# US 2013/0155578 A1 · Capacitor and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155578 A1
- Document ID: US20130155578A1
- Status: Published application
- Kind: A1
- Application number: 13/615,650
- Filed: 2012-09-14
- Published: 2013-06-20
- Earliest claimed: 2011-12-15
- Assignees: Industrial Technology Research Institute
- Inventors: Hsieh-Ho Tsai; Yu-Lin Hsin; Yu-Ming Lin; Li-Key Chen; Mei-Hua Wang; Chih-Kuang Chang
- Web page: https://patentgrep.com/patent/US20130155578A1

## CPC

- H01G 11/24: characterised by structural features of the materials making up or comprised in the electrodes, e.g. form, surface area or porosity; characterised by the structural features of powders or particles used therefor
- H01G 11/28: arranged or disposed on a current collector; Layers or phases between electrodes and current collectors, e.g. adhesives
- H01G 11/32: Carbon-based
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- Y02E 60/13: Energy storage using capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A capacitor and a manufacturing method thereof are provided. Two electrodes are disposed opposite to each other. Two electrode protection layers are respectively disposed on inner sides of the electrodes and include carbon particles each covered and bonded with a polymer shell. Active carbon layers are disposed on opposite inner sides of the electrode protection layers. The separator is disposed between the active carbon layers. The electrolyte fills between the electrode protection layers. The polymer shells of each electrode protection layer are bonded to the surface of the corresponding electrode by first and second functional groups. The first functional groups include thiol groups. The second functional groups include epoxy groups or carboxylic groups. The electrode protection layers serve as adhesion layers between the active carbon layers and the electrodes, and protect the electrodes from being corroded by the acid electrolyte solution.

## Claims

### Claim 1

A capacitor comprising:
two electrodes disposed opposite to each other;
two electrode protection layers respectively disposed on opposite inner sides of the electrodes, the electrode protection layers comprising carbon particles each covered and bonded with a polymer shell;
two active carbon layers respectively disposed on opposite inner sides of the electrode protection layers;
a separator disposed between the active carbon layers; and
an electrolyte filling space between the two electrode protection layers,
wherein the polymer shells of the electrode protection layers are bonded to surfaces of the electrodes through first and second functional groups, the first functional groups comprise thiol groups, and the second functional groups comprise epoxy groups or carboxylic groups.

### Claim 2 (depends on 1)

The capacitor as recited in claim 1, wherein the polymer shells of each of the electrode protection layers are bonded to the surface of one of the electrodes through cross-linking based on the first and second functional groups.

### Claim 3 (depends on 1)

The capacitor as recited in claim 1, wherein the first functional groups are bonded to the surfaces of the electrodes.

### Claim 4 (depends on 1)

The capacitor as recited in claim 1, wherein the polymer shells have the second functional groups.

### Claim 5 (depends on 1)

The capacitor as recited in claim 1, wherein the polymer shells have the first and second functional groups.

### Claim 6 (depends on 1)

The capacitor as recited in claim 1, wherein each of the polymer shells comprises a plurality of polymer chains, and a weight-average molecular weight of each of the polymer chains ranges from about 50,000 to about 150,000.

### Claim 7 (depends on 6)

The capacitor as recited in claim 6, wherein each of the polymer chains comprises polyglycidyl methacrylate, poly 2-(4-vinylphenyl)oxirane, or polyacrylic acid.

### Claim 8 (depends on 1)

The capacitor as recited in claim 1, wherein the carbon particles comprise active carbon, carbon nano-tubes, diamond particles, graphite powder, carbon black, carbon fibers, graphenes, or a mixture thereof.

### Claim 9 (depends on 1)

The capacitor as recited in claim 1, wherein the carbon particles account for about 85 wt % to about 97 wt % of each of the electrode protection layers.

