# US 2013/0156661 A1 · Systems and methods for metal recovery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0156661 A1
- Document ID: US20130156661A1
- Status: Published application
- Kind: A1
- Application number: 13/716,819
- Filed: 2012-12-17
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: Freeport-Mcmoran Corporation
- Inventors: Joanna M. Robertson; Thomas R. Bolles; Wayne W. Hazen; Lawrence D. May; Jay C. Smith; David R. Baughman
- Web page: https://patentgrep.com/patent/US20130156661A1

## CPC

- C25C 1/12: of copper
- C22B 1/02: Roasting processes (C22B1/16 takes precedence)
- C22B 1/26: Cooling of roasted, sintered, or agglomerated ores
- C22B 3/02: Apparatus therefor
- C22B 3/12: in inorganic alkaline solutions
- C22B 3/14: containing ammonia or ammonium salts
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 15/0002: {Preliminary treatment}
- C22B 15/0078: {with ammoniacal solutions, e.g. ammonium hydroxide}
- C22B 15/0086: {by physical methods}
- C22B 23/005: {Preliminary treatment of ores, e.g. by roasting or by the Krupp-Renn process}
- C22B 23/0446: {with an ammoniacal liquor or with a hydroxide of an alkali or alkaline-earth metal}
- C22B 23/0453: {Treatment or purification of solutions, e.g. obtained by leaching (C22B23/0407 takes precedence)}
- C25C 1/00: Electrolytic production, recovery or refining of metals by electrolysis of solutions (C25C5/00 takes precedence)
- C25C 5/02: from solutions
- C25C 7/02: Electrodes (consumable anodes for the refining the metals C25C1/00 - C25C5/00); Connections thereof
- Y02P 10/20: Recycling
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Various embodiments provide a process roasting a metal bearing material under oxidizing conditions to produce an oxidized metal bearing material, roasting the oxidized metal bearing material under reducing conditions to produce a roasted metal bearing material, leaching the roasted metal hearing material in a basic medium to yield a pregnant leach solution, conditioning the pregnant leach solution to thrill a preprocessed metal bearing material; and leaching the preprocessed metal bearing material in acid medium.

## Claims

### Claim 1

A process comprising:
roasting a metal bearing material under oxidizing conditions to produce an oxidized metal bearing material;
roasting the oxidized metal bearing material under reducing conditions to produce a roasted metal bearing material;
leaching the roasted metal bearing material in a basic medium to yield a pregnant leach solution;
conditioning the pregnant leach solution to form a preprocessed metal bearing material; and
leaching the preprocessed metal bearing material in acid medium.

### Claim 2 (depends on 1)

The process of claim 1, wherein the basic medium comprises at least one of ammonia, ammonium carbonate, and ammonium sulfate.

### Claim 3 (depends on 2)

The process of claim 2, wherein the acid medium comprises sulfuric acid.

### Claim 4 (depends on 2)

The process of claim 2, wherein the conditioning comprises crystallizing the pregnant leach solution to form the preprocessed metal bearing material and a vapor.

### Claim 5 (depends on 1)

The process of claim 1, wherein the oxidizing conditions comprise an oxygen gas containing atmosphere.

### Claim 6 (depends on 1)

The process of claim 1, wherein the reducing conditions comprise at least one of a carbon monoxide gas containing atmosphere and a hydrogen gas containing atmosphere.

### Claim 7 (depends on 4)

The process of claim 4, further comprising condensing the vapor into a condensate and recycling the condensate into the basic medium.

### Claim 8 (depends on 4)

The process of claim 4, further comprising washing the preprocessed metal bearing material with water.

### Claim 9 (depends on 4)

The process of claim 4, further comprising adding seed crystals to the pregnant leach solution.

### Claim 10 (depends on 5)

The process of claim 5, wherein the oxidizing conditions further comprise a temperature of from about 550° C.; to about 700° C.

### Claim 11 (depends on 6)

The process of claim 6, wherein the reducing conditions further comprise a temperature of from about 475° C. to about 575° C.

### Claim 12 (depends on 1)

The process of claim 1, further comprising grinding a metal bearing ore to yield the metal bearing material.

### Claim 13 (depends on 1)

The process of claim 1, wherein the leaching the preprocessed metal bearing material in acid medium yields an acidic pregnant leach solution and further comprising recovering a metal value from the acidic pregnant leach solution.

### Claim 14

A system comprising:
an oxidizing roaster configured to receive oxygen gas and configured to heat a metal bearing material to temperatures of from about 200° C. to about 800° C.;
a reducing roaster configured to receive at least one of carbon monoxide gas and hydrogen gas and configured to heat the metal bearing material to temperatures of from about 200° C. to about 800° C.;
a basic leaching vessel configured to receive a roasted metal bearing material from the roaster;
a crystallizer configured to crystallize the roasted metal bearing material to yield a preprocessed metal bearing material; and
an acid leaching vessel configured to receive the preprocessed metal bearing material from the crystallizer.

### Claim 15 (depends on 14)

The system of claim 14, wherein the basic leaching vessel is configured to receive at least one of ammonia and ammonium carbonate.

### Claim 16 (depends on 14)

The system of claim 14, wherein the acid leaching vessel is configured to receive sulfuric acid.

### Claim 17 (depends on 14)

The system of claim 14, wherein the crystallizer is configured to produce a condensate comprising ammonia.

### Claim 18

A process comprising:
oxidizing sulfides of copper by roasting under oxygen gas to produce an oxidized copper bearing material;
reducing copper by roasting the oxidized copper bearing material under at least one of hydrogen and carbon monoxide to produce a roasted copper bearing material;
leaching the roasted copper bearing material using ammonia to yield a pregnant leach solution;
precipitating copper containing compounds from the pregnant leach solution; and
leaching the copper containing compounds in acid medium.

### Claim 19 (depends on 18)

The process of claim 18, further comprising precipitating cobalt containing compounds from the pregnant leach solution.

### Claim 20 (depends on 19)

The process of claim 19, wherein the precipitating comprises adding copper containing seed crystals to the pregnant leach solution.