# US 2013/0139390 A1 · Method for producing a lead-free sliding bearing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0139390 A1
- Document ID: US20130139390A1
- Status: Published application
- Kind: A1
- Application number: 13/703,137
- Filed: 2010-06-10
- Published: 2013-06-06
- Earliest claimed: 2010-06-10
- Assignees: Federal-Mogul Wiesbaden GmbH
- Inventors: Holger Schmitt; Daniel Meister; Roman Lewandowski; Andrzej Broniszewski
- Web page: https://patentgrep.com/patent/US20130139390A1

## CPC

- B23P 15/003: {bearings (see also F16C33/00)}
- C22C 9/02: with tin as the next major constituent
- F16C 33/121: {Use of special materials}
- F16C 33/14: Special methods of manufacture; Running-in
- F16C 2204/10: Alloys based on copper
- F16C 2204/12: with tin as the next major constituent
- Y02T 10/86: Optimisation of rolling resistance, e.g. weight reduction
- Y10T 29/49709: Specific metallic composition
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In a method for producing a lead-free sliding bearing, a copper-based material comprising a total of 0.1% to 3% of the elements aluminum, magnesium, silicon, titanium, zircon, and chromium is sintered. Additionally, up to 15% tin can be included in order to ensure optimal properties for use in the internal combustion engine.

## Claims

### Claim 1

A method for the production of a lead-free sliding bearing, in which a copper-based material comprising a total of 0.1% to 3% by weight of the elements aluminium, magnesium, silicon, titanium, zirconium and chromium is sintered, with the material being mixed with at least one of tin and copper powder prior to sintering.

### Claim 2 (depends on 1)

The method according to claim 1, wherein characterised in that the material contains a total of at least 0.2% by weight of the elements aluminium, magnesium, silicon, titanium, zirconium and chromium.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the material contains up to 15% by weight of tin.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the material furthermore contains a solid lubricant.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the material furthermore contains hard particles.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the material furthermore contains chip breakers.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the material comprises at least 5% of particles having a size of <5 μm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the material is mixed with tin and copper powder prior to sintering.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the material contains a total of at most 1% by weight of the elements aluminium, magnesium, silicon, titanium, zirconium and chromium.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the material contains about 6% by weight tin.

### Claim 11 (depends on 4)

The method of claim 4, wherein the solid lubricant selected from the list consisting of h-BN and C.

### Claim 12 (depends on 5)

The method according to claim 5, wherein the hard particles comprises at least one selected from the group consisting of carbides, nitrides and phosphides.