# US 2013/0155507 A1 · Plastic polarized lens, method for producing the same, and polarized film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155507 A1
- Document ID: US20130155507A1
- Status: Published application
- Kind: A1
- Application number: 13/813,312
- Filed: 2011-08-10
- Published: 2013-06-20
- Earliest claimed: 2010-08-12
- Assignees: Mitsui Chemicals, Inc.
- Inventors: Akinori Ryu; Seiichi Kobayashi; Hiroyuki Kamio; Yoshiharu Kobayashi; Mitsuru Sakai; Yoshimitsu Aiiso
- Web page: https://patentgrep.com/patent/US20130155507A1

## CPC

- G02B 1/08: made of polarising materials
- B29C 33/10: with incorporated venting means
- B29C 39/10: incorporating preformed parts or layers, e.g. casting around inserts or for coating articles {(coating a surface by casting in general B05D1/30, B29C39/126 takes precedence)}
- B29C 39/12: Making multilayered or multicoloured articles {(B29C39/021 takes precedence)}
- C09B 47/00: Porphines; Azaporphines {(non-dyeing compounds C07D487/22)}
- G02B 1/041: {Lenses}
- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- B29K 2075/00: Use of {PU, i.e.} polyureas or polyurethanes {or derivatives thereof}, as moulding material
- B29K 2995/0034: Polarising
- G02B 2207/113: Fluorescence
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C09B: ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES {, e.g. PIGMENTS}; MORDANTS; LAKES (fermentation or enzyme using processes to synthesise a desired chemical compound C12P)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The plastic polarized lens (10) of the present invention contains a polarized film (12) and layers (resin layers) (14a and 14b) comprising a thiourethane-based resin stacked over both surfaces of the polarized film (12), and the polarized film contains an organic coloring compound represented by the following general formula (1).

## Claims

### Claim 1

A plastic polarized lens comprising:
a polarized film and
layers comprising a thiourethane-based resin stacked over both surfaces of the polarized film,
wherein the polarized film contains an organic coloring compound represented by the following general formula (1):
wherein A1 to A8 each independently represent a hydrogen atom, a halogen atom, a nitro group, a cyano group, a hydroxy group, an amino group, a carboxyl group, a sulfone group, a linear, branched, or cyclic alkyl group having 1 to 20 carbon atoms, an alkoxy group having 1 to 20 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, a monoalkylamino group having 1 to 20 carbon atoms, a dialkylamino group having 2 to 20 carbon atoms, an aralkyl group having 7 to 20 carbon atoms, an aryl group having 6 to 20 carbon atoms, a heteroaryl group, an alkylthio group having 1 to 20 carbon atoms, or an arylthio group having 1 to 20 carbon atoms, or may form a ring other than an aromatic ring through a linking group, and M represents two hydrogen atoms, a divalent metal atom, a trivalent mono-substituted metal atom, a tetravalent di-substituted metal atom, or an oxy metal.

### Claim 2 (depends on 1)

The plastic polarized lens according to claim 1, wherein the organic coloring compound is represented by the following general formula (1a):
wherein t-C4H9 represents a tertiary butyl group, four tertiary butyl groups correspond to A1 or A2, A3 or A4, A5 or A6, and A7 or A8, respectively in the formula (1), and represent a position isomer structure, four groups that are not tertiary butyl groups in A1 to A8 represent a hydrogen atom; M represents a divalent copper atom, a divalent palladium atom, or divalent vanadium oxide (—V(═O)—).

### Claim 3 (depends on 1)

The plastic polarized lens according to claim 1, wherein the polarized film is comprised of a thermoplastic polyester.

### Claim 4 (depends on 1)

The plastic polarized lens according to claim 1, wherein the organic coloring compound is contained in the amount of 50 to 7000 ppm in the polarized film.

### Claim 5 (depends on 1)

The plastic polarized lens according to claim 1, wherein the thiourethane-based resin is obtained by reacting
(A) at least one kind of isocyanate compounds selected from the group consisting of a polyisocyanate compound, an isocyanate compound having an isothiocyanate group, and a polyisothiocyanate compound with
(B) at least one kind of active hydrogen compounds selected from the group consisting of thiol compounds and polythiol compounds having a hydroxy group.

### Claim 6 (depends on 3)

The plastic polarized lens according to claim 3, wherein the polarized film is shaped under the condition of the temperature T1 represented by the following formula:
Glass transition temperature of the thermoplastic polyester+20° C.≦T1≦Glass transition temperature of the thermoplastic polyester+120° C.

