# US 2013/0157427 A1 · Etching composition and method for fabricating semiconductor device using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157427 A1
- Document ID: US20130157427A1
- Status: Published application
- Kind: A1
- Application number: 13/708,362
- Filed: 2012-12-07
- Published: 2013-06-20
- Earliest claimed: 2011-12-16
- Assignees: Soulbrain Co., Ltd.; SK hynix Inc.
- Inventors: Sung-Hyuk Cho; Kwon Hong; Hyung-Soon Park; Gyu-Hyun Kim; Ji-Hye Han; Jung-Hun Lim; Jin-Uk Lee; Jae-Wan Park; Chan-Keun Jung
- Web page: https://patentgrep.com/patent/US20130157427A1

## CPC

- H10P 50/642: {Chemical etching}
- H10B 41/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10D 30/025: {of vertical IGFETs (of VDMOS H10D30/0291; of vertical TFTs H10D30/0318)}
- H10P 50/283: {by chemical means}
- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10D 8/00: Diodes (variable-capacitance diodes H10D1/64; gated diodes H10D12/00)
- H10D 8/045: {of PN junction diodes}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention provides an etching composition, comprising a silyl phosphate compound, phosphoric acid and deionized water, and a method for fabricating a semiconductor, which includes an etching process employing the etching composition. The etching composition of the invention shows a high etching selectivity for a nitride film with respect to an oxide film. Thus, when the etching composition of the present invention is used to remove a nitride film, the effective field oxide height (EEH) may be easily controlled by controlling the etch rate of the oxide film. In addition, the deterioration in electrical characteristics caused by damage to an oxide film or etching of the oxide film may be prevented, and particle generation may be prevented, thereby ensuring the stability and reliability of the etching process.

## Claims

### Claim 1

An etching composition comprising a silyl phosphate compound represented by the following formula 1, phosphoric add and deionized water:
wherein R1 is selected from the group consisting of hydrogen, hydroxyl, substituted or unsubstituted (C1-C20)alkyl, (C1-C20)alkoxy, (C2-C20)alkenyl, (C3-C20)cycloalkyl, amino(C1-C20)alkyl, amino(C1-C10)alkylamino(C1-C10)alkyl, (C6-C20)aryl, (C1-C20)alkylcarbonyl, (C1-C20)alkylcarbonyloxy and cyano(C1-C10)alkyl;
wherein R2 and R3 are each independently selected from the group consisting of hydrogen, hydroxyl, substituted or unsubstituted (C1-C20)alkyl, (C1-C20)alkoxy, (C2-C20)alkenyl, (C3-C20)cycloalkyl, amino(C1-C20)alkyl, amino(C1-C10) alkylamino(C1-C10)alkyl, (C6-C20)aryl, (C1-C20)alkylcarbonyl, (C1-C20)alkylcarbonyloxy, cyano(C1-C10)alkyl, and a group represented by the following formula 3:
wherein R4 and R5 are each independently selected from the group consisting of hydrogen, (C1-C10)alkyl, (C2-C10)alkenyl, (C3-C20)cycloalkyl, amino(C1-C10)alkyl, and (C1-C10)alkyl substituted with one or more substituents selected from the group consisting of halogen, phenyl and cyclohexene oxide; and
wherein n is an integer of 1≦n≦4.

### Claim 2 (depends on 1)

The etching composition of claim 1, wherein R1 is selected from the group consisting of hydrogen, (C1-C10)alkyl, (C2-C10)alkenyl, (C3-C20)cycloalkyl, amino(C1-C10)alkyl, and (C1-C10)alkyl substituted with one or more substituents selected from the group consisting of halogen, phenyl and cyclohexene oxide.

