# US 2013/0157426 A1 · Method for producing a conductive nanoparticle memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157426 A1
- Document ID: US20130157426A1
- Status: Published application
- Kind: A1
- Application number: 13/758,566
- Filed: 2013-02-04
- Published: 2013-06-20
- Earliest claimed: 2009-03-27
- Assignees: Centre National De La Recherche Scientifique; Commisariat A L'energie Atomique Aux Energies
- Inventors: Simon DELEONIBUS; Jean-Marie Basset; Paul Campbell; Thibaut Gutel; Paul-Henri Haumesser; Gilles Marchand; Catherine Santini
- Web page: https://patentgrep.com/patent/US20130157426A1

## CPC

- H10D 30/0413: {of FETs having charge-trapping gate insulators, e.g. MNOS transistors}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10B 43/00: EEPROM devices comprising charge-trapping gate insulators
- H10D 30/0411: {of FETs having floating gates}
- H10D 30/681: {having only two programming levels (Floating gate IGFETs programmable by two single electrons H10D30/688)}
- H10D 30/6893: {wherein the floating gate has multiple non-connected parts, e.g. multi-particle floating gate}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10D 64/685: {being perpendicular to the channel plane}
- B82Y 40/00: Manufacture or treatment of nanostructures
- Y10S 977/773: Nanoparticle, i.e. structure having three dimensions of 100 nm or less
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H10B: ELECTRONIC MEMORY DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for producing a memory device with nanoparticles, comprising the steps of: a) forming, in a semi-conductor substrate, source and drain regions, and at least one first dielectric on a zone of the substrate arranged between the source and drain regions and intended to form a channel of the memory device, b) deposition of an ionic liquid, comprising nanoparticles of an electrically conductive material in suspension, covering the first dielectric, c) formation of a deposition of nanoparticles on the first dielectric, d) removal of the remaining ionic liquid, e) forming a second dielectric and a control gate on at least one part of the deposition of nanoparticles.

## Claims

### Claim 1

A method for producing a memory device with nanoparticles, comprising at least the steps of:
a) forming, in a substrate based on at least one semi-conductor, source and drain regions, and at least one first dielectric on at least one zone of the substrate arranged between the source and drain regions, said at least one zone intended to form a channel of the memory device,
b) depositing of at least one ionic liquid that is an organic salt or mixture of organic salts in a liquid state, wherein nanoparticles of at least one electrically conductive material are suspended in the ionic liquid, said ionic liquid covering at least said first dielectric, and
c) forming, after step b), a deposition of said nanoparticles at least on said first dielectric,
d) removing, after step c), the ionic liquid remaining on the first dielectric,
e) forming, after step d), at least one second dielectric and at least one control gate on at least one part of the nanoparticles deposited on the first dielectric,
wherein the method further comprises applying a non-zero difference of electric potentials between the substrate and the ionic liquid during at least one part of step c) of the forming the deposition of nanoparticles, and wherein the difference of electric potentials is applied, via the substrate, between at least one of the source and drain region, and the ionic liquid.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the forming of the source and drain regions during step a) is obtained by steps comprising:
a1) forming at least one dummy gate on the substrate, at said at least one zone intended to form the channel of the memory device, and
a2) implanting dopants in the substrate using the dummy gate as an implantation mask, wherein doped zones of the substrate obtained from the implanting form the source and drain regions,
wherein the dummy gate is removed before implementing step b).

### Claim 3 (depends on 2)

The method according to claim 2, further comprising, between step a2) and the removal of the dummy gate, the following steps:
forming spacers based on at least one dielectric material against lateral flanks of the dummy gate,
depositing at least one coating layer on the dummy gate, the spacers and the source and drain regions, and
planarizing the coating layer with stoppage on the dummy gate.

### Claim 4 (depends on 3)

The method according to claim 3, further comprising, between the removal of the dummy gate and the step b) of depositing the ionic liquid, a step of etching at least one part of the spacers in contact with the substrate, forming hollows underneath a remaining part of the spacers, the ionic liquid also being deposited, during step b), in said hollows, and the nanoparticles also being deposited, during step c), at zones of the substrate situated in said hollows.

### Claim 5 (depends on 3)

The method according to claim 3, further comprising, between the step of forming spacers and the step of depositing the coating layer, a step of silicidating at least one part of the source and drain regions.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the step c) of forming the deposition of nanoparticles comprises at least one step of incubating the substrate and the ionic liquid for a time lasting between five minutes and one hour.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the step d) of removing the ionic liquid comprises a step of rinsing by a solvent and a step of drying, or a step of degradation by a heat treatment at a temperature between 200° C. and 500° C.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the step e) of forming the second dielectric and the control gate is obtained by steps comprising:
e1) depositing a layer based on a dielectric material at least on the nanoparticles deposited in step b),
e2) depositing a layer based on an electrically conductive material on the layer based on dielectric material, and
e3) planarizing at least said layer based on electrically conductive material and said layer based on dielectric material.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the ionic liquid comprises at least one cation of alkyl substituent bearing imidazolium.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the ionic liquid is chosen among BMIMNTf2, HMIMNTf2 or OMIMNTf2, the nanoparticles in suspension in the ionic liquid are based on ruthenium.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the step b) includes depositing the ionic liquid by spin coating or by spraying.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the nanoparticles in suspension in the ionic liquid are ruthenium.