# US 2013/0157416 A1 · Methods of forming a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157416 A1
- Document ID: US20130157416A1
- Status: Published application
- Kind: A1
- Application number: 13/717,899
- Filed: 2012-12-18
- Published: 2013-06-20
- Earliest claimed: 2010-01-29
- Assignees: Intersil Americas Inc.
- Inventors: Rick Carlton Jerome; Francois Hebert; Craig McLachlan; Kevin Hoopingarner
- Web page: https://patentgrep.com/patent/US20130157416A1

## CPC

- H10P 14/60: of insulating materials
- H10P 90/1914: {using bonding}
- H10P 90/00: Preparation of wafers not covered by a single main group of this subclass, e.g. wafer reinforcement
- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10P 90/1922: {using silicon etch back techniques, e.g. BESOI or ELTRAN}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10W 40/254: {Diamond}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method and structure for a semiconductor device, the device including a handle wafer, a diamond layer formed directly on a front side of the handle wafer, and a thick oxide layer formed directly on a back side of the handle wafer, the oxide of a thickness to counteract tensile stresses of the diamond layer. Nitride layers are formed on the outer surfaces of the diamond layer and thick oxide layer and a polysilicon is formed on outer surfaces of the nitride layers. A device wafer is bonded to the handle wafer to form the semiconductor device.

## Claims

### Claim 1

A method of forming a semiconductor device, comprising:
on a device wafer, depositing a thin nitride layer between a diamond layer and the device wafer, wherein the thin nitride layer comprises a thickness of about 500 Å to about 3000 Å;
depositing a polysilicon layer on the device wafer;
planarizing the polysilicon on an active side of the device wafer; and
attaching the planarized side of the device wafer to a handle wafer to form the semiconductor device.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thin nitride layer is deposited to thickness of about 1000 Å.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
depositing polysilicon on the handle wafer side of the semiconductor device; and
polishing a device side of the semiconductor device.

### Claim 4 (depends on 3)

The method of claim 3, wherein polishing comprises polishing the device side of the semiconductor device to within about 0.1 to about 100 μm of a diamond-silicon interface of the device wafer.

### Claim 5

A method of forming a semiconductor device, comprising:
growing a pad oxide on front and back sides of a device wafer;
depositing a thin (first) nitride layer over the front and back side pad oxide layers;
growing a diamond layer on the front side thin nitride layer;
depositing a second nitride layer on the diamond layer and the back side first nitride layer;
etching the back side to substantially remove the first and second nitride layers; growing
a thick oxide on the etched back side of the device wafer;
depositing a polysilicon layer on the front and back side of the device wafer;
planarizing the polysilicon on the front side of the device wafer; and
attaching the planarized side of the device wafer to a handle wafer to form the semiconductor device.

### Claim 6 (depends on 5)

The method of claim 5, wherein growing the pad oxide comprises growing to a thickness of about 650 Å.

### Claim 7 (depends on 5)

The method of claim 5, wherein depositing the first nitride layer comprises depositing to a thickness of about 500 to about 3000 Å.

### Claim 8 (depends on 7)

The method of claim 7, wherein depositing the first nitride layer comprises depositing to a thickness of about 1200 Å.

### Claim 9 (depends on 5)

The method of claim 5, wherein growing the diamond layer comprises growing to a thickness of about 1.5 μm.

### Claim 10 (depends on 5)

The method of claim 5, wherein depositing the second nitride layer comprises depositing to a thickness of about 500 to about 3000 Å.

### Claim 11 (depends on 10)

The method of claim 10, wherein depositing the second nitride layer comprises 1200 Å.

### Claim 12 (depends on 5)

The method of claim 5, wherein growing a thick oxide comprises growing to a thickness of about 2 μm.