# US 2013/0156678 A1 · Graphene Films and Methods of Making Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0156678 A1
- Document ID: US20130156678A1
- Status: Published application
- Kind: A1
- Application number: 13/704,054
- Filed: 2011-06-16
- Published: 2013-06-20
- Earliest claimed: 2010-06-16
- Assignees: The Research Foundation for The State University of New York
- Inventors: Sarbajit Banerjee; Vincent Lee; Luisa Whitaker
- Web page: https://patentgrep.com/patent/US20130156678A1

## CPC

- C01B 32/182: Graphene
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 32/19: by exfoliation
- C01B 32/192: starting from graphitic oxides
- C01B 32/198: Graphene oxide
- C01B 32/23: Oxidation
- C25D 13/02: with inorganic material
- C25D 13/18: using modulated, pulsed, or reversing current
- C25D 13/22: Servicing or operating {apparatus or multistep processes}
- H01G 11/36: Nanostructures, e.g. nanofibres, nanotubes or fullerenes
- C01B 2204/30: Purity
- C01B 2204/32: Size or surface area
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

Provided are methods for forming graphene or functionalized graphene thin films. Also provided are graphene and functionalized graphene thin films formed by the methods. For example, electrophoretic deposition methods and stamping methods are used. Defect-free thin films can be formed. Patterned films can be formed. The methods can provide conformal coatings on non-planar substrates.

## Claims

### Claim 1

A method for forming graphene thin films or functionalized graphene coatings comprising the steps of:
a) providing a conducting substrate; and
b) electrophoretically forming the graphene or functionalized graphene using a solution comprising exfoliated graphene sheets or exfoliated functionalized graphene sheets;
such that a thin film of graphene or functionalized graphene is formed on the substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein if the functionalized graphene thin film is graphene oxide, the method further comprises the step of exposing the graphene oxide thin film to a reducing agent, such that graphene thin film is formed.

### Claim 3 (depends on 2)

The method of claim 2, wherein the reducing agent is in a slurry, a solution, liquid form, or gaseous form.

### Claim 4 (depends on 2)

The method of claim 2, wherein the reducing agent is ammonia, hydrazine, phenylhydrazine, sodium borohydride, potassium borohydride, lithium borohydride, calcium hydride, lithium hydride, sodium hydride, potassium hydride, lithium aluminum hydride, strontium hydride, barium hydride, ascorbic acid, sulfuric acid, hydroiodic acid, carbon monoxide, sodium bisulfite, potassium hydroxide, potassium napthalide, lithium napthalide, sodium napthalide, potassium phenanthrene, lithium phenanthrene, sodium phenanthrene, lithium biphenyl, sodium biphenyl, potassium biphenyl, metallic sodium, metallic potassium, metallic lithium, or a combination thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the electrophoretic deposition is carried out by applying a voltage having a DC component and/or an AC component between two electrodes, wherein the voltage is continuous, pulsed, or arbitrarily increasing or decreasing with time, and, if the voltage has an AC component, the AC component has variable frequency and amplitude.

### Claim 6 (depends on 1)

The method of claim 1, further comprising the step of thermally annealing the graphene or functionalized graphene thin film.

### Claim 7 (depends on 6)

The method of claim 6, wherein the thermal annealing is carried out at a temperature of 50° C. to 750° C., over a time of from 1 minute to 10 hours or the thermal annealing is carried out at a pressure of from 1×10−9 torr to 1×103 torr.

### Claim 8 (depends on 6)

The method of claim 6, wherein the thermal annealing is carried out in an atmosphere of air, hydrogen, oxygen, argon, helium, nitrogen, methane, ethane, propane, butane, carbon monoxide, carbon dioxide, acetylene, ethylene, or a mixture thereof.

### Claim 9 (depends on 2)

The method of claim 2, further comprising the step of thermally annealing the reduced graphene oxide thin film.

### Claim 10 (depends on 9)

The method of claim 9, wherein the thermal annealing is carried out at a temperature of 50° C. to 750° C., over a time of from 1 minute to 10 hours or at a pressure of from 1×10−9 torr to 1×103 torr.

### Claim 11 (depends on 9)

The method of claim 9, wherein the thermal annealing is carried out in an atmosphere of air, hydrogen, oxygen, argon, helium, nitrogen, methane, ethane, propane, butane, carbon monoxide, carbon dioxide, acetylene, ethylene, or a mixture thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein the solvent of the solution comprising exfoliated graphene oxide sheets or reduced graphene sheets is water, acetonitrile, methanol, ethanol, acetylacetonate, acetone, methyl ethyl ketone (MEK), 2-propanol, n-propanol, butanol, 1,3-butanediol, ethylene glycol, tetrahydrofuran, dimethylformamide, dimethyl sulfoxide, benzyl benzoate, N-methylpyrrolidone, γ-butyrolactone, pentane, hexanes, cyclohexane, cyclohexanone, benzene, toluene, xylenes, pyridine, methyl acetate, ethyl acetate, acetic acid, chloroform, dichloromethane, carbon tetrachloride, carbon disulfide, glyme, diglyme, triglyme, liquid NH3, ionic liquid or a mixture thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein the exfoliated graphene or exfoliated functionalized graphene sheets are present in the solution at concentrations of from 1×10−6 mg/mL to

### Claim 14 (depends on 1)

The method of claim 1, wherein the solution further comprises an additive selected from a salt, a surfactant, a polyelectrolyte, a biological macromolecule, and combinations thereof.

### Claim 15 (depends on 1)

The method of claim 1, wherein the conducting substrate is a non-planar substrate.

### Claim 16 (depends on 1)

The method of claim 1, wherein the graphene thin film or functionalized graphene thin film is formed on a continuous area of at least 16 square inches.

### Claim 17

A graphene or functionalized graphene thin film, wherein the thin film is free of detectible pin-hole defects.

### Claim 18 (depends on 17)

The graphene or functionalized graphene thin film of claim 17, wherein the thin film has 1% per unit area or less defects per square centimeter, or wherein the thin film has 3% or less impurities.

### Claim 19 (depends on 17)

The graphene or functionalized graphene thin film of claim 17, wherein surface contamination with extraneous impurities is limited to 3% or less surface coverage.

### Claim 20 (depends on 17)

The graphene or functionalized graphene thin film of claim 17, wherein the film covers a continuous area of at least 16 square inches.