# US 2013/0156683 A1 · Method of reducing magnetic and/or oxidic contaminants in lithium metal oxygen compounds

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0156683 A1
- Document ID: US20130156683A1
- Status: Published application
- Kind: A1
- Application number: 13/812,637
- Filed: 2011-07-04
- Published: 2013-06-20
- Earliest claimed: 2010-07-26
- Assignees: Sued-Chemie IP GmbH & Co. KG
- Inventors: Michael Holzapfel; Christian Vogler
- Web page: https://patentgrep.com/patent/US20130156683A1

## CPC

- B02C 23/08: Separating or sorting of material, associated with crushing or disintegrating (B02C23/18 takes precedence {; beater mills combined with sifting devices B02C13/13, B02C13/14; for tumbling mills B02C17/1835})
- C01B 25/37: Phosphates of heavy metals
- C01G 1/02: Oxides
- C01G 23/005: {Alkali titanates}
- C01G 31/00: Compounds of vanadium
- C01G 37/00: Compounds of chromium
- C01G 45/1228: of the type (MnO2)-, e.g. LiMnO2 or Li(MxMn1-x)O2
- C01G 45/1235: of the type (Mn2O4)2-, e.g. Li2Mn2O4 or Li2(MxMn2-x)O4
- C01G 45/1242: of the type (Mn2O4)-, e.g. LiMn2O4 or Li(MxMn2-x)O4
- C01G 45/1257: containing lithium, e.g. Li2MnO3 or Li2(MxMn1-x)O3
- C01G 49/0027: {containing one alkali metal}
- C01G 51/42: containing alkali metals, e.g. LiCoO2
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/54: of the type (Mn2O4)-, e.g. Li(NixMn2-x)O4 or Li(MyNixMn2-x-y)O4
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2006/80: Compositional purity
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- B02C: CRUSHING, PULVERISING, OR DISINTEGRATING IN GENERAL; MILLING GRAIN ({household tools and machines for pulverising foodstuffs, e.g. coffee and spice mills A47J42/00; pharmaceutical mortars A61J3/02; mechanical processing of refuse and garbage B03B9/06; dressing mould materials by grinding B22C5/04}; obtaining metallic powder by crushing, grinding or milling B22F9/04; {recovery of plastics by disintegrating B29B17/00; crushing raw materials in starch making C08B30/02; beaters for papermaking D21D1/02; crushing devices specially for transport in mines E21F13/002; slag crushing devices F23J1/00; fuel milling devices in combustion apparatus F23K1/00; household devices for crushing coal F24B15/02; ice disintegrating devices F25C5/02})
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of reducing magnetic and/or oxidic contaminants in lithium metal oxygen compounds in particle form, in order to obtain purified lithium metal oxygen compounds, by means of treatment in a grinding process and sifting process with continuous or non-continuous removal and obtaining of the purified lithium metal oxygen compound. The grinding process and sifting process are terminated prematurely before the residue amounts to less than 1% of the quantity m. The residue, containing contaminants, is discarded.

## Claims

### Claim 1

A method of reducing magnetic and/or oxidic contaminants in doped and non-doped lithium metal oxygen compounds in particle form, comprising the steps of:
a) providing a lithium metal oxygen compound in a quantity m, containing contaminants;
b) introducing a portion of from 5 to 15% of the quantity m of the lithium metal oxygen compound;
c) grinding and sifting the lithium metal oxygen compound with continuous removal and obtaining of the purified lithium metal oxygen compound to a residue of from 3% to 0.01% of the quantity m;
d) removing the purified lithium metal oxygen compound;
e) discarding the residue; and
f) repeating steps b) to e) until the whole quantity m has been converted.

### Claim 2 (depends on 1)

The method according to claim 1, characterized in that wherein the particles of the lithium metal oxygen compound have a carbon-containing coating at least in parts.

### Claim 3 (depends on 1)

The method according to claim 1 wherein the lithium metal oxygen compound is present doped with B, Al, Mg, Ca, Sr, P, Si, Ti, V, Cr, Mn, Fe, Co, Ni, Zr, Zn, Sn, Nb, Mo, Ru, or W, or mixtures thereof.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the lithium metal oxygen compound has an empirical formula with Lix, with 0<x and 0<y selected from LixMO2, LixM2O4, LixM5O12, LixMyO4, LixM2O4, LixM2O3, LixM3O4, Li2MO3, LixM2O3, LixM3O4, LiMO2, LiM′0.5M″0.5O2, or wherein the lithium metal oxygen compound has an empirical formula with Li1+x with 0<x and 0<y selected from Li1+xM2−xO4, Li1+xM2O4, Li2MO3, Li1+xM′2−xM″x(PO4)3, or wherein the lithium metal oxygen compound has an empirical formula L1−x with 0<x and 0<y selected from Li1−xM′yM″2−yO4, L1−xM′1.5M″0.5O4, or Li1-31 xM′yM″1−yO2.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the introduction of the lithium metal oxygen compound is terminated after introducing a portion of from 5 to 15% of the quantity m.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the purified lithium metal oxygen compound is continuously removed and obtained during the grinding and sifting.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the lithium metal oxygen compound is subjected to a grinding process and sifting process until the residue has been reduced to a portion of from 3% to 0.01% of the quantity m.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the grinding process and the sifting process are terminated before the residue has fallen below 3% to 0.01% of the quantity m.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the residue of from 3% to 0.01% of the quantity m, 2% to 0.5% of the quantity m is removed and discarded.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the grinding and sifting of the lithium metal oxygen compound is carried out in a single device.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the grinding and sifting of the lithium metal oxygen compound is carried out in separate devices.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the method according to steps a) to e) also comprises a further grinding step.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the further grinding step takes place in a further device separate from the grinding and/or sifting device.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the grinding and/or sifting and the further grinding step takes place in a single device.

### Claim 15 (depends on 1)

A lithium metal oxygen compound, obtainable by a the method according to claim 1, containing magnetic and/or oxidic contaminants of less than 20 ppm relative to the total weight of the lithium metal oxygen compound.