# US 2013/0157410 A1 · Memory Cell Constructions, and Methods for Fabricating Memory Cell Constructions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157410 A1
- Document ID: US20130157410A1
- Status: Published application
- Kind: A1
- Application number: 13/763,664
- Filed: 2013-02-09
- Published: 2013-06-20
- Earliest claimed: 2011-03-08
- Assignees: Micron Technology, Inc.
- Inventors: Jun Liu; Jian Li
- Web page: https://patentgrep.com/patent/US20130157410A1

## CPC

- H10N 70/021: {Formation of switching materials, e.g. deposition of layers}
- H10D 48/04: of devices having bodies comprising selenium or tellurium in uncombined form
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10N 70/061: {Shaping switching materials}
- H10N 70/063: {by etching of pre-deposited switching material layers, e.g. lithography}
- H10N 70/231: {based on solid-state phase change, e.g. between amorphous and crystalline phases, Ovshinsky effect}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/861: {Thermal details}
- H10N 70/8828: {Tellurides, e.g. GeSbTe}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Some embodiments include methods for fabricating memory cell constructions. A memory cell may be formed to have a programmable material directly against a material having a different coefficient of expansion than the programmable material. A retaining shell may be formed adjacent the programmable material. The memory cell may be thermally processed to increase a temperature of the memory cell to at least about 300° C., causing thermally-induced stress within the memory cell. The retaining shell may provide a stress which substantially balances the thermally-induced stress. Some embodiments include memory cell constructions. The constructions may include programmable material directly against silicon nitride that has an internal stress of less than or equal to about 200 megapascals. The constructions may also include a retaining shell silicon nitride that has an internal stress of at least about 500 megapascals.

## Claims

### Claim 1

A method for fabricating a memory cell construction, comprising:
forming a memory cell to comprise a programmable material directly against another material; said other material having a different coefficient of expansion than the programmable material;
forming a retaining shell adjacent the programmable material;
exposing the memory cell to thermal processing to increase a temperature of the materials of the memory cell by at least about 200° C.; the exposure to said thermal processing creating a first stress due to the different rates of thermal expansion of the programmable material and the other material; the retaining shell providing a second stress which is at least about equal to the first stress to substantially balance the first stress.

### Claim 2 (depends on 1)

The method of claim 1 wherein the retaining shell comprises one or more of metal, carbon, silicon nitride and silicon dioxide.

### Claim 3 (depends on 1)

The method of claim 1 wherein the programmable material comprises germanium, antimony and tellurium; and wherein the retaining shell comprises silicon nitride having an internal stress of at least about 500 megapascals.

### Claim 4 (depends on 3)

The method of claim 3 wherein said other material comprises silicon nitride having an internal stress of less than or equal to about 200 megapascals.

### Claim 5 (depends on 1)

The method of claim 1 wherein the retaining shell is a laminate of two or more materials.

### Claim 6 (depends on 1)

The method of claim 1 wherein said laminate includes silicon dioxide and silicon nitride.

### Claim 7 (depends on 1)

The method of claim 1 wherein said laminate includes carbon and silicon nitride.

### Claim 8 (depends on 1)

The method of claim 1 wherein the retaining shell extends at least about half-way around an outer periphery of the programmable material along a cross-section through the programmable material and the retaining shell.

### Claim 9 (depends on 1)

The method of claim 1 wherein the retaining shell extends around at least about three-fourths of an outer periphery of the programmable material along a cross-section through the programmable material and the retaining shell.

### Claim 10 (depends on 1)

The method of claim 1 wherein the first stress is primarily a compressive stress, and wherein the second stress is primarily a tensile stress.

### Claim 11 (depends on 1)

The method of claim 1 wherein the first stress is primarily a tensile stress, and wherein the second stress is primarily a compressive stress.

### Claim 12 (depends on 1)

The method of claim 1 wherein the second stress is primarily an intrinsic stress within a material of the retaining shell, and is at least about 500 megapascals.

### Claim 13 (depends on 12)

The method of claim 12 wherein said material of the retaining shell comprises silicon nitride.

### Claim 14

A method for fabricating a memory cell construction, comprising:
forming a base comprising a bottom electrode extending through an electrically insulative material;
forming programmable material over the base, a bottom surface of the programmable material extending across the bottom electrode and the electrically insulative material;
forming a top electrode over the programmable material;
patterning the top electrode and the programmable material to have coextensive sidewall surfaces along a cross-section through the top electrode and the programmable material; said sidewall surfaces extending upwardly from a top surface of the base material;
forming a retaining shell that extends along the sidewall surfaces of the programmable material and the top electrode, and that extends over the top electrode;
and exposing the memory cell to thermal processing to increase a temperature of the programmable material, the base and the top electrode to at least about 300° C.; the exposure to said thermal processing creating a first stress due to thermal mismatch of the programmable material and the base material; the retaining shell providing a second stress which is at least about equal to the first stress to substantially balance the first stress.

### Claim 15 (depends on 14)

The method of claim 14 wherein the retaining shell and the electrically insulative material comprise a common composition.

### Claim 16 (depends on 14)

The method of claim 14 wherein the programmable material comprises germanium, antimony and tellurium; wherein the electrically insulative material comprises silicon nitride having an internal stress of less than or equal to about 200 megapascals; and wherein the retaining shell comprises silicon nitride having an internal stress of at least about 500 megapascals.

### Claim 17 (depends on 16)

The method of claim 16 further comprising forming silicon dioxide to be directly between the silicon nitride of the retaining shell and the programmable material.

### Claim at position 18

18-34. (canceled)

### Claim 35 (depends on 16)

The method of claim 16 wherein the bottom electrode comprises of one or more of TiSiN, TiN, and TaSiN.