# US 2013/0152825 A1 · Method for producing a clinker for hydraulic cement with low co2 emission and high resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0152825 A1
- Document ID: US20130152825A1
- Status: Published application
- Kind: A1
- Application number: 13/704,699
- Filed: 2011-06-17
- Published: 2013-06-20
- Earliest claimed: 2010-06-18
- Assignees: Cemex Research Group AG
- Inventors: Homero Ramirez Tovias; Juan Carlos Martinez; Norma Leticia Garza Gonzalez; Karla Serrano Gonzalez
- Web page: https://patentgrep.com/patent/US20130152825A1

## CPC

- C04B 7/32: Aluminous cements
- C04B 7/02: Portland cement
- C04B 7/323: {Calcium aluminosulfate cements, e.g. cements hydrating into ettringite}
- C04B 7/345: Hydraulic cements not provided for in one of the groups C04B7/02 - C04B7/34
- C04B 7/367: {Avoiding or minimising carbon dioxide emissions}
- C04B 7/421: {Inorganic materials}
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing a clinker for cement, comprising grinding a raw flour comprising, especially, Al2O3, Fe2O3 and SO3 in contents such that the formula for calculating SO3 content of=0.261×Al2O3−0.638×Fe2O3+k, where 2.5<k<3.5, then by sintering flour in an overn wherein the temperature is between 1250° C. and 1350° C. and oxygen content is between 2.5% and 10% by volume.

## Claims

### Claim at position 1

1-6. (canceled)

### Claim 7

A process for the manufacture of a clinker for cement, comprising grinding a raw meal comprising Al2O3, Fe2O3 and SO3 in contents such that the formula for calculating SO3 content of=0.261×Al2O3−0.638×Fe2O3+k, where 2.5<k<3.5, and sintering said raw meal in a kiln where temperature is between 1250° C. and 1350° C. and oxygen content is between 2.5% and 10% by volume.

### Claim 8 (depends on 7)

The process as claimed in claim 7, wherein the Al2O3 content is between 3% and 10% by weight and the Fe2O3 content is between 0.5% and 2% by weight.

### Claim 9 (depends on 7)

The process as claimed in claim 7, wherein the oxygen content of the kiln is between 4% and 8% by volume.

### Claim 10

A clinker composition, comprising:
from 30% to 70% by weight of alite (C3S),
from 10% to 40% by weight of belite (C2S),
from 5% to 15% by weight of calcium sulfoaluminate (C4A3S),
from 1% to 7% by weight of ferrite (C4AF),
from 3% to 10% by weight of anhydrite (CS), and
the remainder being composed of lime and/or of C3A.

### Claim 11 (depends on 10)

The composition as claimed in claim 10, further comprising from 0.1% to 1.5% by weight of fluorite (CaF2).

### Claim 12 (depends on 11)

The composition as claimed in claim 11, wherein saud composition comprises from 0.2% to 1% by weight of fluorite (CaF2).