# US 2013/0096270 A1 · Porphyrin copolymer containing thienothiadiazole units, preparation method and uses thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0096270 A1
- Document ID: US20130096270A1
- Status: Published application
- Kind: A1
- Application number: 13/702,105
- Filed: 2010-06-07
- Published: 2013-04-18
- Earliest claimed: 2010-06-07
- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.
- Inventors: Mingjie Zhou; Jie Huang; Yijin Liu
- Web page: https://patentgrep.com/patent/US20130096270A1

## CPC

- C08G 61/123: {derived from five-membered heterocyclic compounds}
- C08F 236/20: unconjugated
- C08G 61/124: {with a five-membered ring containing one nitrogen atom in the ring}
- C08G 61/126: {with a five-membered ring containing one sulfur atom in the ring}
- C09K 11/06: containing organic luminescent materials
- H10K 85/151: {Copolymers}
- H10K 85/361: {Polynuclear complexes, i.e. complexes comprising two or more metal centers}
- C08G 2261/124: alternating
- C08G 2261/148: Side-chains having aromatic units
- C08G 2261/3221: containing one or more nitrogen atoms as the only heteroatom, e.g. pyrrole, pyridine or triazole
- C08G 2261/3243: containing one or more sulfur atoms as the only heteroatom, e.g. benzothiophene
- C08G 2261/3246: containing nitrogen and sulfur as heteroatoms
- C08G 2261/91: Photovoltaic applications
- C09K 2211/1011: Condensed systems
- C09K 2211/1029: containing one nitrogen atom as the heteroatom
- C09K 2211/1466: containing nitrogen as the only heteroatom
- C09K 2211/1483: containing nitrogen and sulfur as heteroatoms
- H10K 10/484: {characterised by the channel regions}
- H10K 30/20: comprising organic-organic junctions, e.g. donor-acceptor junctions
- H10K 30/50: Photovoltaic [PV] devices
- H10K 50/11: characterised by the electroluminescent [EL] layers
- H10K 85/30: Coordination compounds
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A porphyrin copolymer containing thienothiadiazole units, preparation method and uses thereof are disclosed. The copolymer has the structural formula (I), wherein: R1, R2, R3, R4 are same or different and each represents a C1-C32 alkyl; n is an integer of 1-100. The copolymer comprises fluorene units, thienothiadiazole units and porphyrin units, which enhance the density of electron cloud in copolymer skeleton, make the band-gap of the copolymer become narrow, thereby broaden the spectral response range of the copolymer, and improve the photoelectric transformation efficiency.

## Claims

### Claim 1

A porphyrin copolymer containing thienothiadiazole units, which has the structural formula (I):
wherein, R1, R2, R3, R4 are same or different and each represents a C1-C32 alkyl, and n is an integer of 1-100.

### Claim 2 (depends on 1)

The porphyrin copolymer containing thienothiadiazole units of claim 1, wherein each unit of the porphyrin copolymer containing thienothiadiazole units has two identical fluorenyl group containing alkyl.

### Claim 3 (depends on 1)

The porphyrin copolymer containing thienothiadiazole units of claim 1, wherein the R1, R2, R3 and R4 are same and each represents a C8-C32 alkyl.

### Claim 4 (depends on 1)

The porphyrin copolymer containing thienothiadiazole units of claim 1, wherein n is an integer of 10-50.

### Claim 5

A preparation method of a porphyrin copolymer containing thienothiadiazole units, comprising:
compounds A, B, C and D with following structural formulae are provided separately:
wherein R1, R2, R3 and R4 are same or different, and each of them represents a C1-C32 alkyl;
in a system containing a catalyst, an oxidant and an organic solvent, the oxidative condensation of compounds A, B and C is carried out to give the 5,15-bis(9,9-dialkyl fluorene)porphyrin;
in a system containing a catalyst and an organic solvent, the 5,15-bis(9,9-dialkyl fluorene)porphyrin is bromination substituted to give the 5,15-dibromo-10,20-bis(9,9-dialkylfluorene)porphyrin;
with the present of a catalyst and an organic solvent, the Suzuki coupling reaction of 5,15-dibromo-10,20-bis(9,9-dialkylfluorene)porphyrin and compound D is carried out to give the copolymer of following structural formula (I):
wherein n is an integer of 1-100.

### Claim 6 (depends on 5)

The preparation method of a porphyrin copolymer containing thienothiadiazole units of claim 5, wherein the procedure of the said oxidative condensation includes: under anhydrous and oxygen-free conditions, compounds A, B, and C are dissolved in an organic solvent, an organic acid is added as the catalyst, the mixture is stirred under 20° C.-100° C. for 1-24 hours, dichloro dicyanobenzoquinone (DDQ) is added as the oxidant, and stirred for another 1-60 minutes, the reaction is quenched by adding triethylamine, and the product is obtained following purification.

### Claim 7 (depends on 5)

The preparation method of a porphyrin copolymer containing thienothiadiazole units of claim 5, wherein the procedure of the said Suzuki coupling reaction includes: under oxygen-free condition, compound D and 5,15-dibromo-10,20-bis(9,9-dialkyl fluorene)porphyrin are added to an organic solvent in a molar ratio of 1:1.5-1.5:1, the oxygen is removed by evacuation then nitrogen is purged in, and a catalyst is added, the mixture is heated to 50-120° C. for 12-80 hours, after cooling, the mixture is added to an aqueous solution of sodium diethyldithiocarbamate, then the mixture is heated with stirring at 60-80° C. for 12-14 hours.

### Claim 8 (depends on 5)

The preparation method of a porphyrin copolymer containing thienothiadiazole units of claim 5, wherein the R1, R2, R3 and R4 are same and each represents a C8-C32 alkyl, the n is an integer of 10-50.

### Claim 9 (depends on 5)

The preparation method of a porphyrin copolymer containing thienothiadiazole units of claim 5, wherein the catalyst in the said Suzuki coupling reaction is an organic palladium or a mixture of organic palladium and an organic phosphine ligand in a molar ratio of 1:2-20, the molar amount of the catalyst in the said Suzuki coupling reaction is 0.05-20% of the molar amount of the compound D, and the organic solvent is a weak polar or polar aprotic organic solvent or the mixture thereof.

### Claim 10 (depends on 1)