### Claim 7 (depends on 1)

The plastic polarized lens according to claim 1, wherein the formation of the adhesive layer or surface modification treatment of the adhesive layer is carried over at least one surface of the polarized film.

### Claim 8 (depends on 3)

The plastic polarized lens according to claim 3, wherein the thermoplastic polyester is a polyethylene terephthalate.

### Claim 9 (depends on 5)

The plastic polarized lens according to claim 5, wherein the isocyanate compound (A) is a diisocyanate compound and the active hydrogen compound (B) is a polythiol compound.

### Claim 10 (depends on 5)

The plastic polarized lens according to claim 5, wherein the isocyanate compound (A) is at least one kind of diisocyanate compound selected from the group consisting of 2,5-bis(isocyanatomethyl)bicyclo-[2.2.1]-heptane, 2,6-bis(isocyanatomethyl)bicyclo-[2.2.1]-heptane, and m-xylylene diisocyanate, and
the active hydrogen compound (B) is at least one kind of polythiol compound selected from the group consisting of pentaerythritoltetrakis(3-mercaptopropionate), 4-mercaptomethyl-1,8-dimercapto-3,6-dithiaoctane, 5,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 4,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, and 4,8-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane.

### Claim 11 (depends on 1)

The plastic polarized lens according to claim 1, wherein the refractive index at e-line of the thiourethane-based resin is in a range of 1.57 to 1.70.

### Claim 12 (depends on 1)

The plastic polarized lens according to claim 1, wherein the refractive index at e-line of the thiourethane-based resin is in a range of 1.59 to 1.70.

### Claim 13

A method of producing a plastic polarized lens, comprising:
producing a resin film containing an organic coloring compound represented by the following general formula (1);
shaping the resin film to obtain a polarized film;
fixing the polarized film in a lens casting mold in a state in which the polarized film is apart from the mold;
injecting a monomer mixture into the space between both surfaces of the polarized film and the mold; and
stacking layers comprising a thiourethane-based resin over both surfaces of the polarized film by polymerizing and curing the monomer mixture:
wherein A1 to A8 each independently represent a hydrogen atom, a halogen atom, a nitro group, a cyano group, a hydroxy group, an amino group, a carboxyl group, a sulfone group, a linear, branched, or cyclic alkyl group having 1 to 20 carbon atoms, an alkoxy group having 1 to 20 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, a monoalkylamino group having 1 to 20 carbon atoms, a dialkylamino group having 2 to 20 carbon atoms, an aralkyl group having 7 to 20 carbon atoms, an aryl group having 6 to 20 carbon atoms, a heteroaryl group, an alkylthio group having 1 to 20 carbon atoms, or an arylthio group having 1 to 20 carbon atoms, or may form a ring other than an aromatic ring through a linking group, and M represents two hydrogen atoms, a divalent metal atom, a trivalent mono-substituted metal atom, a tetravalent di-substituted metal atom, or an oxy metal).

### Claim 14 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, wherein the organic coloring compound is represented by the following general formula (1a):
wherein t-C4H9 represents a tertiary butyl group, four tertiary butyl groups correspond to A1 or A2, A3 or A4, A5 or A6, and A7 or A8, respectively, in the formula (1), and represent a position isomer structure, four groups that are not tertiary butyl groups in A1 to A8 represent a hydrogen atom; M represents a divalent copper atom, a divalent palladium atom, or divalent vanadium oxide (—V(═O)—).

### Claim 15 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, wherein the resin film is a thermoplastic polyester film.

### Claim 16 (depends on 15)

The method of producing a plastic polarized lens according to claim 15, wherein the shaping the resin film includes:
shaping the thermoplastic polyester film under the temperature condition of the glass transition temperature of the thermoplastic polyester+20° C. or higher and the glass transition temperature+120° C. or lower.

### Claim 17 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, wherein the monomer mixture includes:
(A) at least one kind of isocyanate compounds selected from the group consisting of a polyisocyanate compound, an isocyanate compound having an isothiocyanate group, and a polyisothiocyanate compound,
(B) at least one kind of active hydrogen compound selected from the group consisting of thiol compounds and polythiol compounds having a hydroxy group.

### Claim 18 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, further comprising:
subjecting at least one surface of the polarized film to a surface modification treatment before the fixing the polarized film.

