# US 2013/0155576 A1 · Electrode and/or capacitor formation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155576 A1
- Document ID: US20130155576A1
- Status: Published application
- Kind: A1
- Application number: 13/817,723
- Filed: 2011-07-20
- Published: 2013-06-20
- Earliest claimed: 2011-05-31
- Assignees: Indian Ins tit u te of Technology Madras
- Inventors: Sundara Ramaprabhu; Ashish Kumar Mishra
- Web page: https://patentgrep.com/patent/US20130155576A1

## CPC

- H01G 9/0029: {Processes of manufacture}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C01B 32/225: Expansion; Exfoliation
- C01B 32/23: Oxidation
- H01G 11/30: characterised by their material
- H01G 11/46: Metal oxides
- Y02E 60/13: Energy storage using capacitors
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Technologies are generally described related to the design, manufacture and/or use of electrodes, capacitors, or any other similar component. In an example, a system effective to form a component may include a container effective to receive graphite nanoplatelets and effective to receive ruthenium chloride. The system may include a coating device in communication with the container. The system may further include a processor arranged in communication with the container and the coating device. The processor may be configured to control the container effective to combine the ruthenium chloride with the graphite nanoplatelets under reaction conditions sufficient to form a ruthenium oxide graphite nanoplatelets nanocomposite. The processor may further be configured to control the coaling device effective to coat a support with the ruthenium oxide graphite nanoplatelets nanocomposite.

## Claims

### Claim 1

A method of forming a component, the method comprising:
combining ruthenium oxide with graphite nanoplatelets to form a combination; and
placing at least a part of the combination on a support.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the support includes a first support and a second support, and wherein placing at least the part of the combination on the support further comprises:
placing at least a first portion of the combination on the first support;
placing at least a second portion of the combination on the second support; and
placing a separator on a first side of the first support and on a first side of the second support, wherein the separator includes an electrolyte.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein the support includes a first support and a second support, and wherein placing at least the part of the combination on the support further comprises:
placing at least a first portion of the combination on the first support;
placing at least a second portion of the combination on the second support; and
placing a separator on a first side of the first support and on a first side of the second support, the separator including polypropylene and a solution including sulfuric acid.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the support includes a first support and a second support, and wherein placing at least the part of the combination on the support further comprises:
placing at least a first portion of the combination on the first support;
placing at least a second portion of the combination on the second support;
placing a separator including an electrolyte on a first side of the first support and on a first side of the second support;
placing a first contact on a second side of the first support; and
placing a second contact on a second side of the second support.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein the support includes a first support and a second support, and wherein placing at least the part of the combination on the support further comprises:
placing at least a first portion of the combination on the first support;
placing at least a second portion of the combination on the second support;
placing a separator including an electrolyte on a first side of the first support and on a first side of the second support;
placing a first contact on a second side of the first support;
placing a second contact on a second side of the second support;
placing a third support on the first contact;
placing a fourth support on the second contact; and
placing a clamp on the third and fourth support.

### Claim 6 (depends on 1)

The method as recited in claim 1, further comprising: reacting graphite in a container including an acid under sufficient reaction conditions to form the graphite nanoplatelets.

### Claim 7 (depends on 1)

The method as recited in claim 1, further comprising:
reacting graphite in a first container including a first acid under first sufficient reaction conditions to form the graphite nanoplatelets;
reacting the graphite nanoplatelets in a second container including a second acid under second sufficient reaction conditions to form functionalized graphite nanoplatelets; and
combining ruthenium chloride with the functionalized graphite nanoplatelets.

### Claim 8 (depends on 1)

The method as recited in claim 1, wherein combining the ruthenium oxide with the graphite nanoplatelets comprises:
reacting graphite in a first container including a first acid under first sufficient reaction conditions to form acid intercalated graphite;
heating the acid intercalated graphite under sufficient conditions to form graphite nanoplatelets;
reacting the graphite nanoplatelets in a second container including a second acid under second sufficient reaction conditions to form functionalized graphite nanoplatelets;
combining ruthenium chloride with the functionalized graphite nanoplatelets to form a result; and
reducing the result with a solution including sodium.

### Claim 9 (depends on 1)

The method as recited in claim 1, further comprising:
brushing at least a first portion of the combination on a first piece of carbon paper; and
brushing at least a second portion of the combination on a second piece of carbon paper.

