# US 2013/0155580 A1 · Wet Electrolytic Capacitor Containing an Improved Anode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155580 A1
- Document ID: US20130155580A1
- Status: Published application
- Kind: A1
- Application number: 13/710,515
- Filed: 2012-12-11
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: AVX Corporation
- Inventors: Tomas Karnik; Jan Petrzilek; Martin Biler
- Web page: https://patentgrep.com/patent/US20130155580A1

## CPC

- H01G 9/0525: {Powder therefor}
- H01G 9/0029: {Processes of manufacture}
- H01G 9/048: characterised by their structure (H01G11/22 takes precedence)
- H01G 9/052: Sintered electrodes
- H01G 9/145: Liquid electrolytic capacitors (H01G11/00 takes precedence)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A wet electrolytic capacitor that includes a sintered porous anode body containing a dielectric layer, a fluid electrolyte, and a cathode is provided. At least one longitudinally extending channel is recessed into the anode body. The channel may have a relatively high aspect ratio (length divided by width), such as about 2 or more, in some embodiments about 5 or more, in some embodiments from about 10 to about 200, in some embodiments from about 15 to about 150, in some embodiments from about 20 to about 100, and in some embodiments, from about 30 to about 60.

## Claims

### Claim 1

A wet electrolytic capacitor comprising:
an anode containing a sintered porous anode body that extends in a longitudinal direction and is coated with a dielectric, wherein the anode body contains a sidewall positioned between a proximal end and an opposing distal end, wherein a longitudinally extending channel is recessed into the sidewall;
a fluid electrolyte; and
a cathode that contains a substrate.

### Claim 2 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the porous anode body is formed from a powder that contains tantalum, niobium, or an electrically conductive oxide thereof.

### Claim 3 (depends on 2)

The wet electrolytic capacitor of claim 2, wherein the powder has a specific charge of from about 20,000 to about 450,000 μF*V/g.

### Claim 4 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the anode body has a length in the longitudinal direction and a width and depth, and wherein the ratio of the length to both the width and depth is from about 1.1 to about 10.

### Claim 5 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the longitudinally extending channel intersects both the distal end and the proximal end.

### Claim 6 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein an anode lead extends from the proximal end of the anode in the longitudinal direction.

### Claim 7 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the anode body has a generally cylindrical shape.

### Claim 8 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the channel has an aspect ratio of about 2 or more.

### Claim 9 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the channel has an aspect ratio of from about 15 to about 150.

### Claim 10 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the channel has a length of from about 1 to about 60 millimeters and a width of from about 0.02 to about 15 millimeters.

### Claim 11 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the channel has a substantially constant width.

### Claim 12 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the channel has a depth that is from about 5% to about 50% of the thickness of the porous anode body.

### Claim 13 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein a plurality of longitudinally extending channels are recessed into the sidewall of the anode body.

### Claim 14 (depends on 13)

The wet electrolytic capacitor of claim 13, wherein from 4 to 10 channels are recessed into the anode body.

### Claim 15 (depends on 13)

The wet electrolytic capacitor of claim 13, wherein the channels are distributed in a generally symmetrical manner about a longitudinal center of the anode body.

### Claim 16 (depends on 13)

The wet electrolytic capacitor of claim 13, wherein the anode body contains first and second longitudinally extending channels, the first channels being recessed into the sidewall to a different depth than the second channels.

### Claim 17 (depends on 16)

The wet electrolytic capacitor of claim 16, wherein the first channels have a depth that is from about 25% to about 45% of the thickness of the anode body, and the second channels have a depth that is from about 10% to about 25% of the thickness of the anode body.

### Claim 18 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the channel is substantially parallel to the longitudinal direction.

### Claim 19 (depends on 1)

The wet electrolytic capacitor of claim 1, further comprising an electrochemically active material that is disposed on a surface of the substrate.

### Claim 20 (depends on 19)

The wet electrolytic capacitor of claim 19, wherein the electrochemically active material contains a conductive polymer.

### Claim 21 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the substrate comprises titanium, tantalum, or a combination thereof.

### Claim 22 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the fluid electrolyte is aqueous.

### Claim 23 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the fluid electrolyte has a pH of from about 4.5 to about 7.0.

### Claim 24 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the substrate is in the form of a casing within which the anode and the fluid electrolyte are positioned.

### Claim 25 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the capacitor exhibits a volumetric efficiency of from about 20,000 to about 95,000 μF*V/cm3.

### Claim 26 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the maximum ripple current is about 2.5 Amps or more.

### Claim 27 (depends on 1)

The wet electrolytic capacitor of claim 1, wherein the anode contains about 50 ppm carbon or less.

### Claim 28

A wet electrolytic capacitor comprising:
an anode containing a generally cylindrical, sintered porous anode body having a sidewall positioned between a proximal end and an opposing distal end, the anode body being coated with a dielectric, wherein a plurality of longitudinally extending channels are recessed into the sidewall of the anode body, the anode body containing tantalum, niobium, or an electrically conductive oxide thereof, wherein the anode further comprises an anode lead wire that extends from the proximal end of the anode in the longitudinal direction;
an aqueous fluid electrolyte; and
a generally cylindrical metal casing within which the anode and the fluid electrolyte are positioned, wherein an electrochemically active material is disposed on an interior surface of the casing.

### Claim 29 (depends on 28)

The wet electrolytic capacitor of claim 28, wherein the channels have an aspect ratio of about 2 or more.

### Claim 30 (depends on 28)

The wet electrolytic capacitor of claim 28, wherein the channels have an aspect ratio of from about 15 to about 150.

### Claim 31 (depends on 28)

The wet electrolytic capacitor of claim 28, wherein the channels have a substantially constant width.

### Claim 32 (depends on 28)

The wet electrolytic capacitor of claim 28, wherein the channels are distributed in a generally symmetrical manner about a longitudinal center of the anode body.

### Claim 33 (depends on 28)

The wet electrolytic capacitor of claim 28, wherein the anode body contains first and second longitudinally extending channels, the first channels being recessed into the sidewall of the anode body to a different depth than the second channels.

### Claim 34

A method for forming a wet electrolytic capacitor, the method comprising:
pressing a powder into a porous anode body that extends in a longitudinal direction, wherein a longitudinally extending channel is recessed into the anode body;
sintering the porous anode body;
anodically oxidizing the sintered, anode body to form an anode; and
placing the anode into electrical communication with a cathode and a fluid electrolyte.