### Claim 19 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, further comprising:
forming an adhesive layer over at least one surface of the polarized film before the fixing the polarized film.

### Claim 20 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, further comprising:
subjecting at least one surface of the polarized film to a surface modification treatment; and
forming an adhesive layer over the surface that has been subjected to a surface modification treatment,
before the fixing the polarized film.

### Claim 21 (depends on 15)

The method of producing a plastic polarized lens according to claim 15, wherein the thermoplastic polyester is a polyethylene terephthalate.

### Claim 22 (depends on 17)

The method of producing a plastic polarized lens according to claim 17, wherein the isocyanate compound (A) is a diisocyanate compound and the active hydrogen compound (B) is a polythiol compound.

### Claim 23 (depends on 17)

The method of producing a plastic polarized lens according to claim 17, wherein the isocyanate compound (A) is at least one kind of diisocyanate compounds selected from the group consisting of 2,5-bis(isocyanatomethyl)bicyclo-[2.2.1]-heptane, 2,6-bis(isocyanatomethyl)bicyclo-[2.2.1]-heptane, and m-xylylene diisocyanate, and
the active hydrogen compound (B) is at least one kind of polythiol compounds selected from the group consisting of pentaerythritoltetrakis(3-mercaptopropionate), 4-mercaptomethyl-1,8-dimercapto-3,6-dithiaoctane, 5,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, 4,7-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane, and 4,8-dimercaptomethyl-1,11-dimercapto-3,6,9-trithiaundecane.

### Claim 24 (depends on 13)

The method of producing a plastic polarized lens according to claim 13, wherein the viscosity at 20° C. of the monomer mixture is 200 mPa·s or less in the injecting step.

### Claim 25

A polarized film comprising a resin containing an organic coloring compound represented by the following general formula (1):
wherein A1 to A8 each independently represent a hydrogen atom, a halogen atom, a nitro group, a cyano group, a hydroxy group, an amino group, a carboxyl group, a sulfone group, a linear, branched, or cyclic alkyl group having 1 to 20 carbon atoms, an alkoxy group having 1 to 20 carbon atoms, an aryloxy group having 6 to 20 carbon atoms, a monoalkylamino group having 1 to 20 carbon atoms, a dialkylamino group having 2 to 20 carbon atoms, an aralkyl group having 7 to 20 carbon atoms, an aryl group having 6 to 20 carbon atoms, a heteroaryl group, an alkylthio group having 1 to 20 carbon atoms, or an arylthio group having 1 to 20 carbon atoms, or may form a ring other than an aromatic ring through a linking group, and M represents two hydrogen atoms, a divalent metal atom, a trivalent mono-substituted metal atom, a tetravalent di-substituted metal atom, or an oxy metal.

### Claim 26 (depends on 25)

The polarized film according to claim 25, wherein the organic coloring compound is represented by the following general formula (1a):
wherein t-C4H9 represents a tertiary butyl group, four tertiary butyl groups correspond to A1 or A2, A3 or A4, A5 or A6, and A7 or A8, respectively, in the formula (1), and represent a position isomer structure, four groups that are not tertiary butyl groups in A1 to A8 represent a hydrogen atom; M represents a divalent copper atom, a divalent palladium atom, or divalent vanadium oxide (—V(═O)—).

### Claim 27 (depends on 25)

The polarized film according to claim 25, wherein the resin is a thermoplastic polyester.

### Claim 28 (depends on 25)

The polarized film according to claim 25, wherein the organic coloring compound is contained in the amount of 50 to 7000 ppm in the polarized film.

### Claim 29 (depends on 27)

The polarized film according to claim 27, wherein the thermoplastic polyester is a polyethylene terephthalate.

### Claim 30 (depends on 25)

The polarized film according to claim 25, which is used in a plastic polarized lens having layers comprising a thiourethane-based resin laminated over both surfaces of the polarized film.

### Claim 31 (depends on 30)

A method for producing the polarized film according to claim 30, comprising:
producing a resin film containing the organic coloring compound; and
shaping the resin film.

### Claim 32 (depends on 31)

The method for producing the polarized film according to claim 31, wherein the resin film is a thermoplastic polyester film.

### Claim 33 (depends on 32)

The method for producing the polarized film according to claim 32, wherein the shaping the resin film includes:
shaping the thermoplastic polyester film under the temperature condition of the glass transition temperature of the thermoplastic polyester+20° C. or higher and the glass transition temperature+120° C. or lower.