# US 2013/0157409 A1 · Selective atomic layer deposition of passivation layers for silicon-based photovoltaic devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157409 A1
- Document ID: US20130157409A1
- Status: Published application
- Kind: A1
- Application number: 13/715,767
- Filed: 2012-12-14
- Published: 2013-06-20
- Earliest claimed: 2011-12-16
- Inventors: Kaushik VAIDYA; Hari K. PONNEKANTI
- Web page: https://patentgrep.com/patent/US20130157409A1

## CPC

- H10F 71/129: {Passivating}
- H10F 77/311: {for photovoltaic cells}
- H10W 20/081: {by forming openings in the dielectric parts}
- Y02E 10/50: Photovoltaic [PV] energy
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Embodiments of the invention generally provide methods for forming a silicon-based photovoltaic device. In one embodiment, a method includes forming a pattern inhibitor layer on a back surface of a substrate, wherein the pattern inhibitor layer covers a first portion of the back surface and a second portion of the back surface remains substantially free of the pattern inhibitor layer. The method further includes forming a passivation layer containing aluminum oxide on the second portion of the back surface and maintaining the pattern inhibitor layer substantially free of the passivation layer during a selective atomic layer deposition (S-ALD) process. Additionally, the method includes removing the pattern inhibitor layer from the back surface to reveal the first portion of the back surface and subsequently forming a contact layer on the first portion of the back surface.

## Claims

### Claim 1

A method for forming passivation materials on a substrate, comprising:
forming a pattern inhibitor layer on a back surface of a substrate, wherein the pattern inhibitor layer covers a first portion of the back surface and a second portion of the back surface remains substantially free of the pattern inhibitor layer;
forming a passivation layer comprising aluminum oxide on the second portion of the back surface using a selective atomic layer deposition process, wherein the pattern inhibitor layer is substantially free of the material used to form the passivation layer after performing the selective atomic layer deposition process;
removing the pattern inhibitor layer from the first portion of the back surface; and
forming a contact layer on the first portion of the back surface after removing the pattern inhibitor layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the pattern inhibitor layer is formed during a screen-printing process by applying an inhibitor solution to the first portion of the back surface.

### Claim 3 (depends on 3)

The method of claim 3, wherein the inhibitor solution comprises a hydrophobic self-assembled monolayer compound.

### Claim 4 (depends on 1)

The method of claim 1, wherein the pattern inhibitor layer is formed during a microcontact-printing process.

### Claim 5 (depends on 4)

The method of claim 4, wherein the microcontact-printing process further comprises:
exposing a pattern stamp to an inhibitor solution; and
contacting the back surface of the substrate with the inhibitor solution contained on the pattern stamp to form the pattern inhibitor layer on the first portion of the back surface.

### Claim 6 (depends on 4)

The method of claim 4, wherein the inhibitor solution comprises octadecyltrichlorosilane.

### Claim 7 (depends on 1)

The method of claim 1, wherein the pattern inhibitor layer comprises octadecyltrichlorosilane.

### Claim 8 (depends on 1)

The method of claim 1, wherein the passivation layer is formed by sequentially exposing the substrate to trimethyl aluminum and water vapor while depositing the aluminum oxide during the selective atomic layer deposition process.

### Claim 9 (depends on 8)

The method of claim 8, wherein the passivation layer has a thickness within a range from about 20 nm to about 80 nm.

### Claim 10 (depends on 1)

The method of claim 1, wherein the contact layer comprises aluminum and silver.

### Claim 11 (depends on 1)

The method of claim 1, wherein a metallic paste comprising aluminum and silver is disposed within the first portion of the back surface while forming the contact layer.

### Claim 12 (depends on 11)

The method of claim 11, further comprising heating the metallic paste to form a metallic silicide comprising aluminum silver silicide during a silicidization process, wherein the contact layer comprises the metallic silicide material.

### Claim 13 (depends on 1)

The method of claim 1, wherein the pattern inhibitor layer is removed from the back surface by dissolving the pattern inhibitor layer in a solvent selected from the group consisting of water, acetone, methyl ethyl ketone, diethyl ketone, benzene, toluene, xylene, derivatives thereof, mixtures thereof, and combinations thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the first portion of the back surface has a positive pattern for the contact layer and the second portion of the back surface has a negative pattern for the passivation layer.

### Claim 15 (depends on 1)

The method of claim 1, wherein the first portion of the back surface of the substrate has a surface area ratio within a range from about 2% to about 10% of the back surface.

### Claim 16 (depends on 1)

The method of claim 1, wherein native oxides and contaminants are removed from the back surface of the substrate during a preclean process prior to forming the pattern inhibitor layer.

### Claim 17

A method for forming passivation materials on a substrate, comprising:
forming a pattern inhibitor layer on a back surface of a substrate during a screen-printing process, wherein a positive pattern of the back surface is covered by the pattern inhibitor layer and a negative pattern of the back surface is substantially free of the pattern inhibitor layer;
forming a passivation layer comprising aluminum oxide on the back surface within the negative pattern and maintaining the pattern inhibitor layer substantially free of the passivation layer during a selective atomic layer deposition process;
removing the pattern inhibitor layer from the positive pattern of the back surface; and
forming a contact layer on the back surface within the positive pattern after removing the pattern inhibitor layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein the screen-printing process further comprises applying an inhibitor solution comprising octadecyltrichlorosilane to the first portion of the back surface.

### Claim 19

A method for forming passivation materials on a substrate, comprising:
forming a pattern inhibitor layer on a back surface of a substrate during a microcontact-printing process, wherein a positive pattern of the back surface is covered by the pattern inhibitor layer and a negative pattern of the back surface is substantially free of the pattern inhibitor layer;
forming a passivation layer comprising aluminum oxide on the back surface within the negative pattern and maintaining the pattern inhibitor layer substantially free of the passivation layer during a selective atomic layer deposition process;
removing the pattern inhibitor layer from the positive pattern of the back surface; and
forming a contact layer on the back surface within the positive pattern after removing the pattern inhibitor layer.

### Claim 20 (depends on 19)

The method of claim 19, wherein the microcontact-printing process further comprises:
exposing a pattern stamp to octadecyltrichlorosilane; and
contacting the back surface of the substrate with the inhibitor solution contained on the pattern stamp to form the pattern inhibitor layer on the first portion of the back surface.