# US 2013/0153204 A1 · Ram bop shear blade process to enhance the toughness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0153204 A1
- Document ID: US20130153204A1
- Status: Published application
- Kind: A1
- Application number: 13/331,494
- Filed: 2011-12-20
- Published: 2013-06-20
- Earliest claimed: 2011-12-20
- Assignees: Hydril USA Manufacturing LLC
- Inventors: William L. CARBAUGH; Leonard CHILDERS; Viral SHAH
- Web page: https://patentgrep.com/patent/US20130153204A1

## CPC

- E21B 33/063: {for shearing drill pipes (cutting of wireline E21B29/04)}
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A shear ram assembly apparatus for providing the capability to shear larger diameter well casings and internal components during ram-type blowout preventer operation while requiring less force to perform the cutting. Components of the shear ram assembly apparatus, include but not limited to a plurality of hardened cutting blades that are coated with a compound that increases the hardness and reduces the coefficient of friction of the cutting blades. In this regard, a smaller force is required to perform the cutting and the cutting blades receive less wear per cut and provide greater assurance that each cut of this failsafe apparatus is successful.

## Claims

### Claim 1

A shear ram assembly apparatus for operation in a ram-type blowout preventer, said apparatus comprising:
a hardened cutting blade wherein said hardened cutting blade is coated with a compound for preventing cutting surface deformation and reducing required shear force during cutting; and
a ram block having said coated hardened cutting blade.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein said coating is applied with a physical vapor deposition (PVD) process.

### Claim 3 (depends on 1)

The apparatus of claim 1, wherein said coating is applied with a chemical vapor deposition (CVD) process.

### Claim 4 (depends on 1)

The apparatus of claim 1, wherein said coating prevents cutting surface deformation during cutting by increasing hardness of said cutting edge.

### Claim 5 (depends on 1)

The apparatus of claim 1, wherein said coating reduces required shear force during cutting by decreasing said cutting surface coefficient of friction.

### Claim 6 (depends on 2)

The apparatus of claim 2, wherein said coating is applied at a temperature of approximately 300° F.

### Claim 7 (depends on 2)

The apparatus of claim 2, wherein said compound comprises titanium and nitrogen.

### Claim 8 (depends on 7)

The apparatus of claim 7, wherein said compound is titanium nitride (TiN).

### Claim 9 (depends on 7)

The apparatus of claim 7, wherein said compound is a glass ceramic matrix of titanium aluminum oxynitride (TiAlON).

### Claim 10 (depends on 7)

The apparatus of claim 7, wherein said compound is titanium carbon nitride (TiCN).

### Claim 11 (depends on 1)

The apparatus of claim 1, wherein said coated hardened cutting blade is either attached to the ram block or integrally formed with the ram block.

### Claim 12

A ram-type blowout preventer (BOP) comprising:
a casing for enclosing said ram-type blowout preventer components;
a plurality of opposing actuators connected to said casing for actuating a plurality of ram blocks attached to said actuators;
a hardened cutting blade for each of said plurality of ram blocks, wherein said hardened cutting blade is coated with a compound for preventing cutting surface deformation and reducing required shear force during cutting.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein said coating is applied with a physical vapor deposition (PVD) process.

### Claim 14 (depends on 12)

The apparatus of claim 12, wherein said coating prevents cutting surface deformation during cutting by increasing hardness of said cutting edge.

### Claim 15 (depends on 12)

The apparatus of claim 12, wherein said coating reduces required shear force during cutting by decreasing said cutting surface coefficient of friction.

### Claim 16 (depends on 13)

The apparatus of claim 13, wherein said coating is applied at a temperature of approximately 300° F.

### Claim 17 (depends on 13)

The apparatus of claim 13, wherein said compound comprises titanium and nitrogen.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein said compound is titanium nitride (TiN).

### Claim 19 (depends on 17)

The apparatus of claim 17, wherein said compound is a glass ceramic matrix of titanium aluminum oxynitride (TiAlON).

### Claim 20 (depends on 12)

The apparatus of claim 12, wherein said coated hardened cutting blade is either attached to a corresponding ram block or integrally formed with the corresponding ram block.

### Claim 21

A method for reducing the force required to shear an oilfield tubular and preventing deformation of a cutting blade associated with said ram-type blowout preventer (BOP), said method comprising:
applying a thin coating of a compound to said cutting blade wherein said compound comprises titanium and nitrogen; and
using a physical vapor deposition process to apply the coating to increase the hardness and reduce the coefficient of friction of said cutting blades.