### Claim 10

A system effective to form a component, the system comprising:
a container configured effective to receive graphite nanoplatelets and effective to receive ruthenium chloride;
a coating device arranged in communication with the first container; and
a processor arranged in communication with the first container and the coating device, wherein the processor is configured to:
control the first container effective to combine the ruthenium chloride with the graphite nanoplatelets under reaction conditions sufficient to form a ruthenium oxide graphite nanoplatelets nanocomposite; and
control the coating device effective to coat a support with the ruthenium oxide graphite nanoplatelets nanocomposite.

### Claim 11 (depends on 10)

The system as recited in claim 10, wherein the container is a first container, and the system further comprises:
a second container arranged in communication with the first container, wherein the second container is effective to receive graphite and an acid; and
wherein:
the processor is further configured to control the second container effective to react the acid and the graphite under reaction conditions sufficient to form the graphite nanoplatelets.

### Claim 12 (depends on 10)

The system as recited in claim 10, wherein the container is a first container, and the system further comprises:
a second container arranged in communication with the first container, wherein the second container is effective to receive graphite and a first acid;
a third container arranged in communication with the first container and the second container, wherein the third the third container includes a second acid; and
the processor is further configured to:
control the second container effective to react the first acid and the graphite under reaction conditions sufficient to form the graphite nanoplatelets;
control the third container effective to react the second acid and the graphite nanoplatelets under sufficient reaction conditions to form functionalized graphite nanoplatelets; and
control the third container effective to combine the ruthenium chloride with the functionalized graphite nanoplatelets under reaction conditions sufficient to form a ruthenium oxide graphite nanoplatelets nanocomposite.

### Claim 13 (depends on 10)

The system as recited in claim 10, wherein the container is a first container, and the system further comprises:
an oven;
a second container arranged in communication with the oven and the first container, wherein the second container is effective to receive graphite and a first acid;
a third container arranged in communication with the first container and the second container, wherein the third the third container includes a second acid; and
a fourth container; and wherein:
the processor is further configured to:
control the second container effective to react the first acid and the graphite reaction conditions sufficient to form acid intercalated graphite;
control the oven effective to heat the acid intercalated graphite under sufficient reaction conditions to form the graphite nanoplatelets;
control the third container to effective to react the second acid and the graphite nanoplatelets under sufficient reaction conditions to form functionalized graphite nanoplatelets;
control the first container effective to combine the ruthenium chloride with the functionalized graphite nanoplatelets to form a result; and
control the fourth container effective to reduce the result with a solution including sodium to form the ruthenium oxide graphite nanoplatelets nanocomposite.

### Claim 14 (depends on 10)

The system as recited in claim 10, wherein the coating device is configured effective to brush at least a part of the combination on a first piece of carbon paper, and brush at least a part of the combination on a second piece of carbon paper.

### Claim 15 (depends on 1)

A component produced according to claim 1, the component comprising:
a support;
a nanocomposite on the support, wherein the nanocomposite includes ruthenium oxide and graphite nanoplatelets.

### Claim 16 (depends on 15)

The component as recited in claim 15, wherein the support is a first support, and the component further comprises:
the nanocomposite on a second support; and
a separator between the first and the second support, wherein the separator includes an electrolyte.

### Claim 17 (depends on 15)

The component as recited in claim 15, wherein:
the nanocomposite includes ruthenium oxide nanoparticles.

### Claim 18 (depends on 15)

The component as recited in claim 15, wherein the support is a first support, and the component further comprises:
the nanocomposite on a second support; and
a separator between the first and the second support, wherein the separator includes polypropylene and a solution including sulfuric acid.

### Claim 19 (depends on 15)

The component as recited in claim 15, wherein the support is a first support, and the component further comprises:
the nanocomposite on a second support;
a separator on a first side of the first support and on a first side of the second support, wherein the separator includes polypropylene and a solution including sulfuric acid;
a first contact on a second side of the first support; and
a second contact on a second side of the second support.

### Claim 20 (depends on 15)

The component as recited in claim 15, wherein the support is a first support, and the component further comprises:
the nanocomposite on a second support;
a separator on a first side of the first support and on a first side of the second support, wherein the separator includes polypropylene and a solution including sulfuric acid;
a first contact on a second side of the first support;
a second contact on a second side of the second support;
a third support on the first contact;
a fourth support on the second contact; and
a clamp on the third and fourth support.