# US 2013/0156555 A1 · Braze materials, brazing processes, and components with wear-resistant coatings formed thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0156555 A1
- Document ID: US20130156555A1
- Status: Published application
- Kind: A1
- Application number: 13/326,656
- Filed: 2011-12-15
- Published: 2013-06-20
- Earliest claimed: 2011-12-15
- Assignees: General Electric Company
- Inventors: David Edwin Budinger; Jonathan Reid Biberstine
- Web page: https://patentgrep.com/patent/US20130156555A1

## CPC

- B22F 7/064: {using an intermediate powder layer}
- B22F 1/09: {Mixtures of metallic powders}
- B23K 1/0018: {Brazing of turbine parts}
- B23K 35/0244: {Powders, particles or spheres; Preforms made therefrom}
- B23K 35/3046: {Co as the principal constituent}
- C22C 19/056: {with the maximum Cr content being at least 10% but less than 20%}
- C22C 19/07: based on cobalt
- B22F 2007/068: {repairing articles}
- B23K 2101/34: Coated articles {; Surface treated articles}
- F05D 2230/237: Brazing
- F05D 2230/90: Coating; Surface treatment
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

Braze materials, brazing processes, and coatings produced therefrom, for example, a wear-resistant coating suitable for protecting surfaces subjected to wear at high temperatures. The braze material includes first particles formed of a metallic alloy and second particles formed of a cobalt-base braze alloy having a melting point below the melting point of the first particles. The braze alloy consists of, by weight, 3.5 to 15.0% silicon, 2.0 to 6.0% boron, and the balance cobalt and incidental impurities, and the second particles constitute at least 30 up to 90 weight percent of the first and second particles combined. Following a brazing cycle performed on the braze material, a wear-resistant coating is formed in which the first particles are dispersed in a matrix of the braze alloy.

## Claims

### Claim 1

A braze material comprising:
a plurality of first particles of a metallic alloy having a melting point; and
a plurality of second particles of a cobalt-base braze alloy having a melting point below the melting point of the metallic alloy, the cobalt-base braze alloy consisting of, by weight, 3.5 to 15.0% silicon, 2.0 to 6.0% boron, and the balance cobalt and incidental impurities, the second particles constituting at least 30 up to 90 weight percent of the first and second particles combined.

### Claim 2 (depends on 1)

The braze material according to claim 1, wherein the cobalt-base braze alloy has a melting temperature of less than 1175° C.

### Claim 3 (depends on 1)

The braze material according to claim 1, wherein the cobalt-base braze alloy consists of, by weight, 7.3 to 7.7% silicon, 3.6 to 4.0% boron, and the balance cobalt and the incidental impurities.

### Claim 4 (depends on 1)

The braze material according to claim 1, wherein the cobalt-base braze alloy consists of, by weight, about 7.5% silicon, about 3.8% boron, and the balance cobalt and the incidental impurities.

### Claim 5 (depends on 1)

The braze material according to claim 1, wherein the second particles constitute about 40 to about 55 weight percent of the first and second particles combined.

### Claim 6 (depends on 1)

The braze material according to claim 1, wherein the metallic alloy is a cobalt-base alloy.

### Claim 7 (depends on 6)

The braze material according to claim 6, wherein:
the metallic alloy consists of, by weight, 27 to 30% molybdenum, 16.5 to 18.5% chromium, 3.0 to 3.8% silicon, up to 1.5% iron, up to 1.5% nickel, up to 0.15% oxygen, up to 0.03% sulfur, up to 0.03% phosphorus, and up to 0.08% carbon, the balance cobalt and incidental impurities; or
the metallic alloy consists of, by weight, about 26.0 to about 30.0% chromium, about 18.0 to about 21.0% tungsten, about 4.0 to about 6.0% nickel, about 0.75 to about 1.25% vanadium, about 0.7 to about 1.0% carbon, up to 3.0% iron, up to 1.0% manganese, up to 0.5% molybdenum, up to 1.0% silicon, up to 0.10% boron, and the balance cobalt and incidental impurities; or
the metallic alloy has a combined chromium, nickel and tungsten content of about 40 to 60 weight percent.

### Claim 8 (depends on 1)

The braze material according to claim 1, wherein the braze material is in the form of a paste and consists essentially of the first and second particles and a binder.

### Claim 9 (depends on 1)

The braze material according to claim 1, wherein the braze material is in the form of a tape and consists essentially of the first and second particles and a binder.

