
forming a metal silicide layer on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein providing the heat energy to the contact metal layer further comprises:
controlling a substrate temperature at between about 250 degrees Celsius and about 500 degrees Celsius.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal contact layer is formed in a processing chamber incorporated in a cluster system the same as where the thermal annealing processing chamber is incorporated to.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal silicide layer is formed on sidewalls of a gate electrode layer disposed on the substrate.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the metal silicide layer further comprises:
forming the metal silicide layer with plane (111) orientation.

### Claim 6 (depends on 1)

The method of claim 1, wherein the contact metal layer is formed by a chemical vapor deposition (CVD) process.

### Claim 7 (depends on 1)

The method of claim 1, wherein the metal contact layer is a cobalt layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein providing the heat energy to the contact metal layer further comprises:
performing the thermal annealing process for between about 30 seconds and about 180 seconds.

### Claim 9

A method for forming a metal silicidation process in a contact structure in a semiconductor device, comprising:
providing a substrate having film stack including a first dielectric layer disposed on a first electrode layer disposed thereon, wherein the film stack has an opening formed in the film stack through the first dielectric layer and the first electrode layer;
forming a contact metal layer lining sidewalls and a bottom of the opening;
providing a heat energy to the contact metal;
supplying a gas mixture including a nitrogen gas and a hydrogen gas while providing the heat energy to the contact; and
forming a metal silicide layer in the opening of the film stack.

### Claim 10 (depends on 9)

The method of claim 9, wherein the nitrogen gas and the hydrogen gas is supplied at a ratio between about 1:10 and about 1:1.

### Claim 11 (depends on 9)

The method of claim 9, wherein the film stack further comprises a second electrode disposed on the first dielectric layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the film stack further comprises a second dielectric layer disposed on the second electrode layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the opening is formed through the second dielectric layer and the second electrode layer.

### Claim 14 (depends on 9)

The method of claim 9, wherein forming the metal silicide layer in the opening of the film stack further comprising:
forming metal silicide layer in the first electrode layer.

### Claim 15 (depends on 9)

The method of claim 9, further comprising:
removing the contact metal layer unreacted with the first dielectric layer from the substrate.

### Claim 16 (depends on 9)

The method of claim 9, wherein the film stack further comprises a silicon containing layer disposed between the substrate and the first electrode layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the silicon containing layer is one of a polysilicon layer, a microcrystalline silicon layer, a monocrystalline silicon layer, a doped polysilicon layer, a doped microcrystalline silicon layer or a doped monocrystalline silicon layer.

### Claim 18 (depends on 11)

The method of claim 11, wherein the first and the second electrode layer are one of a polysilicon layer, a doped silicon layer or silicon containing materials.

### Claim 19

A method for forming a metal silicidation process in a contact structure in a semiconductor device, comprising:
providing a substrate having a contact metal layer disposed thereon in a thermal annealing processing chamber;
providing a heat energy to the contact metal layer in the thermal processing chamber;
supplying a gas mixture including only hydrogen gas while providing the heat energy to the contact layer in the thermal processing chamber; and
forming an amorphous type metal silicide layer on the substrate.

### Claim 20 (depends on 19)

The method of claim 19, wherein the metal silicide layer is formed on sidewalls of a gate electrode layer disposed on the substrate.