# US 2013/0153645 A1 · Process for Hybrid Integration of Focal Plane Arrays

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0153645 A1
- Document ID: US20130153645A1
- Status: Published application
- Kind: A1
- Application number: 13/680,825
- Filed: 2012-11-19
- Published: 2013-06-20
- Earliest claimed: 2011-11-17
- Assignees: Princeton Lightwave, Inc.
- Inventors: Mark Andrew Owens; Sabbir Sajjad Rangwala; Bora Muammer Onat; Domenick Salvemini
- Web page: https://patentgrep.com/patent/US20130153645A1

## CPC

- H10F 39/809: {of hybrid image sensors}
- H10F 39/811: {Interconnections}
- H10W 90/00: Package configurations
- H10W 72/016: {of strap connectors}
- H10W 72/07125: {Means for controlling the bonding environment, e.g. valves or vacuum pumps}
- H10W 72/07141: {Means for applying energy, e.g. ovens or lasers}
- H10W 72/07178: {Means for aligning}
- H10W 72/07223: {Active alignment, e.g. using optical alignment using marks or sensors}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/073: {of die-attach connectors}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 90/722: {between stacked chips}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for aligning a first substrate relative to a second substrate by enabling reflow of low-melting-temperature solder bumps is disclosed. Reflow of the solder bumps induces a force that moves one substrate relative to the other to improve alignment accuracy between bond pads located on each substrate. The method further enables reduction of surface oxide on the solder bumps that would otherwise inhibit reliable solder joint formation.

## Claims

### Claim 1

A method for joining a first substrate and a second substrate, the method comprising:
providing the first substrate, the first substrate including a first plurality of bonding sites, each having one of a first plurality of solder bumps;
providing the second substrate, the second substrate including a second plurality of bonding sites, each having one of a second plurality of solder bumps;
reducing a surface oxide on each of the first plurality of solder bumps and second plurality of solder bumps;
reflowing the first plurality of solder bumps and second plurality of solder bumps;
enabling physical contact between the first plurality of solder bumps and the second plurality of solder bumps to form a first plurality of solder joints; and
enabling a reduction of the surface energy of each of the first plurality of solder joints.

### Claim 2 (depends on 1)

The method of claim 1 wherein physical contact between the first plurality of solder bumps and second plurality of solder bumps is enabled by operations comprising:
separating the first plurality of bonding sites and second plurality of bonding sites by a first separation distance, d1; and
enabling each of the first plurality of solder bumps and second plurality of solder bumps to project above their respective bonding sites by a height, h1, where h1≧0.5*d1.

### Claim 3 (depends on 2)

The method of claim 2 wherein the projection of each of the first plurality of solder bumps and second plurality of solder bumps above their respective bonding sites by height h1 is enabled by operations comprising:
providing each of the first plurality of bonding sites and second plurality of bonding sites with a bond pad having a surface area, a1, each bond pad being surrounded by a first material;
providing each of the first plurality of solder bumps and second plurality of solder bumps such that each solder bump has a cross-sectional area, a2, at its respective bond pad, where a2>a1, wherein each of the first plurality of solder bumps and second plurality of solder bumps comprises a second material that is substantially non-wetting with the first material; and
melting each of the first plurality of solder bumps and second plurality of solder bumps.

### Claim 4 (depends on 1)

The method of claim 1 wherein the surface oxide is reduced while the first substrate and second substrate are located in a first chamber.

### Claim 5 (depends on 4)

The method of claim 4 wherein the reduction of the surface energy is enabled while the first substrate and second substrate are located in the first chamber.

### Claim 6 (depends on 1)

The method of claim 1 further comprising positioning the first substrate and second substrate in a first chamber, wherein the surface oxide is reduced while the first substrate and second substrate remain in the first chamber, and wherein physical contact between the first plurality of solder bumps and the second plurality of solder bumps is enabled while the first substrate and second substrate remain in the first chamber, and further wherein the first plurality of solder bumps and the second plurality of solder bumps are reflowed while the first substrate and second substrate remain in the first chamber.

### Claim 7 (depends on 1)

The method of claim 1 wherein the surface oxide is reduced by heating the first plurality of solder bumps and the second plurality of solder bumps in the presence of hydrogen.

### Claim 8 (depends on 1)

The method of claim 1 wherein the first substrate is provided such that it further comprises a focal-plane array and the second substrate is provided such that it further comprises a read-out integrated circuit.

### Claim 9 (depends on 1)

The method of claim 1 wherein the first substrate is provided such that each of the first plurality of solder bumps consists of indium, and wherein the second substrate is provided such that each of the second plurality of solder bumps consists of indium.

### Claim 10

A method for joining a first substrate having a first plurality of bonding sites arranged in a first arrangement and a second substrate having a second plurality of bonding sites arranged in a second arrangement that is complimentary with the first arrangement, each of the firs plurality of bonding sites and the second plurality of bonding sites having a solder bump disposed on it, the method comprising:
positioning the first substrate and second substrate in a first chamber;
reducing a surface oxide of the solder bumps;
arranging the first substrate and second substrate such that each of the first plurality of bonding sites and a corresponding one of the second plurality of bonding sites is physically coupled via a solder joint comprising two solder bumps;
enabling relative motion of the first substrate and second substrate; and
enabling a reduction of the surface energy of the solder joints.

### Claim 11 (depends on 10)

The method of claim 10 further comprising purging oxygen from the first chamber.

### Claim 12 (depends on 11)

The method of claim 11 further comprising introducing a first gas to the first chamber, the first gas being operable for enabling reduction of the surface oxide of the solder bumps.

### Claim 13 (depends on 12)

The method of claim 12 further comprising heating the first gas.

### Claim 14 (depends on 12)

The method of claim 12 wherein the first gas comprises hydrogen.

### Claim 15 (depends on 12)

The method of claim 12 wherein the first gas comprises a gas selected from the group consisting of argon, nitrogen, forming gas, sulfur hexafluoride, and chlorine-containing gas.

### Claim 16 (depends on 10)

The method of claim 10 further comprising heating the solder bumps during reduction of the surface oxide.

### Claim 17 (depends on 10)

The method of claim 10 further comprising exposing the solder bumps to hydrogen during reduction of the surface oxide.

### Claim 18 (depends on 10)

The method of claim 10 further comprising exposing the solder bumps to hydrogen and heating the solder bumps during reduction of the surface oxide.

### Claim 19 (depends on 10)

The method of claim 10 wherein physical coupling of the first plurality of bonding sites and second plurality of bonding sites is enabled by operations comprising:
providing the first substrate such that each of the first plurality of bonding sites has a bond pad having a surface area, a1, that is surrounded by a first material;
providing the second substrate such that each of the second plurality of bonding sites has a bond pad having a surface area, a1, that is surrounded by the first material;
providing each of the solder bumps such that it has a cross-sectional area, a2, at its respective bond pad, where a2>a1, wherein each of the solder bumps comprises a second material that is substantially non-wetting with the first material;
positioning the first substrate and second substrate such that the first plurality of bonding sites and second plurality of bonding sites are separated by a first separation distance, d1; and
melting each of the solder bumps such that it projects above its respective bonding site by a height, h1, that is greater than or equal to 0.5*d1.