# US 2013/0153866 A1 · Materials and methods for organic light-emitting device microcavity

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0153866 A1
- Document ID: US20130153866A1
- Status: Published application
- Kind: A1
- Application number: 13/528,896
- Filed: 2012-06-21
- Published: 2013-06-20
- Earliest claimed: 2011-06-21
- Assignees: Kateeva, Inc.
- Inventors: Jianglong CHEN; Ian MILLARD; Steven VAN SLYKE; Inna TREGUB; Conor MADIGAN
- Web page: https://patentgrep.com/patent/US20130153866A1

## CPC

- H10K 71/135: {using ink-jet printing}
- H10H 20/01: Manufacture or treatment
- H10K 59/876: {comprising a resonant cavity structure, e.g. Bragg reflector pair}
- H10K 71/40: Thermal treatment, e.g. annealing in the presence of a solvent vapour
- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10K 50/852: comprising a resonant cavity structure, e.g. Bragg reflector pair
- H10K 50/854: comprising scattering means
- H10K 71/13: using printing techniques, e.g. ink-jet printing or screen printing
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

The present teachings provide methods for forming organic layers for an organic light-emitting device (OLED) using an inkjet printing or thermal printing process. The method can further use one or more additional processes, such as vacuum thermal evaporation (VTE), to create an OLED stack. OLED stack structures are also provided wherein at least one of the charge injection or charge transport layers is formed by an inkjet printing or thermal printing method at a high deposition rate. The structure of the organic layer can be amorphous, crystalline, porous, dense, smooth, rough, or a combination thereof, depending on deposition parameters and post-treatment conditions. An OLED microcavity is also provided and can be formed by one of more of the methods.

## Claims

### Claim 1

A method of forming a microcavity for an organic light-emitting device, the method comprising:
depositing an ink from an inkjet printhead onto a substrate comprising a first reflective electrode, to form a printed layer, the ink being defined by a carrier and dissolved or suspended film-forming organic material;
driving off the carrier from the printed layer to form a first organic buffer layer on the substrate;
depositing a light-emitting organic material over the first organic buffer layer to form an emitting layer such that the first organic buffer layer is disposed between the substrate and the emitting layer, the light-emitting organic material emitting light, upon excitation, at a peak emission wavelength; and
depositing a second reflective electrode over the emitting layer such that the emitting layer is disposed between the first reflective electrode and the second reflective electrode, to form an OLED microcavity;
wherein at least one of the first and second reflective electrodes is semi-transparent, the first reflective electrode and the second reflective electrode are separated from one another by a distance, the distance corresponds to a depth of the microcavity, and the depth of the microcavity is configured for resonance emission of the peak emission wavelength.

### Claim 2 (depends on 1)

The method of claim 1, wherein the carrier fluid is driven off by at least one of a vacuum, heating, a gas stream, exposure to radiation, or a combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the emitting layer is spaced from the first reflective electrode by a first distance and spaced from the second reflective electrode by a second distance, and the first and second distances are optimized for maximum luminosity of the microcavity during operation.

### Claim 4 (depends on 1)

The method of claim 1, wherein the depositing an ink comprises depositing a liquid ink directly onto the first reflective electrode.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first organic emitting layer is deposited directly onto the buffer layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first organic buffer layer comprises at least one of a hole injection layer, a hole transport layer, an emission layer, an electron transport layer, and an electron injection layer.

### Claim 7 (depends on 1)

The method of claim 1, further comprising baking the first organic buffer layer at a first bake temperature of from about 50° C. to about 250° C. for a first bake time of from about 5.0 milliseconds to about 5.0 hours.

### Claim 8 (depends on 1)

The method of claim 1, further comprising baking the first organic buffer layer at a first bake temperature of from about 50° C. to about 250° C. for a first bake time of from about 5.0 milliseconds to about 5.0 hours, to form a first baked organic layer for an organic light-emitting device.

### Claim 9 (depends on 8)

The method of claim 8, wherein at least one of the bake temperature, the bake time, the concentration of the film-forming organic material in the ink, and the thickness of the first organic buffer layer, are adjusted such that the first baked organic layer exhibits a porous structure.

### Claim 10 (depends on 8)

The method of claim 8, wherein at least one of the bake temperature and bake time are adjusted so that the first baked organic layer exhibits a rough character.

