# US 2013/0157186 A1 · Magnetic carrier, two-component developer, replenishing developer, and method of forming image

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157186 A1
- Document ID: US20130157186A1
- Status: Published application
- Kind: A1
- Application number: 13/718,301
- Filed: 2012-12-18
- Published: 2013-06-20
- Earliest claimed: 2011-12-19
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Manabu ONO; Osamu Ieda; Takahiro Ishii; Hiroaki Yoshida; Akira Kambayashi; Hiroko Endo; Motomi Noguchi
- Web page: https://patentgrep.com/patent/US20130157186A1

## CPC

- G03G 9/1075: {Structural characteristics of the carrier particles, e.g. shape or crystallographic structure}
- G03G 9/107: having magnetic components
- G03G 9/1085: {with non-ferrous metal oxide, e.g. MgO-Fe2O3}
- G03G 9/1135: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G 9/1139: {Inorganic components of coatings}
- G03G 13/08: using a solid developer, e.g. powder developer
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A magnetic carrier having excellent charge-imparting ability includes a magnetic particle and a coating layer disposed on a surface of the magnetic particle. The coating layer includes at least a resin component including an acrylic polymer and hydrotalcite dispersed in a form of particles having a predetermined number-average particle. A content of the hydrotalcite CH (parts by weight) is in a range of approximately 3 or more to approximately 30 parts by weight or less based on 100 parts by weight of the resin component. A content of the acrylic monomer unit CA (mol %) with respect to a total monomer unit included in the resin component and the content of the hydrotalcite CH satisfy the following relationship: 78≦CH×0.38+CA≦99.

## Claims

### Claim 1

A magnetic carrier comprising:
a magnetic particle; and
a coating layer disposed on a surface of the magnetic particle,
wherein the coating layer comprises at least a resin component containing approximately 70 wt % or more of a polymer comprising an acrylic monomer CA as a component and hydrotalcite CH dispersed in a form of particles having a number-average particle diameter ranging from approximately 0.1 μm or more to approximately 0.6 μm or less,
a content of the hydrotalcite CH in parts by weight is in a range of approximately 3 parts by weight or more to approximately 30 parts by weight or less based on 100 parts by weight of the resin component, and
a content of the acrylic monomer unit CA in mol % with respect to a total monomer unit included in the resin component and the content of the hydrotalcite CH in parts by weight satisfy the following relationship:
78≦CH×0.38+CA≦99, where 3≦CH≦30.

### Claim 2 (depends on 1)

The magnetic carrier of claim 1, wherein the hydrotalcite comprises aluminum and magnesium, and a molar ratio of magnesium to aluminum is in a range of approximately 0.25 or more to approximately 3.50 or less.

### Claim 3 (depends on 1)

The magnetic carrier of claim 1, wherein the resin comprises approximately 90 wt % or more of a tetrahydrofuran soluble component and a weight-average molecular weight of the tetrahydrofuran soluble component is in a range of approximately 30,000 or more to approximately 300,000 or less.

### Claim 4

A two-component developer comprising:
a magnetic carrier; and
a toner,
wherein the magnetic carrier comprises:
a magnetic particle; and
a coating layer disposed on a surface of the magnetic particle,
wherein the coating layer comprises at least a resin component containing approximately 70 wt % or more of a polymer comprising an acrylic monomer CA as a component and hydrotalcite CH dispersed in a form of particles having a number-average particle diameter ranging from approximately 0.1 μm or more to approximately 0.6 μm or less,
a content of the hydrotalcite CH in parts by weight is in a range of approximately 3 parts by weight or more to approximately 30 parts by weight or less based on 100 parts by weight of the resin component, and
a content of the acrylic monomer unit CA in mol % with respect to a total monomer unit included in the resin component and the content of the hydrotalcite CH in parts by weight satisfy the following relationship:
78≦CH×0.38+CA≦99, where 3≦CH≦30.

### Claim 5 (depends on 4)

The two-component developer of claim 4, wherein the hydrotalcite comprises aluminum and magnesium, and a molar ratio of magnesium to aluminum is in a range of approximately 0.25 or more to approximately 3.50 or less.

### Claim 6 (depends on 4)

The two-component developer of claim 4, wherein the resin comprises approximately 90 wt % or more of a tetrahydrofuran soluble component and a weight-average molecular weight of the tetrahydrofuran soluble component is in a range of approximately 30,000 or more to approximately 300,000 or less.

### Claim 7 (depends on 4)

The two-component developer of claim 4, wherein the toner comprises inorganic particles having a number-average particle diameter ranging from approximately 0.01 μm or more to approximately 0.15 μm or less, and
a shape factor ML2/A of the toner is in a range of approximately 120 or more to approximately 160 or less and is greater than that of the magnetic carrier.

### Claim 8

A replenishing developer used in a two-component developing method in which an electrostatic latent image is developed while the replenishing developer is supplied to a developing device and at least excessive magnetic carriers inside the developing device are discharged from the developing device,
wherein the replenishing developer is a two-component developer comprising a magnetic carrier and a toner,
in which the magnetic carrier comprises:
a magnetic particle; and
a coating layer disposed on a surface of the magnetic particle,
wherein the coating layer comprises at least a resin component containing approximately 70 wt % or more of a polymer comprising an acrylic monomer CA as a component and hydrotalcite CH dispersed in a form of particles having a number-average particle diameter ranging from approximately 0.1 μm or more to approximately 0.6 μm or less,
a content of the hydrotalcite CH in parts by weight is in a range of approximately 3 parts by weight or more to approximately 30 parts by weight or less based on 100 parts by weight of the resin component, and
a content of the acrylic monomer unit CA in mol % with respect to a total monomer unit included in the resin component and the content of the hydrotalcite CH in parts by weight satisfy the following relationship:
78≦CH×0.38+CA≦99, where 3≦CH≦30;
and the two-component developer comprises the magnetic carrier in an amount ranging from approximately 2 parts by weight or more to approximately 50 parts by weight or less based on 100 parts by weight of the toner.