### Claim 10

A manufacturing method of a capacitor, comprising:
providing two electrodes;
forming an electrode protection layer on a surface of each of the electrodes, the electrode protection layers comprising carbon particles each covered and bonded with a polymer shell, wherein a method of forming the electrode protection layers comprises:
respectively performing a surface treatment step on the surface of each of the electrodes, so as to generate first functional groups on the surface of each of the electrodes, the first functional groups comprising thiol groups;
grafting polymer chains onto surfaces of the carbon particles to form modified carbon particles, the polymer chains having second functional groups, the second functional groups comprising epoxy groups or carboxylic groups;
covering the treated surfaces of the electrodes with the modified carbon particles; and
adding a cross-linking agent to the surfaces of the carbon particles and carrying out a cross-linking reaction to form the electrode protection layer on each of the electrodes;
forming an active carbon layer on a surface of each of the electrode protection layers, wherein the surface of each of the electrode protection layers is not opposite to the electrode;
placing the two electrodes opposite to each other, such that the active carbon layers are located on respective inner sides of the two electrodes, and placing a separator between the active carbon layers; and
injecting an electrolyte between the electrode protection layers.

### Claim 11 (depends on 10)

The manufacturing method of the capacitor as recited in claim 10, wherein each of the polymer shells comprises a plurality of polymer chains, and a weight-average molecular weight of each of the polymer chains ranges from about 50,000 to about 150,000.

### Claim 12 (depends on 11)

The manufacturing method of the capacitor as recited in claim 11, wherein each of the polymer chains comprises polyglycidyl methacrylate, poly 2-(4-vinylphenyl)oxirane, or polyacrylic acid.

### Claim 13 (depends on 10)

The manufacturing method of the capacitor as recited in claim 10, wherein the carbon particles comprise active carbon, carbon nano-tubes, diamond particles, graphite powder, carbon black, carbon fibers, graphenes, or a mixture thereof.

### Claim 14 (depends on 10)

The manufacturing method of the capacitor as recited in claim 10, wherein the carbon particles account for about 85 wt % to about 97 wt % of each of the electrode protection layers.

### Claim 15 (depends on 10)

The manufacturing method of the capacitor as recited in claim 10, wherein a material used in the surface treatment step comprises thiol-containing organic acid or thiol-containing organic amine.

### Claim 16

A manufacturing method of a capacitor, comprising:
providing two electrodes;
forming an electrode protection layer on a surface of each of the electrodes, the electrode protection layers comprising carbon particles each covered and bonded with a polymer shell, wherein a method of forming the electrode protection layers comprises:
grafting polymer chains onto surfaces of the carbon particles to form modified carbon particles, the polymer chains having first and second functional groups, the first functional groups comprising epoxy groups or carboxylic groups, the second functional groups comprising thiol groups;
covering the surface of each of the electrodes with the modified carbon particles; and
adding a cross-linking agent to the surfaces of the carbon particles and carrying out a cross-linking reaction to form the electrode protection layer on each of the electrodes;
forming an active carbon layer on a surface of each of the electrode protection layers, wherein the first surface of each of the electrode protection layers is not opposite to the electrode;
placing the two electrodes opposite to each other, such that the active carbon layers are located on respective inner sides of the two electrodes, and placing a separator between the active carbon layers; and
injecting an electrolyte between the electrode protection layers.

### Claim 17 (depends on 16)

The manufacturing method of the capacitor as recited in claim 16, wherein a weight-average molecular weight of each of the polymer chains ranges from about 50,000 to about 150,000.

### Claim 18 (depends on 17)

The manufacturing method of the capacitor as recited in claim 17, wherein each of the polymer chains comprises polyglycidyl methacrylate, poly 2-(4-vinylphenyl)oxirane, or polyacrylic acid.

### Claim 19 (depends on 16)

The manufacturing method of the capacitor as recited in claim 16, wherein the carbon particles comprise active carbon, carbon nano-tubes, diamond particles, graphite powder, carbon black, carbon fibers, graphenes, or a mixture thereof.

### Claim 20 (depends on 16)

The manufacturing method of the capacitor as recited in claim 16, wherein the carbon particles account for about 85 wt % to about 97 wt % of each of the electrode protection layers.