# US 2013/0156660 A1 · Rare earth recovery from phosphor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0156660 A1
- Document ID: US20130156660A1
- Status: Published application
- Kind: A1
- Application number: 13/714,276
- Filed: 2012-12-13
- Published: 2013-06-20
- Earliest claimed: 2011-12-15
- Assignees: REEnewal Corporation
- Inventors: Narayan V. Thakur
- Web page: https://patentgrep.com/patent/US20130156660A1

## CPC

- C01F 17/241: containing two or more rare earth metals, e.g. NdPrO3 or LaNdPrO3
- C01F 17/13: by using ion exchange resins, e.g. chelate resins
- C01F 17/17: involving a liquid-liquid extraction
- C01F 17/218: Yttrium oxides or hydroxides
- C01F 17/224: Oxides or hydroxides of lanthanides
- C01F 17/229: Lanthanum oxides or hydroxides
- C01F 17/235: Cerium oxides or hydroxides
- C01F 17/271: Chlorides
- C01F 17/276: Nitrates
- C22B 59/00: Obtaining rare earth metals
- C01P 2006/80: Compositional purity
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method is described to produce high purity rare earth oxides of the elements La, Ce, Tb, Eu and Y from phosphor, such as waste phosphor powders originating in various consumer products. One approach involves leaching the powder in two stages and converting to two groups of relatively high purity mixed rare earth oxides. The first group containing Eu and Y is initially separated by solvent extraction. Once separated, Eu is purified using Zn reduction with custom apparatus. Y is purified by running another solvent extraction process using tricaprylmethylammonium chloride. Ce is separated from the second group of oxides, containing La, Ce and Tb by using solvent extraction. Subsequently, La and Tb are separated from each other and converted to pure oxides by using solvent extraction processes. A one-stage leaching process, wherein all rare earths get leached into the solution and subsequently processed, is also described.

## Claims

### Claim 1

A method for recovery of a rare earth constituent from a phosphor, the method comprising:
leaching a rare earth constituent from a phosphor to form a rare earth leachate solution;
adjusting the rare earth leachate solution to a pH of about 2, and then precipitating the rare earth constituent from the rare earth leachate solution as one or more rare earth oxalates; and
converting the one or more rare earth oxalates to one or more rare earth oxides.

### Claim 2 (depends on 1)

The method of claim 1, wherein the one or more rare earth oxides is greater than 95% pure.

### Claim 3 (depends on 1)

The method of claim 1, wherein the one or more rare earth oxides is about 99% pure.

### Claim 4 (depends on 1)

The method of claim 1, wherein the phosphor is a powder.

### Claim 5 (depends on 4)

The method of claim 4, wherein the phosphor powder is derived from phosphor waste.

### Claim 6 (depends on 1)

The method of claim 1, wherein the rare earth constituent comprises compounds comprising a rare earth element selected from the group consisting of La, Ce, Eu, Tb, Y and combinations thereof

### Claim 7 (depends on 6)

The method of claim 6, wherein the leaching comprises a first stage of preferentially leaching Eu and Y-comprising compounds from the phosphor by dilute H2SO4 to form a Eu and Y leachate, while La, Ce and Tb-comprising compounds from the phosphor are preferentially retained in an un-leached residue.

### Claim 8 (depends on 7)

The method of claim 7, wherein the dilute H2SO4 is about 6N H2SO4.

### Claim 9 (depends on 7)

The method of claim 7, further comprising a second stage of preferentially leaching La, Ce and Tb-comprising compounds from the un-leached residue of first stage by concentrated H2SO4 to form a La, Ce and Tb leachate.

### Claim 10 (depends on 9)

The method of claim 9, wherein the concentrated H2SO4 is about 36N H2SO4.

### Claim 11 (depends on 6)

The method of claim 6, wherein the leaching comprises a single stage of leaching La, Ce, Eu, Tb and Y-comprising compounds from the phosphor by concentrated H2SO4.

### Claim 12 (depends on 11)

The method of claim 11, wherein the concentrated H2SO4 is about 36N H2SO4.

### Claim 13 (depends on 9)

The method of claim 9, wherein the first stage Eu and Y leachate and second stage La, Ce and Tb leachate are further separately processed through the precipitation and conversion operations resulting in a high purity mixture of Eu and Y oxides and a separate high purity mixture of La, Ce and Tb oxides.

### Claim 14 (depends on 11)

The method of claim 11, wherein a high purity mixture of La, Ce, Eu, Tb, and Y oxides results.

