# US 2013/0153222 A1 · Lightweight hollow particles for use in cementing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0153222 A1
- Document ID: US20130153222A1
- Status: Published application
- Kind: A1
- Application number: 13/328,032
- Filed: 2011-12-16
- Published: 2013-06-20
- Earliest claimed: 2011-12-16
- Assignees: Baker Hughes Incorporated
- Inventors: Thomas J. Pisklak; Elizabeth G. Morillo; Qi Qu
- Web page: https://patentgrep.com/patent/US20130153222A1

## CPC

- C09K 8/473: Density reducing additives, e.g. for obtaining foamed cement compositions
- C04B 14/104: {Bentonite, e.g. montmorillonite}
- C04B 18/027: {Lightweight materials}
- C04B 20/12: Multiple coating or impregnating
- C04B 38/009: {Porous or hollow ceramic granular materials, e.g. microballoons (C04B18/027, C04B20/002 take precedence)}
- C04B 38/08: by adding porous substances
- C09K 8/467: containing additives for specific purposes
- C04B 14/24: porous, e.g. foamed glass
- E21B 33/13: Methods or devices for cementing, for plugging holes, crevices or the like
- Y10T 428/2991: Coated
- Y10T 428/2996: Glass particles or spheres
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A lightweight composite having an activated surface contains a lightweight hollow core particle having cement grains which may be adhered to the hollow core or embedded in the surface of the hollow core. The hollow core particle may be prepared from calcium carbonate and a mixture of clay, such as bentonite, and a glassy inorganic material, such as glass spheres, glass beads, glass bubbles, borosilicate glass and fiberglass.

## Claims

### Claim 1

A composite comprising a lightweight hollow core and cement grains, wherein the lightweight hollow core is formed from calcium carbonate, clay and an inorganic material and further wherein the cement grains are adhered to the surface of the lightweight hollow core, embedded in the surface of the lightweight hollow core or are both adhered to the surface of the lightweight hollow core and embedded in the surface of the lightweight hollow core.

### Claim 2 (depends on 1)

The composite of claim 1, wherein the particle size of the lightweight hollow core is between from about 20 to about 40 mesh.

### Claim 3 (depends on 1)

The composite of claim 1, wherein at least a portion of the surface of the lightweight hollow core is treated with a coating layer and further wherein the cement grains are adhered onto the coating layer.

### Claim 4 (depends on 1)

The composite of claim 1, wherein the inorganic material is spherical.

### Claim 5 (depends on 1)

The composite of claim 1, wherein the lightweight hollow sphere is formed from bentonite and an inorganic material selected from the group consisting of inorganic glass, pozzolanic microspheres and ceramic spheres.

### Claim 6 (depends on 5)

The composite of claim 5, wherein the material is inorganic glass selected from the group consisting of glass spheres, glass beads, glass bubbles, borosilicate glass and fiberglass.

### Claim 7 (depends on 6)

The composite of claim 6, wherein the inorganic glass is borosilicate glass.

### Claim 8 (depends on 7)

The composite of claim 7, wherein the lightweight hollow core is formed from about 5 to about 50 percent by weight bentonite and from about 50 to about 95 percent by weight borosilicate glass.

### Claim 9 (depends on 1)

The composite of claim 1 prepared by treating at least a portion of the lightweight hollow particle with a coating layer, applying dry cement onto the coating layer, and hardening the cement.

### Claim 10 (depends on 1)

The composite of claim 1 prepared by adding cement powder to the lightweight hollow core, drying the mixture, heat treating the mixture at a rate of 10° C./min to 800° C., and then cooling the resulting product.

### Claim 11 (depends on 1)

A cementitious slurry comprising the composite of claim 1.

### Claim 12 (depends on 11)

A method of cementing within a gas or oil well, comprising pumping into the well the cementitious slurry of claim 11 and allowing the slurry to harden to a solid mass.

### Claim 13

A lightweight hollow particle prepared by heating a precursor powder comprising (i) calcium carbonate and (ii) a mixture of bentonite and a glassy inorganic material comprising borosilicate glass to a temperature between from about 650° C. to about 850° C. for a time sufficient to decompose the calcium carbonate and at least partially melt the glassy inorganic material, wherein gases evolved during the heating expand the semi-molten glassy inorganic material outwardly to render the lightweight hollow sphere.

### Claim 14 (depends on 13)

The lightweight hollow particle of claim 13, wherein the particle size of the precursor powder is less than or equal to 325 mesh.

### Claim 15 (depends on 13)

The lightweight hollow particle of claim 13, wherein a binder is further mixed with the calcium carbonate and the mixture of bentonite and glassy inorganic material.

### Claim 16 (depends on 13)

The lightweight hollow particle of claim 13, wherein the particle size of the lightweight hollow particle is between from about 20 to about 40 mesh.

### Claim 17 (depends on 13)

The lightweight hollow particle of claim 13, wherein the hollow particle is at least partially treated with a coating layer.

### Claim 18

A method of preparing a lightweight cement particle comprising:
(a) mixing calcium carbonate and a glassy inorganic material comprising bentonite, inorganic glass and, optionally, a binder;
(b) heating the mixture to the softening temperature of the inorganic glass to produce a lightweight hollow core particle;
(c) applying a coating to at least a partial surface of the lightweight core particle;
(d) applying cement grains to the coated lightweight core particle; and
(e) hardening the coating.

### Claim 19 (depends on 18)

The method of claim 18, wherein the particle size of the lightweight hollow core particle of step (b) is between from about 20 to about 40 mesh.

### Claim 20 (depends on 18)

The method of claim 18, wherein the inorganic glass is borosilicate glass.

### Claim 21

A method of preparing a lightweight cement particle comprising:
(a) mixing calcium carbonate and a mixture of an inorganic material and bentonite and forming lightweight particles;
(b) adding cement powder to the formed lightweight particles;
(c) drying the product of step (b);
(d) heating the dried product of step (c) to the glass transition temperature of the inorganic material; and
(e) cooling the product of step (d).

### Claim 22 (depends on 21)

The method of claim 21, wherein the inorganic material is borosilicate glass.