# US 2013/0096269 A1 · Ethylene-based terpolymer having high elasticity and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0096269 A1
- Document ID: US20130096269A1
- Status: Published application
- Kind: A1
- Application number: 13/646,350
- Filed: 2012-10-05
- Published: 2013-04-18
- Earliest claimed: 2011-10-18
- Assignees: Korea Institute of Industrial Technology
- Inventors: Dong Hyun Kim; Joon Chul Lee; Hyun Ki Kim; Tae Wan Kim
- Web page: https://patentgrep.com/patent/US20130096269A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/65908: {in combination with an ionising compound other than alumoxane, e.g. (C6F5)4B-X+}
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65927: {two cyclopentadienyl rings being mutually bridged}
- Y10S 526/943: Polymerization with metallocene catalysts
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The present invention relates to an ethylene-based terpolymer having high elasticity and a preparation method thereof, and more particularly, to a highly elastic, ethylene-based terpolymer, which comprises a specific molar ratio of a ethylene unit, a C6-12 α-olefin unit and at least one functional unit selected from the group consisting of divinylbenzene and para-methylstyrene and to a method of preparing the highly elastic, ethylene-based terpolymer using a metallocene catalyst.

## Claims

### Claim 1

A highly elastic, ethylene-based terpolymer comprising
60-95 mole % of an ethylene unit,
3-35 mole % of a C6-12 α-olefin unit, and
0.5-5 mole % of at least one functional unit selected from the group consisting of divinylbenzene and para-methylstyrene,
the ethylene-based terpolymer having a weight-average molecular weight of 50,000-200,000 and a glass transition temperature between -20° C. and -60° C.

### Claim 2 (depends on 1)

The highly elastic, ethylene-based terpolymer of claim 1, wherein the terpolymer comprises 80-95 mole % of the ethylene unit, 4-18 mole % of the C6-12 α-olefin unit, and 0.5-2 mole % of the at least one functional unit selected from the group consisting of divinylbenzene and para-methylstyrene.

### Claim 3 (depends on 1)

The highly elastic, ethylene-based terpolymer of claim 1, wherein the terpolymer has a molecular weight distribution of 1-3.5.

### Claim 4 (depends on 1)

The highly elastic, ethylene-based terpolymer of claim 1, wherein the terpolymer has a Tan δ of 0.1-0.5.

### Claim 5

A method for preparing a highly elastic, ethylene-based terpolymer, the method comprising a step of polymerizing 60-95 mole % of an ethylene unit, 3-35 mole % of a C6-12 α-olefin unit and 0.5-5 mole % of at least one functional unit selected from the group consisting of divinylbenzene and para-methylstyrene using a metallocene catalyst.

### Claim 6 (depends on 5)

The method of claim 5, wherein the metallocene catalyst comprises a group 4 transition metal as a chiral metal, and cyclopentadienyl or its derivative, fluorenyl or its derivative, or indenyl or its derivative as a ligand, and has a bridged (ansa) structure or a non-bridged structure.

### Claim 7 (depends on 6)

The method of claim 6, wherein the metallocene catalyst is ethylbis(indenyl)zirconium dichloride.

### Claim 8 (depends on 5)

The method of claim 5, wherein catalytic activity in the polymerization is 2500-5000.

### Claim 9 (depends on 5)

The method of claim 5, wherein the metallocene catalyst is used together with an alkylaluminoxane cocatalyst, an organic aluminum cocatalyst, a boron compound cocatalyst, or a mixture thereof

### Claim 10 (depends on 9)

The method of claim 9, wherein the alkylaluminoxane cocatalyst is selected from the group consisting of methylaluminoxane, ethylaluminoxane, propylaluminoxane, butylaluminoxane and isobutylaluminoxane; the organic alkyl aluminum cocatalyst is selected from the group consisting of trimethylaluminum, triethylaluminum and diisobutylaluminum chloride; and the boron compound cocatalyst is selected from the group consisting of tris(pentafluorophenyl)borane, N,N-dimethylanilinium tetrakis(pentafluorophenyl)borate and triphenylmethylinium tetrakis(pentafluorophenyl)borate.

### Claim 11 (depends on 5)

The method of claim 5, wherein the polymerization is carried out at a temperature of 20 to 40° C.

### Claim 12 (depends on 5)

The method of claim 5, wherein the polymerization is carried out for 20 minutes to 1 hour.