# US 2013/0157108 A1 · Lithium composite metal oxide and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0157108 A1
- Document ID: US20130157108A1
- Status: Published application
- Kind: A1
- Application number: 13/820,612
- Filed: 2011-09-02
- Published: 2013-06-20
- Earliest claimed: 2010-09-06
- Assignees: Sumitomo Chemical Company, Limited
- Inventors: Kenji Takamori; Yuichiro Imanari
- Web page: https://patentgrep.com/patent/US20130157108A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C01G 45/1221: Manganates or manganites with trivalent manganese, tetravalent manganese or mixtures thereof
- C01G 51/44: containing manganese
- C01G 51/50: of the type (MnO2)n-, e.g. Li(CoxMn1-x)O2 or Li(MyCoxMn1-x-y)O2
- C01G 53/44: containing manganese
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 50/491: Porosity
- C01P 2002/50: Solid solutions
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- H01M 10/052: Li-accumulators
- H01M 50/443: Particulate material
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a non-aqueous electrolyte secondary battery capable of exhibiting high discharge capacity maintenance rate at a high current rate, a lithium composite metal oxide useful therefor, and a method for producing the lithium composite metal oxide. This lithium composite metal oxide comprises Ni, Mn, Co, and Fe, and the BET specific surface area thereof is 3 m2/g to 15 m2/g. According to the present invention, a non-aqueous electrolyte secondary battery which exhibits high discharge capacity maintenance rate at a high current rate compared to a conventional lithium secondary battery can be obtained, and thus the secondary battery is very useful especially for applications where high discharge capacity maintenance rate at a high current rate is required, that is, non-aqueous electrolyte secondary batteries for automobiles or for power tools such as electric tools.

## Claims

### Claim 1

A lithium composite metal oxide comprising Ni, Mn, Co and Fe, wherein BET specific surface area is 3 m2/g to 15 m2/g.

### Claim 2 (depends on 1)

The lithium composite metal oxide according to claim 1, wherein the mean particle diameter as measured by laser diffraction and scattering is 0.1 μm to less than 1 μm.

### Claim 3 (depends on 1)

The lithium composite metal oxide according to claim 1, wherein the mean primary particle diameter is 0.05 μm to 0.4 μm.

### Claim 4 (depends on 1)

The lithium composite metal oxide according to claim 1 represented by the following formula (A):
Lia(Ni1-x-y-zMnxCoyFez)O2 (A)
wherein,
0.9≦a≦1.3,
0.3≦x≦0.6,
0.01≦y≦0.4,
0.01≦z≦0.1, and
0.3≦x+y+z≦0.7.

### Claim 5

A method for producing a lithium composite metal oxide comprising the following steps (1), (2) and (3) in that order:
(1) obtaining a co-precipitate slurry by bringing a raw material aqueous solution containing Ni ions, Mn ions, Co ions, Fe ions and sulfate ions into contact with alkali to form a co-precipitate,
(2) obtaining the co-precipitate from the co-precipitate slurry, and
(3) obtaining a lithium composite metal oxide by mixing the co-precipitate and a lithium compound, and calcining the resulting mixture by holding at a temperature of 650° C. to 950° C.

### Claim 6 (depends on 5)

The production method according to claim 5, wherein the step (2) is the following step (2′):
(2′) obtaining the co-precipitate by subjecting the co-precipitate slurry to solid- liquid separation followed by washing and drying.

### Claim 7 (depends on 5)

The production method according to claim 5, wherein the raw material aqueous solution is an aqueous solution obtained by dissolving a sulfate of Ni, a sulfate of Mn, a sulfate of Co and a sulfate of Fe in water.

### Claim 8 (depends on 7)

The production method according to claim 7, wherein the sulfate of Fe is a sulfate of divalent Fe.

### Claim 9 (depends on 5)

A lithium composite metal oxide obtained by the production method according to claim 5.

### Claim 10 (depends on 1)

A positive electrode active material for a non-aqueous electrolyte secondary battery, which material is mainly composed of the lithium composite metal oxide according to claim 1.

### Claim 11 (depends on 10)

A positive electrode for a non-aqueous electrolyte secondary battery, the electrode having the positive electrode active material for a non-aqueous electrolyte secondary battery according to claim 10.

### Claim 12 (depends on 11)

A non-aqueous electrolyte secondary battery having the positive electrode for a non-aqueous electrolyte secondary battery according to claim 11.

### Claim 13 (depends on 12)

The non-aqueous electrolyte secondary battery according to claim 12 further having a separator.

### Claim 14 (depends on 13)

The non-aqueous electrolyte secondary battery according to claim 13, wherein the separator is a separator composed of a laminated film obtained by laminating a heat- resistant porous layer and a porous film.