# US 2013/0155571 A1 · Dielectric thin film-forming composition, method of forming dielectric thin film and dielectric thin film formed by the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155571 A1
- Document ID: US20130155571A1
- Status: Published application
- Kind: A1
- Application number: 13/716,544
- Filed: 2012-12-17
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: STMicroelectronics (Tours) SAS; Mitsubishi Materials Corporation
- Inventors: Toshiaki Watanabe; Hideaki Sakurai; Nobuyuki Soyama; Guillaume Guegan
- Web page: https://patentgrep.com/patent/US20130155571A1

## CPC

- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- H01B 3/10: metallic oxides (ceramics H01B3/12)
- H01G 4/33: Thin- or thick-film capacitors {(thin- or thick-film circuits; capacitors without a potential-jump or surface barrier specially adapted for integrated circuits, details thereof, multistep manufacturing processes therefor)}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A liquid composition is provided for forming a thin film in the form of a mixed composite metal oxide in which a composite oxide B containing copper (Cu) and a composite oxide C containing manganese (Mn) are mixed into a composite metal oxide A represented with the general formula: Ba1-xSrxTiyO3, wherein the molar ratio B/A of the composite oxide B to the composite metal oxide A is within the range of 0.002<B/A<0.05, and the molar ratio C/A of the composite oxide C to the composite metal oxide A is within the range of 0.002<C/A<0.03.

## Claims

### Claim 1

A dielectric thin film-forming composition for forming a BST dielectric thin film, comprising:
a liquid composition for forming a thin film in the form of a mixed composite metal oxide in which a composite oxide B containing copper (Cu) and a composite oxide C containing manganese (Mn) are mixed into a composite metal oxide A represented with the general formula: Ba1-xSrxTiyO3 (wherein, 0.2<x<0.6 and 0.9<y’1.1); wherein,
the liquid composition is composed of an organic metal compound solution in which the raw material for composing the composite metal oxide A, the raw material for composing the composite oxide B and the raw material for composing the composite oxide C are dissolved in an organic solvent at a ratio so as to yield the metal atomic ratio indicated in the aforementioned general formula, and so that the molar ratio B/A of the composite oxide B to the composite metal oxide A is within the range of 0.002<B/A<0.05, and the molar ratio C/A of the composite oxide C to the composite metal oxide A is within the range of 0.002<C/A<0.03.

### Claim 2 (depends on 1)

The dielectric thin film-forming composition according to claim 1, wherein the raw material for composing the composite metal oxide A is a compound in which an organic group is bonded to a metal element through an oxygen atom or nitrogen atom thereof.

### Claim 3 (depends on 2)

The dielectric thin film-forming composition according to claim 2, wherein the raw material for composing the composite metal oxide A is at least one compound selected from the group consisting of a metal alkoxide, metal-diol complex, metal-triol complex, metal carboxylate, metal-β-diketonate complex, metal-β-diketoester complex, metal-β-iminoketo complex and a metal-amino complex.

### Claim 4 (depends on 1)

The dielectric thin film-forming composition according to claim 1, wherein the raw material for composing the composite oxide B is a compound in which an organic group is bonded to elemental copper (Cu) through an oxygen atom or nitrogen atom thereof.

### Claim 5 (depends on 4)

The dielectric thin film-forming composition according to claim 4, wherein the raw material for composing the composite oxide B is at least one compound selected from the group consisting of a carboxylate compound, nitrate compound, alkoxide compound, diol compound, triol compound, β-diketonate compound, β-diketoester compound, β-iminoketo compound and amino compound.

### Claim 6 (depends on 5)

The dielectric thin film-forming composition according to claim 5, wherein the carboxylate compound is copper naphthenate, copper n-octanoate, copper 2-ethylhexanoate, copper n-heptanoate, copper n-hexanoate, copper 2-ethylbutyrate, copper n-valerate, copper i-valerate, copper n-butyrate, copper i-butyrate or copper propionate.

### Claim 7 (depends on 5)

The dielectric thin film-forming composition according to claim 5, wherein the nitrate compound is copper nitrate.

### Claim 8 (depends on 1)

The dielectric thin film-forming composition according to claim 1, wherein the raw material for composing the composite oxide C is a compound in which an organic group is bonded to elemental manganese (Mn) through an oxygen atom or nitrogen atom thereof.

### Claim 9 (depends on 8)

The dielectric thin film-forming composition according to claim 8, wherein the raw material for composing the composite oxide C is at least one compound selected from the group consisting of a carboxylate compound, nitrate compound, alkoxide compound, diol compound, triol compound, β-diketonate compound, β-diketoester compound, β-iminoketo compound and amino compound.

### Claim 10 (depends on 1)

The dielectric thin film-forming composition according to claim 1, further containing at least one stabilizers, selected from the group consisting of a β-diketone, β-ketonic acid, β-ketoester, oxy acid, diol, triol, higher carboxylic acid, alkanolamine and polyvalent amine, at a ratio of 0.2 to 3 moles to 1 mole of the total amount of metal in the composition.

### Claim 11 (depends on 1)

The dielectric thin film-forming composition according to claim 1, wherein the molar ratio B/A of the composite oxide B to the composite metal oxide A is 0.003≦B/A≦0.03.

### Claim 12 (depends on 1)

The dielectric thin film-forming composition according to claim 1, wherein the molar ratio C/A of the composite oxide C to the composite metal oxide A is 0.003≦C/A≦0.02.

### Claim 13 (depends on 1)

A method of forming a dielectric thin film, comprising the steps of:
repeating a step for coating and drying the dielectric thin film-forming composition according to claim 1 on a heat-resistant substrate until a film of a desired thickness is obtained, followed by baking the film at a temperature equal to or higher than the crystallization temperature in air, in an oxidizing atmosphere or in a water vapor-containing atmosphere.

### Claim 14 (depends on 13)

A BST dielectric thin film containing Cu and Mn formed according to the method according to claim 13.

### Claim 15 (depends on 14)

The BST dielectric thin film containing Cu and Mn according to claim 14, wherein a thin film capacitor is formed having a dielectric thin film having a film thickness within the range of 100 to 500 nm as a dielectric layer, and the thin film capacitor has a leak current density of 1.0 μA/cm2 or less, tunability of 80% or more and dielectric loss of 0.0050 or less when a voltage of 20 V is applied thereto.

### Claim 16 (depends on 15)

A composite electronic component of a thin film capacitor, capacitor, IPD, DRAM memory capacitor, multilayer capacitor, transistor gate insulator, non-volatile memory, pyroelectric infrared sensor, piezoelectric element, electro-optical element, actuator, resonator, ultrasonic motor or LC noise filter element having the dielectric thin film according to claim 15.

### Claim 17 (depends on 16)

A composite electronic component of a thin film capacitor, capacitor, IPD, DRAM memory capacitor, multilayer capacitor, transistor gate insulator, non-volatile memory, pyroelectric infrared sensor, piezoelectric element, electro-optical element, actuator, resonator, ultrasonic motor or LC noise filter element having a dielectric thin film corresponding to a frequency band of 100 MHz or more according to claim 16.