# US 2013/0152375 A1 · Magnetic Platinum Catalyst and Method of Making and its Application as an Engine Fuel Enhancer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0152375 A1
- Document ID: US20130152375A1
- Status: Published application
- Kind: A1
- Application number: 13/327,438
- Filed: 2011-12-15
- Published: 2013-06-20
- Earliest claimed: 2011-12-15
- Inventors: Shi Min Chen; Yong Sheng Chen
- Web page: https://patentgrep.com/patent/US20130152375A1

## CPC

- B01J 23/63: with rare earths or actinides
- B01J 23/894: {with rare earths or actinides}
- B01J 35/33: Electric or magnetic properties
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/348: {Electrochemical processes, e.g. electrochemical deposition or anodisation}
- F02M 27/02: by catalysts
- F02M 27/04: by electric means, {ionisation, polarisation} or magnetism
- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- C22C 2202/02: Magnetic
- Y10T 29/49002: Electrical device making
- Y10T 29/49345: Catalytic device making
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- F02M: SUPPLYING COMBUSTION ENGINES IN GENERAL WITH COMBUSTIBLE MIXTURES OR CONSTITUENTS THEREOF
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A magnetic platinum catalyst and its application as an engine fuel enhancer. The method of making the magnetic platinum catalyst includes: the use of neodymium magnetic alloy containing 25-50% of the neutral neodymium (NdFeB) alloys, processed into a diameter of 13 mm, a length 9 mm cylinder, as a catalyst carrier. The surface of the catalyst carrier is treated with antioxidant. A platinum group metal is used as the catalyst rare earth materials to produce a catalyst acid soaking solution. The solution includes 0.01-0.2% platinum and 0.01-0.15% rhodium. The pH of the solution is adjusted to 4 using oxalic acid. After soaking in the solution, draining, and drying, the carrier is placed in a muffle furnace and baked. The catalyst is firmly attached to the surface of the carrier to form a magnetic platinum catalyst having catalyzing ability. Such catalyst is used in connection with engine fuel to enhance its operation.

## Claims

### Claim 1

A method of making a magnetic platinum catalyst comprising the steps of:
a. using powder metallurgy to form a neutral neodymium magnetic alloy containing about 25-50% neodymium into a catalyst carrier;
b. making said catalyst carrier into a cylinder with a diameter of about 13 mm and a length of about 9 mm, said catalyst carrier having a surface;
c. treating said surface of said catalyst carrier with an antioxidant;
d. producing a catalyst acid soaking solution with about 0.01-0.2% platinum and about 0.01-0.15% rhodium;
e. adjusting the pH of said solution to 4 with oxalic acid;
f. soaking said catalyst carrier in said solution for 12-24 hours;
g. draining said catalyst carrier from said solution;
h. drying said catalyst carrier;
i. baking said catalyst carrier in a muffle furnace at about 300-600° C. to firmly attach said catalyst onto said surface of said catalyst carrier.

### Claim 2 (depends on 1)

The method of claim 1 further comprising the step of electro-plating said surface of said catalyst carrier with a layer of nickel, a layer of copper and another layer of nickel, wherein each said electro-plating layer is about 0.006-0.01 mm thick.

### Claim 3 (depends on 1)

The method of claim 1 further comprising the step of magnetizing said catalyst carrier using a magnetizer with a magnetic flux of about 3500-5000 Gauss per square centimeter to form a magnetic platinum catalyst having a strong energy flux of catalyzing power.