### Claim 9 (depends on 8)

The replenishing developer of claim 8, wherein the hydrotalcite comprises aluminum and magnesium, and a molar ratio of magnesium to aluminum is in a range of approximately 0.25 or more to approximately 3.50 or less.

### Claim 10 (depends on 8)

The replenishing developer of claim 8, wherein the resin comprises approximately 90 wt % or more of a tetrahydrofuran soluble component and a weight-average molecular weight of the tetrahydrofuran soluble component is in a range of approximately 30,000 or more to approximately 300,000 or less.

### Claim 11 (depends on 8)

The replenishing developer of claim 8, wherein the toner comprises inorganic particles having a number-average particle diameter ranging from approximately 0.01 μm or more to approximately 0.15 μm or less, and
a shape factor ML2/A of the toner is in a range of approximately 120 or more to approximately 160 or less and is greater than that of the magnetic carrier.

### Claim 12

A method of forming an image, the method comprising:
charging an electrostatic latent image carrier by applying a voltage to a charging member;
forming an electrostatic latent image on the electrostatic latent image carrier charged in the charging;
developing the electrostatic latent image by using a two-component developer and forming a toner image on the electrostatic latent image carrier;
transferring the toner image to a transfer material with or without an intermediate transfer body being disposed therebetween; and
fixing the toner image transferred to the transfer material to the transfer material,
wherein the two-component developer comprises a magnetic carrier and a toner, in which the magnetic carrier comprises:
a magnetic particle; and
a coating layer disposed on a surface of the magnetic particle,
wherein the coating layer comprises at least a resin component containing approximately 70 wt % or more of a polymer comprising an acrylic monomer CA as a component and hydrotalcite CH dispersed in a form of particles having a number-average particle diameter ranging from approximately 0.1 μm or more to approximately 0.6 μm or less,
a content of the hydrotalcite CH in parts by weight is in a range of approximately 3 parts by weight or more to approximately 30 parts by weight or less based on 100 parts by weight of the resin component, and
a content of the acrylic monomer unit CA in mol % with respect to a total monomer unit included in the resin component and the content of the hydrotalcite CH in parts by weight satisfy the following relationship:
78≦CH×0.38+CA≦99, where 3≦CH≦30.

### Claim 13 (depends on 12)

The method of claim 12, wherein the hydrotalcite comprises aluminum and magnesium, and a molar ratio of magnesium to aluminum is in a range of approximately 0.25 or more to approximately 3.50 or less.

### Claim 14 (depends on 12)

The method of claim 12, wherein the resin comprises approximately 90 wt % or more of a tetrahydrofuran soluble component and a weight-average molecular weight of the tetrahydrofuran soluble component is in a range of approximately 30,000 or more to approximately 300,000 or less.

### Claim 15 (depends on 12)

The method of claim 12, wherein the toner comprises inorganic particles having a number-average particle diameter ranging from approximately 0.01 μm or more to approximately 0.15 μm or less, and
a shape factor ML2/A of the toner is in a range of approximately 120 or more to approximately 160 or less and is greater than that of the magnetic carrier.

### Claim 16 (depends on 12)

The method of claim 12, wherein, in the charging, the electrostatic latent image carrier is charged by applying only a direct voltage to a charging member rotatably installed to be in contact with a surface of the electrostatic latent image carrier.

### Claim 17 (depends on 12)

The method of claim 12, wherein the developing is performed in a developing device while a replenishing developer comprising the toner is supplied from a developer supply unit,
the supply of the replenishing developer is controlled based on a result of detection of a toner concentration transferred from a toner concentration detection unit installed in the developing device for measuring a toner concentration in the two-component developer used for development, and
the toner concentration is detected in a range in which a toner supplied from the developer supply unit into the developing device reaches within approximately 5 seconds.

### Claim 18 (depends on 17)

The method of claim 17, wherein the replenishing developer is used in a two-component developing method in which an electrostatic latent image is developed while the replenishing developer is supplied to a developing device and at least excessive magnetic carriers inside the developing device are discharged from the developing device,
wherein the replenishing developer is a two-component developer comprising the magnetic carrier and the toner, in which the two-component developer comprises the magnetic carrier in an amount ranging from approximately 2 parts by weight or more to approximately 50 parts by weight or less based on 100 parts by weight of the toner.

### Claim 19 (depends on 17)

The method of claim 17, wherein the hydrotalcite comprises aluminum and magnesium, and a molar ratio of magnesium to aluminum is in a range of approximately 0.25 or more to approximately 3.50 or less.

### Claim 20 (depends on 17)

The method of claim 17, wherein the resin comprises approximately 90 wt % or more of a tetrahydrofuran soluble component and a weight-average molecular weight of the tetrahydrofuran soluble component is in a range of approximately 30,000 or more to approximately 300,000 or less.