# US 2013/0153963 A1 · Gated iii-v semiconductor structure and method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0153963 A1
- Document ID: US20130153963A1
- Status: Published application
- Kind: A1
- Application number: 13/389,127
- Filed: 2011-06-22
- Published: 2013-06-20
- Earliest claimed: 2010-06-23
- Assignees: Cornell University
- Inventors: James R. Shealy; Richard Brown
- Web page: https://patentgrep.com/patent/US20130153963A1

## CPC

- H10D 30/47: having two-dimensional [2D] charge carrier gas channels, e.g. nanoribbon FETs or high electron mobility transistors [HEMT]
- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/475: {having wider bandgap layer formed on top of lower bandgap active layer, e.g. undoped barrier HEMTs such as i-AlGaN/GaN HEMTs}
- H10P 32/12: between a solid phase and a gaseous phase
- H10P 32/174: {being Group III-V material}
- H10W 74/43: comprising oxides, nitrides or carbides, e.g. ceramics or glasses
- H10D 62/343: {Gate regions of field-effect devices having PN junction gates}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10W 74/137: {the encapsulations being directly on the semiconductor body (H10W74/134 takes precedence)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A gated III-V semiconductor structure and a method for fabricating the gated III-V semiconductor structure includes a threshold modifying dopant region within a III-V semiconductor barrier layer at the base of an aperture through a passivation layer that otherwise passivates the III-V semiconductor barrier layer. The passivation layer, which may comprise an aluminum-silicon nitride material, has particular bandgap and permittivity properties that provide for enhanced performance of a III-V semiconductor device that derives from the III-V semiconductor structure absent a field plate. The threshold modifying dopant region provides the possibility for forming both an enhancement mode gated III-V semiconductor structure and a depletion mode III-V semiconductor structure on the same substrate. The threshold modifying dopant region when comprising a magnesium (Mg) threshold modifying dopant may be incorporated into the gates III-V semiconductor structure using a dicyclopentadienyl magnesium (Cp2Mg) vapor diffusion method or a magnesium-silicon nitride (MgSiN) solid state diffusion method.

## Claims

### Claim 1

A semiconductor structure comprising:
a barrier layer comprising a first III-V semiconductor material located upon a buffer layer comprising a second III-V semiconductor material different than the first III-V semiconductor material in turn located over a substrate;
a passivation layer comprising an aluminum-silicon nitride material located upon the barrier layer and including an aperture that exposes a threshold modifying dopant region located within the barrier layer;
a gate contacting the threshold modifying dopant region located within the barrier layer.

### Claim 2 (depends on 1)

The semiconductor structure of claim 1 wherein the semiconductor structure does not include a field plate.

### Claim 3

A semiconductor structure comprising:
a barrier layer comprising a first III-V semiconductor material located upon a buffer layer comprising a second III-V semiconductor material different than the first III-V semiconductor material in turn located over a substrate;
a passivation layer located upon the barrier layer and including an aperture that exposes a threshold modifying dopant region located within the barrier layer;
a gate contacting the threshold modifying dopant region within the barrier layer, where at least a portion of the passivation layer located upon the barrier layer comprises a passivation material having a bandgap from about 4.5 to about 6 eV and a permittivity from about 6×10̂-11 F/m to about 8×10̂-11 F/m at a frequency from about 1 to about 100 GHz.

### Claim 4 (depends on 3)

The semiconductor structure of claim 3 further comprising a source contact and a drain contact located laterally separated by the gate and also penetrating through the passivation layer and contacting the barrier layer, but not the threshold modifying dopant region within the barrier layer.

### Claim 5 (depends on 3)

The semiconductor structure of claim 3 wherein the passivation material having the bandgap from about 4.5 to about 6 eV and the permittivity from about 6×10̂-11 F/m to about 8×10̂-11 F/m at a frequency from about 1 to about 100 GHz comprises an aluminum-silicon nitride passivation material.

### Claim 6 (depends on 3)

The semiconductor structure of claim 3 wherein each of the buffer layer and the barrier layer comprises a III-V semiconductor material other than a group III nitride semiconductor material.

### Claim 7 (depends on 3)

The semiconductor structure of claim 3 wherein each of the buffer layer and the barrier layer comprises a group III nitride semiconductor material.

### Claim 8 (depends on 3)

The semiconductor structure of claim 3 wherein the threshold modifying dopant region includes a threshold modifying dopant selected from the group consisting of magnesium and beryllium threshold modifying dopants.

