# US 2013/0157163 A1 · Method For Laminating Composite Sheet Using Release Film, Laminate Obtained by the Method, and Release Film For Use in the Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157163 A1
- Document ID: US20130157163A1
- Status: Published application
- Kind: A1
- Application number: 13/805,133
- Filed: 2011-07-01
- Published: 2013-06-20
- Earliest claimed: 2010-07-01
- Assignees: W. L. Gore & Associates, Inc.
- Inventors: Takafum Nanba; Naoki Ohashi
- Web page: https://patentgrep.com/patent/US20130157163A1

## CPC

- H01M 8/1006: Corrugated, curved or wave-shaped MEA
- B32B 27/08: of synthetic resin
- B32B 27/322: {comprising halogenated polyolefins, e.g. PTFE}
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 37/24: with at least one layer not being coherent before laminating, e.g. made up from granular material sprinkled onto a substrate (B32B37/15 takes precedence)
- C25B 9/23: comprising ion-exchange membranes in or on which electrode material is embedded
- H01M 8/0234: Carbonaceous material
- H01M 8/0239: Organic resins; Organic polymers
- H01M 8/0243: in the form of mixtures
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- B32B 38/10: Removing layers, or parts of layers, mechanically or chemically
- B32B 2037/268: {Release layers}
- B32B 2309/02: Temperature
- B32B 2309/027: Ambient temperature
- B32B 2309/105: Thickness
- B32B 2309/12: Pressure
- B32B 2457/18: Fuel cells
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In a carbon black (CB)/PTFE composite porous sheet that can be used as a gas diffusion layer in an electrochemical device in applications involving electro chemical reaction such as a polymer electrolyte fuel cell, electrolysis, gas sensor and the like, wrinkle or breakage may be produced due to its flexibility. A method is provided which makes it possible to easily handle this sheet that is difficult to handle, without giving rise to wrinkle or breakage. The present invention relates to a method for laminating the composite sheet on MEA, comprising the steps of: providing a membrane electrode assembly (MEA); providing a composite sheet comprising functional powder and polytetrafluoroethylene (PTFE); providing a release film; superimposing the composite sheet on the release film and pressing them at normal temperature; superimposing the composite sheet having the release film pressed at normal temperature thereto on MEA and hot-pressing them; and separating the release film from the composite sheet.

## Claims

### Claim 1

A method of laminating a composite sheet to MEA (Membrane Electrode Assembly) comprising the steps of:
providing a membrane electrode assembly (MEA);
providing a composite sheet comprising functional powder and polytetrafluoroethylene (PTFE);
providing a release film;
superimposing the composite sheet on the release film and pressing them at normal temperature;
superimposing the composite sheet having the release film pressed at normal temperature thereto on MEA and hot-pressing them; and
separating the release film from the composite sheet.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein, when the release film is separated from the composite sheet, 180 degree peel adhesive strength (in accordance with JIS K6854-2: 1999) of the release film is not less than 0.005 N/cm and not more than 0.025 N/cm.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the temperature of hot pressing is in the range of 100° C.-140° C.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the functional powder contains at least carbon black, activated carbon, or a mixture thereof.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the composite sheet is porous.

### Claim 6 (depends on 1)

The method as claimed in claim 1 wherein, after the release film is separated from the composite sheet, a part or all of the composite sheet is not transferred to the release film.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein, in the composite sheet pressed to the release film at normal temperature, there is no shift in position of the composite sheet relative to the release film, and no wrinkle or breakage of the composite sheet occurs.

### Claim 8 (depends on 1)

A laminate of a composite sheet to MEA manufactured by the method as claimed in claim 1.

### Claim 9

A laminate wherein a composite sheet comprising functional powder and polytetrafluoroethylene (PTFE) is overlaid on a release film exclusively used in the method as claimed in, and is subjected to pressing at normal temperature.

### Claim 10 (depends on 9)

A laminate as claimed in claim 9, wherein the laminate is in the form of a roll.