# US 2013/0156974 A1 · Method for manufacturing a porous synthetic diamond material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0156974 A1
- Document ID: US20130156974A1
- Status: Published application
- Kind: A1
- Application number: 13/639,841
- Filed: 2011-04-05
- Published: 2013-06-20
- Earliest claimed: 2010-04-07
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Emmanuel Scorsone; Hugues Girard
- Web page: https://patentgrep.com/patent/US20130156974A1

## CPC

- C23C 16/27: Diamond only
- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 16/274: {using microwave discharges}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of manufacturing a diamond layer having a porous three-dimensional structure, the method being of the type which includes growing the diamond layer from a sacrificial material and gradually decomposing said sacrificial material during growth of the diamond layer, said material including the following steps; 1) provision of a substrate capable of supporting the plasma-enhanced chemical vapour deposition growth of the diamond layer on at least one of the surfaces of of the substrate, the substrate comprising, on said at least one surface thereof, a layer made of a sacrificial material having a porous three-dimensional structure capable of gradually decomposing upon contact with said plasma, the layer of sacrificial material containing diamond grains of nanometric size, and 2) growth by plasma-enhanced chemical vapour deposition of the diamond layer from diamond grains and concomitant and gradual decomposition of the scrificial material upon contact with said plasma.

## Claims

### Claim 1

Method for manufacturing a diamond layer having a porous three-dimensional structure, the method being of the type which includes growing the diamond layer from a sacrificial material and gradually decomposing said sacrificial material during growth of the diamond layer, said method including the following steps:
1) provision of a substrate capable of supporting the plasma-enhanced chemical vapour deposition growth of the diamond layer on at least one of the faces of the substrate, the substrate comprising on said at least one face a layer made of a sacrificial material having a porous three-dimensional structure and being able to decompose progressively upon contact with said plasma, the layer of sacrificial material containing diamond grains of nanometric size;
2) growth by plasma-enhanced chemical vapour deposition of the diamond layer from diamond grains and concomitant and gradual decomposition of the sacrificial material upon contact with said plasma.

### Claim 2 (depends on 1)

Method for manufacturing according to claim 1, wherein the growth of the diamond layer is stopped when both the decomposition of the sacrificial material is complete and when the layer of diamond material has a desired porosity.

### Claim 3 (depends on 1)

Method for manufacturing according to claim 1, wherein the decomposition of the sacrificial material comprises the etching of the sacrificial material by the plasma.

### Claim 4 (depends on 1)

Method for manufacturing according to claim 1, wherein the sacrificial material is a polymer.

### Claim 5 (depends on 4)

Method for manufacturing according to claim 4, wherein the sacrificial material is a polypyrrole.

### Claim 6 (depends on 4)

Method for manufacturing according to claim 4, wherein the substrate and the sacrificial material are electrically conductive and the layer of sacrificial material present on at least one face of the substrate is deposited by electro-polymerisation.

### Claim 7 (depends on 1)

Method for manufacturing according to claim 1, wherein the size of the diamond grains is less than or equal to 100 nm, preferably less than or equal to 15 nm.

### Claim 8 (depends on 1)

Method for manufacturing according to claim 1, wherein the porous diamond layer has a porosity occupying from 5 to 50% of the total volume of the porous diamond layer.