### Claim 11 (depends on 8)

The method of claim 8, wherein at least one of the bake temperature and bake time are adjusted so that the first baked organic layer exhibits a smooth character.

### Claim 12 (depends on 11)

The method of claim 11, wherein at least one of the bake temperature, the bake time, the concentration of the film-forming organic material in the ink, and the thickness of the first organic buffer layer, are adjusted such that the first baked organic layer has a surface roughness of from about 0.5 nm to about 10 nm expressed as the root mean square of the surface thickness deviation in an area 10×10 μm2.

### Claim 13 (depends on 11)

The method of claim 11, wherein at least one of the bake temperature, the bake time, the concentration of the film-forming organic material in the ink, and the thickness of the first organic buffer layer, are adjusted such that the first baked organic layer has a surface roughness of less than 5.0 nm expressed as the root mean square of the surface thickness deviation in an area of 10×10 μm2.

### Claim 14 (depends on 1)

The method of claim 1, wherein the film-forming organic material exhibits a glass transition temperature range and the method further comprises baking the first organic buffer layer at a bake temperature of from within the glass transition temperature range to above the glass transition temperature range, to form a crystalline organic layer having a conductivity of from about 1.0×10−9 S/m to about 1.0×10−1 S/m.

### Claim 15 (depends on 14)

The method of claim 14, wherein the bake temperature is from about 250° C. to about 450° C. and the first organic buffer layer is heated at the bake temperature for a bake time of from about 5 milliseconds to about 5.0 hours

### Claim 16 (depends on 14)

The method of claim 14, wherein the crystalline organic layer has a crystallinity as measured by an average grain size of from about 0.5 nm to about 100 μm.

### Claim 17 (depends on 14)

The method of claim 14, wherein the crystalline organic layer comprises at least one of a hole injection layer, a hole transport layer, an emission layer, an electron transport layer, and an electron injection layer.

### Claim 18 (depends on 1)

The method of claim 1, further comprising:
depositing a second ink from an inkjet printhead to the first organic buffer layer, the second ink being defined by a second carrier and dissolved or suspended film-forming organic material; and
driving off the second carrier to form an organic material layer on the first organic buffer layer;
wherein the first reflective electrode is semi-transparent and the first organic buffer layer exhibits a refractive index that is intermediate between a refractive index of the substrate and a refractive index of the organic material layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the refractive index of the substrate is from about 1.01 to about 1.55 and the refractive index of the organic material layer is from about 1.60 to about 5.01.

### Claim 20 (depends on 1)

An organic light-emitting device (OLED) microcavity formed by the method of claim 1.

### Claim 21

A microcavity for an organic light-emitting device, the microcavity comprising:
a substrate comprising a first reflective electrode;
a dry film organic material layer formed on the substrate and comprising a first surface facing the substrate and a second surface opposite the first surface;
an emitting layer over the dry film organic material layer such that the dry film organic material layer is between the first reflective electrode and the emitting layer, the emitting layer comprising a light-emitting organic material that emits light, upon excitation, at a peak emission wavelength; and
a second reflective electrode over the emitting layer such that the emitting layer is between the first reflective electrode and the second reflective electrode,
wherein the second surface exhibits a surface roughness of from about 5.0 nm to about 1.0 μm as the root mean squared of surface thickness deviations in an area 10×10 μm2, the organic light-emitting device stack exhibits an increase in luminosity by a factor of from about 1.01 to about 2.0 relative to the luminosity of the same microcavity but with a second surface having surface roughness of less than 5.0 nm expressed as the root mean square of the surface thickness deviation in an area 10×10 μm2, at least one of the first and second reflective electrodes is semi-transparent, the first reflective electrode and the second reflective electrode are separated from one another by a distance, the distance corresponds to a depth of the microcavity, and the depth of the microcavity is configured for resonance emission of the peak emission wavelength.

### Claim 22 (depends on 21)

The microcavity of claim 21, wherein the dry film organic material layer comprises from about 2 sub-layers to about 20 sub-layers.

### Claim 23 (depends on 21)

The microcavity of claim 21, wherein the dry film organic material layer comprises a baked dry film organic material layer that has been baked at a temperature of at least 50° C.