### Claim 3 (depends on 1)

The etching composition of claim 1, wherein R2 and R3 are each independently selected from the group consisting of hydrogen, hydroxyl, (C1-C10)alkyl, (C1-C10)alkoxy, (C2-C10)alkenyl, (C3-C20)cycloalkyl, amino(C1-C10)alkyl, (C1-C10)alkyl substituted with at least one phenyl, and a group represented by the following formula
wherein R4 and R5 are each independently selected from the group consisting of hydrogen, (C1-C10)alkyl, (C2-C10)alkenyl, (C3-C20)cycloalkyl, amino(C1-C10)alkyl, and (C1-C10)alkyl substituted with one or more substituents selected from the group consisting of halogen, phenyl and cyclohexene oxide.

### Claim 4 (depends on 1)

The etching composition of claim 1, wherein the etching composition comprises 0.01-15 wt % of the silyl phosphate compound, 70-99 wt % of phosphoric acid and a balance of deionized water.

### Claim 5 (depends on 1)

The etching composition of claim 1, wherein the etching composition further comprises one or more additives selected from the group consisting of surfactants, sequestering agents, and anti-corrosive agents.

### Claim 6 (depends on 1)

The etching composition of claim 1, wherein the etching composition is used for etching of a nitride film.

### Claim 7 (depends on 1)

A method for fabricating a semiconductor device, the method comprising an etching process that is carried out using the etching composition of claim 1.

### Claim 8 (depends on 7)

The method of claim 7, wherein the etching process comprises etching a nitride film.

### Claim 9 (depends on 8)

The method of claim 8, wherein the etching process comprises selectively etching the nitride film with respect to an oxide film.

### Claim 10 (depends on 8)

The method of claim 8, wherein the nitride film comprises a silicon nitride film.

### Claim 11 (depends on 8)

The method of claim 8, wherein the etching process is carried out at a temperature between 50 and 300° C.

### Claim 12 (depends on 7)

The method of claim 7, wherein the method comprises a wet-etching process that is carried out using the etching composition in a device isolation process for the semiconductor device.

### Claim 13 (depends on 12)

The method of claim 12, wherein the method comprises:
forming a nitride film on a substrate;
forming a trench in the substrate using the nitride film as a hard mask;
forming an oxide film so as to fill the trench;
performing a chemical mechanical polishing process using the nitride film as a polishing stop film until the nitride film is exposed; and
removing the nitride film by a wet-etching process using the etching composition.

### Claim 14 (depends on 7)

The method of claim 7, wherein the method comprises a wet-etching process which is carried out using the etching composition in a process for forming a channel for a flash memory device.

### Claim 15 (depends on 14)

The method of claim 14, wherein the method comprises:
forming on a substrate a pipe gate electrode film in which a first nitride film for forming a pipe channel is buried;
forming on the resulting substrate a cell gate structure consisting of an alternating stack of a first interlayer insulating film and a first gate electrode film;
selectively etching the cell gate structure to form a pair of first and second holes so as to expose the first nitride film, and forming a second nitride film filling the first and second holes;
selectively etching the cell gate structure to form a trench that isolates the first gate electrode film into portions corresponding to the first and second holes, respectively;
forming on the resulting structure having the trench formed therein a selection gate structure comprising a second interlayer insulating film for forming a selection transistor and a second gate electrode film;
selectively etching the selection gate structure to form third and fourth holes exposing the second nitride film filled in the pair of first and second holes; and
performing a wet-etching process using the etching composition to remove the second nitride film exposed through the third and fourth holes, and the first nitride film below the second nitride film.

### Claim 16 (depends on 7)

The method of claim 7, wherein the method comprises a wet-etching process which is carried out using the etching composition in a process for forming a diode for a phase-change memory device.

### Claim 17 (depends on 16)

The method of claim 16, wherein the method comprises:
providing on a substrate an insulating structure having holes exposing a conductive region;
forming in the holes diodes coming into contact with the conductive region;
sequentially forming a titanium silicide film, a titanium nitride film and a nitride film on each diode;
performing a dry-etching process to form an oxide film in an isolated space between the diodes, followed by a chemical mechanical polishing process;
performing a wet-etching process using the etching composition to remove the nitride film; and
depositing titanium in spaces remaining after removal of the nitride film to form bottom electrodes.