# US 2013/0155517 A1 · Optical film and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155517 A1
- Document ID: US20130155517A1
- Status: Published application
- Kind: A1
- Application number: 13/713,282
- Filed: 2012-12-13
- Published: 2013-06-20
- Earliest claimed: 2011-12-15
- Inventors: Kyoung Gon PARK; Ki Yong KIM; Su Kyong LEE; Mi Jeong CHOI
- Web page: https://patentgrep.com/patent/US20130155517A1

## CPC

- G02B 5/021: {the diffusion taking place at the element's surface, e.g. by means of surface roughening or microprismatic structures}
- G02B 5/0221: {the surface having an irregular structure (G02B5/0226 takes precedence)}
- G02B 5/0268: {characterized by the fabrication or manufacturing method}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

An optical film including a base film, a light spreading pattern on a first surface of the base film, a surface of the light spreading pattern facing away from the base film being an undulating surface, and a light collecting pattern on a second surface of the base film.

## Claims

### Claim 1

An optical film, comprising:
a base film;
a light spreading pattern on a first surface of the base film, the light spreading pattern including no light spreading particles; and
a light collecting pattern on a second surface of the base film.

### Claim 2 (depends on 1)

The optical film as claimed in claim 1, wherein the light spreading pattern has an average haze value ranging from about 1% to about 99%.

### Claim 3 (depends on 1)

The optical film as claimed in claim 1, wherein the light spreading pattern has a standard deviation of the haze value of about 1.5%.

### Claim 4 (depends on 1)

The optical film as claimed in claim 1, wherein the light spreading pattern has a surface roughness Ra from about 0.01 μm to about 2 μm.

### Claim 5 (depends on 1)

The optical film as claimed in claim 1, wherein the light collecting pattern has a brightness uniformity of about 80% or more.

### Claim 6 (depends on 1)

The optical film as claimed in claim 1, wherein the light spreading pattern consists of a curable resin.

### Claim 7 (depends on 1)

The optical film as claimed in claim 1, wherein the light spreading pattern is an undulated pattern.

### Claim 8

An optical film, comprising:
a base film;
a light spreading pattern on a first surface of the base film, a surface of the light spreading pattern facing away from the base film being an undulating surface; and
a light collecting pattern on a second surface of the base film.

### Claim 9

A method of manufacturing an optical film, the method comprising:
forming an undulating pattern on a mold;
transferring the undulating pattern from the mold to a first side of a base film to form a light spreading pattern; and
forming a light collecting pattern on a second surface of the base film.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein forming the undulating pattern on the mold includes:
using a metal roll as the mold, the metal roll including at least one of steel, aluminum, and alloys thereof; and
coating a first coating layer on the metal roll, the first coating layer including at least one of nickel, copper, chromium, aluminum, alloys thereof, ceramic, and DLC.

### Claim 11 (depends on 10)

The method as claimed in claim 10, further comprising coating a second coating layer on the first coating layer.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein coating the second coating layer includes coating on the first coating layer at least one of nickel, copper, chromium, aluminum, alloys thereof, and ceramic.

### Claim 13 (depends on 9)

The method as claimed in claim 9, wherein the undulating pattern of the mold is formed by sand-blasting, etching, laser processing, or drilling the mold.

### Claim 14 (depends on 13)

The method as claimed in claim 13, wherein the undulating pattern of the mold is formed by sand-blasting the mold, the sand-blasting being performed about 1˜50 times using beads.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the beads are prepared by mixing one or more types of particles having an average particle diameter of about 0.1 μm to about 1,000 μm.

### Claim 16 (depends on 14)

The method as claimed in claim 14, wherein the beads are organic beads including at least one of polyester resins, olefin resins, acrylic resins, urethane resins, acryl-urethane resins, epoxy resins and silicone resins, inorganic beads including at least one of glass and ceramic, or composite beads of organic and inorganic beads.

### Claim 17 (depends on 9)

The method as claimed in claim 9, wherein the base film is formed of at least one of polyester resins, olefin resins, acrylic resins, urethane resins, acryl-urethane resins, epoxy resins, and silicone resins.

### Claim 18 (depends on 9)

The method as claimed in claim 9, wherein the base film is formed to have a thickness ranging from about 10 μm to about 1,000 μm.

### Claim 19 (depends on 9)

The method as claimed in claim 9, wherein forming the light spreading pattern on the base film includes:
coating a curable resin on the base film;
pressing the undulating pattern into the curable resin; and
curing the curable resin, such that the light spreading pattern is formed of the curable resin.

### Claim 20 (depends on 9)

The method as claimed in claim 9, wherein the light spreading pattern is formed to include no light spreading particles.