### Claim 10 (depends on 1)

The braze material according to claim 1, wherein the braze material is in the form of a sintered preform and consists of the first and second particles.

### Claim 11 (depends on 1)

A process of using the braze material of claim 1, the process comprising:
applying the braze material to a surface of a substrate region;
heating the braze material to melt the second particles but not the first particles to form a molten braze material in which the first particles are dispersed; and then
allowing the molten braze material to cool, solidify, and form a solid coating on the surface of the substrate region, the solid coating consisting of the cobalt-base braze alloy and the first particles dispersed therein.

### Claim 12 (depends on 11)

The process according to claim 11, wherein the solid coating is more wear resistant than the substrate region.

### Claim 13 (depends on 12)

The process according to claim 12, wherein the metallic alloy is a cobalt-base alloy and wherein:
the cobalt-base alloy consists of, by weight, 27 to 30% molybdenum, 16.5 to 18.5% chromium, 3.0 to 3.8% silicon, up to 1.5% iron, up to 1.5% nickel, up to 0.15% oxygen, up to 0.03% sulfur, up to 0.03% phosphorus, and up to 0.08% carbon, the balance cobalt and incidental impurities; or
the cobalt-base alloy consists of, by weight, about 26.0 to about 30.0% chromium, about 18.0 to about 21.0% tungsten, about 4.0 to about 6.0% nickel, about 0.75 to about 1.25% vanadium, about 0.7 to about 1.0% carbon, up to 3.0% iron, up to 1.0% manganese, up to 0.5% molybdenum, up to 1.0% silicon, up to 0.10% boron, and the balance cobalt and incidental impurities; or
the cobalt-base alloy has a combined chromium, nickel and tungsten content of about 40 to 60 weight percent.

### Claim 14 (depends on 12)

The process according to claim 12, wherein the braze material is heated to a temperature of less than 1175° C. and the substrate region is formed of an alloy whose ductility decreases if heated to a temperature above 1175° C. due to carbide segregation along grain boundaries thereof.

### Claim 15 (depends on 12)

The process according to claim 12, wherein the substrate region is a surface region of a component of a turbomachine.

### Claim 16

A component of an aircraft gas turbine engine, the component comprising:
a substrate region; and
a coating on the substrate region, the coating defining an outermost surface of the component and being more wear resistant than the substrate region, the coating comprising a cobalt-base alloy in which particles are dispersed, the cobalt-base alloy consisting of, by weight, 3.5 to 15.0% silicon, 2.0 to 6.0% boron, and the balance cobalt and incidental impurities, at least some of the particles consisting of a metallic alloy having a melting point that is higher than the cobalt-base alloy, the cobalt-base alloy constituting at least 30 up to 90 weight percent of the coating, the particles constituting at least 10 up to 70 weight percent of the coating.

### Claim 17 (depends on 16)

The component according to claim 16, wherein the cobalt-base alloy consists of, by weight, 7.3 to 7.7% silicon, 3.6 to 4.0% boron, and the balance cobalt and the incidental impurities.

### Claim 18 (depends on 16)

The component according to claim 16, wherein the metallic alloy of the particles is a cobalt-base alloy and wherein:
the cobalt-base alloy consists of, by weight, 27 to 30% molybdenum, 16.5 to 18.5% chromium, 3.0 to 3.8% silicon, up to 1.5% iron, up to 1.5% nickel, up to 0.15% oxygen, up to 0.03% sulfur, up to 0.03% phosphorus, and up to 0.08% carbon, the balance cobalt and incidental impurities; or
the cobalt-base alloy consists of, by weight, about 26.0 to about 30.0% chromium, about 18.0 to about 21.0% tungsten, about 4.0 to about 6.0% nickel, about 0.75 to about 1.25% vanadium, about 0.7 to about 1.0% carbon, up to 3.0% iron, up to 1.0% manganese, up to 0.5% molybdenum, up to 1.0% silicon, up to 0.10% boron, and the balance cobalt and incidental impurities; or
the cobalt-base alloy has a combined chromium, nickel and tungsten content of about 40 to 60 weight percent.

### Claim 19 (depends on 16)

The component according to claim 16, wherein the coating consists of the cobalt-base alloy and the particles dispersed therein, the cobalt-base alloy constitutes at least 30 up to 90 weight percent of the coating, and the particles constitute at least 10 up to 70 weight percent of the coating.

### Claim 20 (depends on 16)

The component according to claim 16, wherein the component is part of an exhaust flap assembly.