### Claim 9 (depends on 3)

The semiconductor structure of claim 3 wherein the semiconductor structure does not include a field plate.

### Claim 10

A semiconductor structure comprising:
a barrier layer comprising a first III-V semiconductor material located upon a buffer layer comprising a second III-V semiconductor material different than the first III-V semiconductor material in turn located over a substrate;
a passivation layer located upon the barrier layer and including an aperture that exposes symmetrically aligned with the aperture a threshold modifying dopant region within the barrier layer;
a source contact and a drain contact separated by the aperture and penetrating through the passivation layer and contacting the barrier layer but not the threshold modifying dopant region within the barrier layer;
a gate located in the aperture and contacting the threshold modifying dopant region within the barrier layer, where at least a portion of the passivation layer located upon the barrier layer comprises a passivation material having a bandgap from about 4.5 to about 6 eV and a permittivity from about 6×10̂-11 F/m to about 8×10̂-11 F/m at a frequency from about 1 to about 100 GHz.

### Claim 11 (depends on 10)

The semiconductor structure of claim 10 wherein the passivation material having the bandgap from about 4.5 to about 6 eV and the permittivity from about 6×10̂-11 F/m to about 8×10̂-11 F/m at a frequency from about 1 to about 100 GHz comprises an aluminum-silicon nitride passivation material.

### Claim 12 (depends on 10)

The semiconductor structure of claim 10 wherein each of the buffer layer and the barrier layer comprises a group III nitride semiconductor material.

### Claim 13 (depends on 10)

The semiconductor structure of claim 10 wherein the threshold modifying dopant region includes a threshold modifying dopant selected from the group consisting of magnesium and beryllium threshold modifying dopants.

### Claim 14 (depends on 10)

The semiconductor structure of claim 10 wherein the semiconductor structure does not include a field plate.

### Claim 15

A method for fabricating a semiconductor structure comprising:
forming a layered structure comprising:
a buffer layer comprising a first III-V semiconductor material formed over a substrate;
a barrier layer comprising a second III-V semiconductor material different from the first III-V semiconductor material formed upon the buffer layer; and
a passivation layer comprising an aluminum-silicon nitride passivation material formed upon the barrier layer;
patterning a portion of the passivation located upon the barrier layer to provide an aperture that exposes a portion of the barrier layer;
forming a threshold modifying dopant region into the barrier layer at the base of the aperture; and
forming a gate contacting the threshold modifying dopant region.

### Claim 16 (depends on 15)

The method of claim 15 wherein a field plate is not formed over the substrate.

### Claim 17

A method for fabricating a semiconductor structure comprising:
forming a layered structure comprising:
a buffer layer comprising a first III-V semiconductor material formed over a substrate;
a barrier layer comprising a second III-V semiconductor material different from the first III-V semiconductor material formed upon the buffer layer; and
a passivation layer comprising a passivation material having a bandgap from about 4.5 to about 6 eV and a permittivity from about 6×10̂-11 F/m to about 8×10̂-11 F/m at a frequency from about 1 to about 100 GHz upon the barrier layer;
patterning a portion of the passivation located upon the barrier layer to provide an aperture that exposes a portion of the barrier layer;
forming a threshold modifying dopant region into the barrier layer at the base of the aperture; and
forming a gate contacting the threshold modifying dopant region.

### Claim 18 (depends on 17)

The method of claim 17 wherein each of the first III-V semiconductor material and the second III-V semiconductor material layer comprises other than a group III nitride semiconductor material.

### Claim 19 (depends on 17)

The method of claim 17 wherein each of the first III-V semiconductor material and the second III-V semiconductor material comprises a group III nitride semiconductor material.

### Claim 20 (depends on 17)

The method of claim 17 wherein the forming the threshold modifying dopant region uses a vapor diffusion dopant source.

### Claim 21 (depends on 20)

The method of claim 20 wherein the vapor diffusion dopant source comprises dicyclopentadienyl magnesium.

### Claim 22 (depends on 17)

The method of claim 17 wherein the forming the threshold modifying dopant region uses a solid diffusion dopant source.

### Claim 23 (depends on 22)

The method of claim 22 wherein the solid diffusion dopant source comprises magnesium-silicon nitride.

### Claim 24 (depends on 17)

The method of claim 17 wherein the threshold modifying dopant region comprises a threshold modifying dopant selected from the group consisting of magnesium and beryllium threshold modifying dopants.