# US 2013/0155155 A1 · Liquid ejecting head, liquid ejecting apparatus, and piezoelectric element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0155155 A1
- Document ID: US20130155155A1
- Status: Published application
- Kind: A1
- Application number: 13/718,053
- Filed: 2012-12-18
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: Seiko Epson Corporation
- Inventors: Hidemichi FURIHATA
- Web page: https://patentgrep.com/patent/US20130155155A1

## CPC

- B41J 2/14233: {of film type, deformed by bending and disposed on a diaphragm}
- B41J 2/161: {of film type, deformed by bending and disposed on a diaphragm}
- B41J 2/1623: {bonding and adhesion}
- B41J 2/1628: {dry etching}
- B41J 2/1629: {wet etching}
- B41J 2/1635: {dividing the wafer into individual chips}
- B41J 2/1642: {thin film formation by CVD [chemical vapor deposition]}
- B41J 2/1645: {thin film formation by spincoating}
- B41J 2/1646: {thin film formation by sputtering}
- B41J 2002/14241: {having a cover around the piezoelectric thin film element}
- B41J 2002/14419: {Manifold}
- B41J 2002/14491: {Electrical connection}
- B41J 2202/03: Specific materials used
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS

## Abstract

A liquid ejecting head contains a piezoelectric element having a piezoelectric layer and an electrode disposed on the piezoelectric layer, in which the piezoelectric layer contains a complex oxide containing bismuth, iron, barium, and titanium and having a perovskite structure, has a yield stress of 5.66 GPa or more, and has a Young's modulus of 114 GPa or more.

## Claims

### Claim 1

A liquid ejecting head, comprising:
a piezoelectric element having a piezoelectric layer and an electrode disposed on the piezoelectric layer,
the piezoelectric layer containing a complex oxide containing bismuth, iron, barium, and titanium and having a perovskite structure, having a yield stress of 5.66 GPa or more, and having a Young's modulus of 114 GPa or more.

### Claim 2 (depends on 1)

A liquid ejecting apparatus, comprising:
the liquid ejecting head according to claim 1.

### Claim 3

A piezoelectric element, comprising:
a piezoelectric layer; and
an electrode disposed on the piezoelectric layer,
the piezoelectric layer containing a complex oxide containing bismuth, iron, barium, and titanium and having a perovskite structure, having a yield stress of 5.66 GPa or more, and having a Young's modulus of 114 GPa or more.