### Claim 15 (depends on 13)

The method of claim 13, wherein the purity of the oxides is greater than 95%.

### Claim 16 (depends on 15)

The method of claim 15, wherein the purity of the oxides is about 99%.

### Claim 17 (depends on 1)

The method of claim 1, further comprising further separation and purification of individual rare earth oxides by solvent extraction or Zn reduction to achieve a high purity of greater than 99%.

### Claim 18 (depends on 13)

The method of claim 13, further comprising separation of high purity Y from the high purity mixture of Eu and Y oxides by solvent extraction with a solvent system comprising a solvent selected from the group consisting of Di-(2-ethylhexyl)phosphoric acid in dilute H2SO4/HCl/HNO3, 2-ethylhexyl 2-ethylhexyl phosphonic acid in dilute H2SO4/HCl/HNO3, and combinations thereof

### Claim 19 (depends on 18)

The method of claim 18, further comprising purification of Y oxide to greater than 99% purity using solvent extraction with tricaprylmethylammonium chloride.

### Claim 20 (depends on 18)

The method of claim 18, further comprising purification of Eu oxide to greater than 99% purity by Zn reduction from a mixture of Eu and Y traces after separation of Y.

### Claim 21 (depends on 18)

The method of claim 18, further comprising separation of greater than 99% high purity Ce oxide from the mixture of oxides of La, Ce and Tb by solvent extraction with a solvent system comprising a solvent selected from the group consisting of Di-(2-ethylhexyl)phosphoric acid, 2-ethylhexyl 2-ethylhexyl phosphonic acid, tributyl phosphate, and combinations thereof

### Claim 22 (depends on 21)

The method of claim 21, further comprising separation of greater than 99% high purity La and Tb by solvent extraction with a solvent system comprising a solvent selected from the group consisting of Di-(2-ethylhexyl)phosphoric acid, 2-ethylhexyl 2-ethylhexyl phosphonic acid, and combinations thereof, after separation of Ce.

### Claim 23 (depends on 1)

The method of claim 1, wherein the phosphor is not fired with an alkali material, such that no caustic fusion occurs.

### Claim 24 (depends on 1)

The method of claim 1, wherein the method does not comprise an alkaline or acidic digestion step between leaching and precipitating.

### Claim 25 (depends on 1)

The method of claim 1, wherein the rare earth constituent comprises compounds comprising a rare earth element selected from the group consisting of La, Ce, Eu, Tb, Y, Gd and combinations thereof.

### Claim 26

A method for recovery of a rare earth constituent from a phosphor, the method comprising:
leaching a rare earth constituent from a phosphor to form a rare earth leachate solution;
preferentially precipitating the rare earth constituent from the rare earth leachate solution as one or more rare earth oxalates;
converting the one or more rare earth oxalates to one or more rare earth oxides, wherein the one or more rare earth oxides have a purity of greater than 95%.

### Claim 27

A method for recovery of a rare earth constituent from a phosphor, the method comprising:
leaching a rare earth constituent from a phosphor to form a rare earth leachate solution;
adjusting the rare earth leachate solution to a pH preferential to the precipitation of rare earth oxalates relative to other metal oxalates, and then precipitating the rare earth constituent from the rare earth leachate solution as one or more rare earth oxalates; and
converting the one or more rare earth oxalates to one or more rare earth oxides.

### Claim 28

A method for recovery of a rare earth constituent from a phosphor, the method comprising:
leaching a rare earth constituent from a phosphor to form a rare earth leachate solution;
precipitating the rare earth constituent from the rare earth leachate solution as one or more rare earth oxalates; and
converting the one or more rare earth oxalates to one or more rare earth oxides;
wherein the phosphor is not fired with an alkali material, such that no caustic fusion occurs.

### Claim 29

A method for recovery of a rare earth constituent from a phosphor, the method comprising:
leaching a rare earth constituent from a phosphor to form a rare earth leachate solution;
precipitating the rare earth constituent from the rare earth leachate solution as one or more rare earth oxalates; and
converting the one or more rare earth oxalates to one or more rare earth oxides;
wherein the method does not comprise an alkaline or acidic digestion between leaching and precipitating.

### Claim 30

A Zn reduction apparatus, comprising:
a column packed with zinc granules;
a receptacle for collecting eluent from the column;
an inlet and an outlet on the receptacle configured for passing gaseous nitrogen through the receptacle;
the apparatus configured and operated to achieve commercial scale Zn reduction for purification of Eu oxide to greater than 99%.