# US 2013/0154051 A1 · Method for forming a deep trench in a microelectronic component substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0154051 A1
- Document ID: US20130154051A1
- Status: Published application
- Kind: A1
- Application number: 13/713,135
- Filed: 2012-12-13
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: STMicroelectronics (Crolles 2) SAS
- Inventors: Arnaud Tournier; François Leverd
- Web page: https://patentgrep.com/patent/US20130154051A1

## CPC

- H10P 50/244: {comprising alternated and repeated etching and passivation steps}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10W 10/0148: {comprising introducing impurities in side walls or bottom walls of trenches, e.g. for forming channel stoppers}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A trench is formed in a semiconductor substrate by depositing an etch mask on the substrate having an opening, etching of the trench through the opening, and doping the walls of the trench. The etching step includes a first phase having an etch power set to etch the substrate under the etch mask, and a second phase having an etch power set smaller than the power of the first phase. Further, the doping of the walls of the trench is applied through the opening of the etch mask.

## Claims

### Claim 1

A method for forming a trench in a semiconductor substrate around an area of a microelectronic element, wherein the geometry of said area defines properties of the microelectronic element, and wherein said area is located in a predetermined thickness of the semiconductor substrate from a surface thereof, said method comprising the deposition on said surface of the substrate of an etch mask masking said area and having an opening of access to the substrate around said area, the ion etching of said trench through said opening over a thickness of the substrate greater than the thickness of said area, and the doping of the walls of the trench, wherein the ion etching comprises:
a first phase etching the trench over the thickness of said area, with an etch power set to etch the substrate under the etch mask;
followed by a second phase etching the trench over the entire thickness thereof, with an etch power smaller than the power of the first phase; and
the doping of the walls of the trench is applied through the opening of the etch mask.

### Claim 2 (depends on 1)

The method of claim 1, wherein the ion etching comprises successive elementary cycles, each etching a portion of the trench, each cycle comprising:
a deposition of a passivation layer on the internal walls of the trench portion etched during previous cycles; and
an anisotropic pulsed plasma ion etching of the trench portion etched during previous cycles; and
the thickness of the passivation layers deposited during the first phase is smaller than the thickness of the passivation layers deposited during the second phase.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ion etching comprises successive elementary cycles, each etching a portion of the trench, each cycle comprising:
a deposition of a passivation layer on the internal walls of the trench portion etched during previous cycles; and
an anisotropic pulsed plasma ion etching of the trench portion etched during previous cycles; and
in that the power of the plasma during the first phase is smaller than the power of the plasma during the second phase.

### Claim 4 (depends on 1)

The method of claim 1, wherein the ion etching comprises successive elementary cycles, each etching a portion of the trench, each cycle comprising:
a deposition of a passivation layer on the internal walls of the trench portion etched during previous cycles; and
an anisotropic pulsed plasma ion etching of the trench portion etched during previous cycles; and
in that the time of application of the plasma ion etching of the elementary cycles of the first phase is shorter than the time of application of the plasma ion etching of the elementary cycles of the second phase.

### Claim 5 (depends on 1)

The method of claim 1, wherein the ion etching comprises successive elementary cycles, each etching a portion of the trench, each cycle comprising:
a deposition of a passivation layer on the internal walls of the trench portion etched during previous cycles; and
an anisotropic pulsed plasma ion etching of the trench portion etched during previous cycles; and
in that the amount of etch gas used during the first phase is greater than the amount of etch gas used during the second phase.

### Claim 6 (depends on 2)

The method of claim 2, wherein the plasma ion etching of the elementary cycles is performed in an atmosphere comprising a passivating species, and comprises at least one first etch sequence followed by a second etch sequence with a power smaller than the power of the first etch sequence.

### Claim 7 (depends on 1)

The method of claim 1, wherein the ion etching is a fluorinated plasma ion etching, and in that the fluorine proportion during the first phase is greater than the fluorine proportion during the second phase.

### Claim 8 (depends on 1)

The method of claim 1, wherein the ion etching is an ion etching with a plasma based on fluorinated compounds selected from the group comprising CF4, CH2F4, C4F8, C5F8, C3F6, SF6, NF3.

### Claim 9 (depends on 1)

The method of claim 1, wherein the etch mask is made of nitride.

### Claim 10 (depends on 1)

The method of claim 1, wherein the trench surrounds an active area of a photodetector, especially CMOS.

### Claim 11

A method, comprising:
depositing a mask over a top surface of a substrate, said mask having an opening;
performing a first etching of the substrate through the opening in the mask to produce a first etched region, said first etching performed at a first etching power such that the first etched region extends underneath the mask to leave a mask overhang;
performing a second etching of the substrate through the opening in the mask to produce a second etched region below the first etched region, said second etching performed at a second etching power less than the first etching power; and
doping sidewalls of the first and second etched regions through the opening in the mask, the mask overhang limiting a thickness of the doped sidewalls of the first etched region near the top surface of the substrate.

### Claim 12 (depends on 11)

The method of claim 11, wherein each of the first and second etching comprises performing successive etch cycles, each etch cycle comprising:
depositing a passivation layer on the internal walls of a trench portion etched during a previous cycle; and
anisotropic pulsed plasma ion etching of the trench portion etched during previous cycles.

### Claim 13 (depends on 12)

The method of claim 12, wherein a thickness of the passivation layer deposited during the first etching is smaller than the thickness of the passivation layer deposited during the second etching.

### Claim 14 (depends on 12)

The method of claim 12, wherein the power of the plasma during the first etching is less than the power of the plasma during the second etching.

### Claim 15 (depends on 12)

The method of claim 12, wherein a time of application of the plasma ion etching of the etch cycles of the first etching is shorter than the time of application of the plasma ion etching of the etch cycles of the second etching.

### Claim 16 (depends on 12)

The method of claim 12, wherein an amount of etch gas used during the first etching is greater than the amount of etch gas used during the second etching.

### Claim 17

A semiconductor structure, comprising:
a substrate including an isolating trench structure;
the isolating trench structure comprising a first etched region having a first sidewall with a first slope and a second etched region extending below the first etched region having a second sidewall with a second slope different from the first slope; and
doped regions of the first and second sidewalls, wherein the doped region of the first sidewall is tapered with a doped thickness widest at a bottom of the first etched region adjacent the second etched region and narrowest at a top of the first etched region adjacent a top surface of the substrate.

### Claim 18 (depends on 17)

The semiconductor structure of claim 17, wherein the doped region of the second sidewall is tapered with a doped thickness widest at a top of the second etched region adjacent the first etched region and narrowest at a bottom of the second etched region adjacent a bottom of the isolating trench structure.