# US 2013/0153892 A1 · Semiconductor device and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0153892 A1
- Document ID: US20130153892A1
- Status: Published application
- Kind: A1
- Application number: 13/713,186
- Filed: 2012-12-13
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Toshinari SASAKI; Shuhei YOKOYAMA; Takashi HAMOCHI; Shunpei YAMAZAKI
- Web page: https://patentgrep.com/patent/US20130153892A1

## CPC

- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A highly reliable semiconductor device that includes a transistor including an oxide semiconductor is provided. In a semiconductor device which includes a bottom-gate transistor including an oxide semiconductor film, the spin density of the oxide semiconductor film is lower than or equal to 1×1018 spins/cm3, preferably lower than or equal to 1×1017 spins/cm3, further preferably lower than or equal to 1×1016 spins/cm3. The conductivity of the oxide semiconductor film is lower than or equal to 1×103 S/cm, preferably lower than or equal to 1×102 S/cm, further preferably lower than or equal to 1×101 S/cm.

## Claims

### Claim 1

A semiconductor device comprising:
a gate electrode layer;
a gate insulating film over the gate electrode layer;
an oxide semiconductor film over the gate insulating film;
source and drain electrode layers over the oxide semiconductor film; and
an oxide insulating film over the source and drain electrode layers, wherein the oxide insulating film is in contact with the oxide semiconductor film and contains nitrogen,
wherein a spin density of the oxide semiconductor film is lower than or equal to 1×1018 spins/cm3.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein conductivity of the oxide semiconductor film is lower than or equal to 1×103 S/cm.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein a spin density of the oxide semiconductor film is lower than or equal to 1×1017 spins/cm3.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein conductivity of the oxide semiconductor film is lower than or equal to 1×102 S/cm.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein the oxide semiconductor film comprises a material selected from indium, gallium, zinc, and a combination thereof.

### Claim 6 (depends on 1)

The semiconductor device according to claim 1, wherein at least one of the gate insulating film and the oxide insulating film comprises a silicon oxynitride film in contact with the oxide semiconductor film.

### Claim 7

A method for manufacturing a semiconductor device, comprising the steps of:
forming a gate electrode layer;
forming a gate insulating film over the gate electrode layer;
forming an oxide semiconductor film over the gate insulating film in a region overlapping with the gate electrode layer;
processing the oxide semiconductor film into an island-shaped oxide semiconductor layer;
forming source and drain electrode layers electrically connected to the island-shaped oxide semiconductor layer; and
forming an oxide insulating film containing nitrogen over the island-shaped oxide semiconductor layer and the source and drain electrode layers, wherein the oxide insulating film is in contact with the island-shaped oxide semiconductor layer,
wherein a spin density of the island-shaped oxide semiconductor layer is lower than or equal to 1×1018 spins/cm3.

### Claim 8 (depends on 7)

The method for manufacturing a semiconductor device, according to claim 7, wherein conductivity of the island-shaped oxide semiconductor layer is lower than or equal to 1×103 S/cm.

### Claim 9 (depends on 7)

The method for manufacturing a semiconductor device, according to claim 7, wherein a spin density of the island-shaped oxide semiconductor layer is lower than or equal to 1×1017 spins/cm3.

### Claim 10 (depends on 7)

The method for manufacturing a semiconductor device, according to claim 7, wherein conductivity of the island-shaped oxide semiconductor layer is lower than or equal to 1×102 S/cm.

### Claim 11 (depends on 7)

The method for manufacturing a semiconductor device, according to claim 7, wherein the oxide insulating film containing nitrogen is formed by a chemical vapor deposition method.

### Claim 12 (depends on 7)

The method for manufacturing a semiconductor device, according to claim 7, wherein the island-shaped oxide semiconductor layer comprises a material selected from indium, gallium, zinc, and a combination thereof.

### Claim 13 (depends on 7)

The method for manufacturing a semiconductor device, according to claim 7, wherein at least one of the gate insulating film and the oxide insulating film comprises a silicon oxynitride film in contact with the island-shaped oxide semiconductor layer.

### Claim 14

A method for manufacturing a semiconductor device, comprising the steps of:
forming a gate electrode layer over a substrate;
forming a gate insulating film over the gate electrode layer; and
forming an oxide semiconductor film over the gate insulating film in a region overlapping with the gate electrode layer by a sputtering method using an oxide target comprising indium, gallium, and zinc while heating the substrate,
wherein the oxide semiconductor film is a c-axis aligned crystalline oxide semiconductor layer, and
wherein a spin density of the oxide semiconductor film is lower than or equal to 1×1018 spins/cm3.

### Claim 15 (depends on 14)

The method for manufacturing a semiconductor device, according to claim 14, wherein conductivity of the oxide semiconductor film is lower than or equal to 1×103 S/cm.

### Claim 16 (depends on 14)

The method for manufacturing a semiconductor device, according to claim 14, wherein a spin density of the oxide semiconductor film is lower than or equal to 1×1017 spins/cm3.

### Claim 17 (depends on 14)

The method for manufacturing a semiconductor device, according to claim 14, wherein conductivity of the oxide semiconductor film is lower than or equal to 1×102 S/cm.

### Claim 18 (depends on 14)

The method for manufacturing a semiconductor device, according to claim 14, wherein the oxide target is a material with a ratio of In:Ga:Zn=1:1:1.

### Claim 19 (depends on 14)

The method for manufacturing a semiconductor device, according to claim 14, wherein the gate insulating film comprises a silicon oxynitride film in contact with the oxide semiconductor film.