### Claim 4

A method of making a magnetic platinum catalyst having a body, comprising the steps of:
a. making a catalyst acid soaking solution comprises the steps of:
i. dissolving 6 grams of H2PtCl6(H2PtCl6.6H20) and 4 grams of RhCl3(RhCl3.3H20) into 1000 ml of water;
ii. adjusting the pH of said solution to 4 with oxalic acid;
iii. allowing said solution to settle for about 2 hours;
iv. stirring said solution for about 10 minutes;
v. heating said solution to about 70° C.;
b. making a catalyst carrier comprises the steps of:
i. using powder metallurgy to form a neutral neodymium magnetic alloy containing about 39% neodymium into a catalyst carrier;
ii. making said catalyst carrier into a cylinder with a diameter of about 13 mm and a length of about 9 mm;
c. making the body for the magnetic platinum catalyst having a surface, comprises the steps of:
i. soaking said catalyst carrier in said catalyst acid soaking solution for 15 hours;
ii. draining said catalyst carrier from said solution;
iii. baking said catalyst carrier in an oven for about 20 minutes at a temperature of about 75-80° C.;
d. cooling said body to room temperature;
e. baking said body in a muffle furnace for 3 hours at a temperature of about 390° C.;
f. turning off the muffle furnace and waiting for the temperature to cool down to below 50° C.;
g. removing said body from said muffle furnace;
h. electro-plating the surface of said body with a layer of nickel, a layer of copper and another layer of nickel, wherein each said electro-plating layer is about 0.006-0.01 mm thick;
i. magnetizing said body using a magnetizer.

### Claim 5 (depends on 1)

An engine fuel enhancer comprising:
a. at least one shell made of a heat-bearing and corrosion-bearing polytetra fluoroethylene material;
b. least one magnetic platinum catalyst produced according to the method of claim 1; and
c. a chamber inside each said shell having a diameter of about 13.2 mm for receiving said magnetic platinum catalyst.

### Claim 6 (depends on 5)

The engine fuel enhancer of claim 5 further comprising at least one functional circuit board and at least one cover, wherein each said circuit board is placed over and attached to each said magnetic platinum catalyst in each said chamber with each said cover enclosing said magnetic platinum catalyst and said circuit board in said chamber of each said shell.

### Claim 7 (depends on 6)

The engine fuel enhancer of claim 6 comprises first and second shells locked to each other, each shell having a north magnetic pole, a south magnetic pole and first and second sides, on said first side of each shell are a pair of locking teeth and a docking slot, and on said second side of each shell is a latch with corresponding teeth;
wherein said latch of said first shell engages said locking teeth of said second shell via said docking slot of said second shell, and said latch of said second shell engages said locking teeth of said first shell via said docking slot of said first shell; and
wherein said north magnetic pole of said first shell faces said south magnetic pole of said second shell.

### Claim 8 (depends on 6)

The engine fuel enhancer of claim 6 wherein said functional circuit board having means to drain external power comprises a functional circuit, an inductance and a power drainage circuit to form a self-motivated power conversion circuit.

### Claim 9 (depends on 7)

A method of enhancing the fuel efficiency of an engine having a fuel line comprising the steps of:
a. providing an engine fuel enhancer of claim 7; and
b. sandwiching said fuel line of said engine between said first and second shells.

### Claim 10 (depends on 5)

A method of enhancing the fuel efficiency of an engine having a fuel tank comprising the steps of:
a. providing an engine fuel enhancer of claim 5; and
b. placing said engine fuel enhancer into said fuel tank.

### Claim 11

A method of making a magnetic platinum catalyst comprising the steps of:
a. making a catalyst acid soaking solution with platinum and rhodium;
b. adjusting the pH of said solution to 4 with oxalic acid;
c. making a catalyst carrier with a neutral neodymium magnetic alloy containing about 25-50% neodymium;
d. treating said catalyst carrier with an antioxidant;
e. soaking said catalyst carrier in said catalyst acid soaking solution;
f. baking said catalyst carrier in a muffle furnace at about 300-600° C.;
g. magnetizing said catalyst with a magnetizer.

### Claim 12 (depends on 11)

An engine fuel enhancer comprising:
a. at least one shell made of a heat-bearing and corrosion-bearing material;
b. at least one magnetic platinum catalyst produced according to the method of claim 11; and
c. a chamber inside each said shell for receiving each said magnetic platinum catalyst.