# US 2013/0096222 A1 · Polyolefin-Based Crosslinked Compositions and Methods of Making Them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0096222 A1
- Document ID: US20130096222A1
- Status: Published application
- Kind: A1
- Application number: 13/273,323
- Filed: 2011-10-14
- Published: 2013-04-18
- Earliest claimed: 2011-10-14
- Assignees: ExxonMobil Chemical Patents Inc.
- Inventors: Sunny Jacob
- Web page: https://patentgrep.com/patent/US20130096222A1

## CPC

- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 2312/06: by radiation
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Provided is a method for providing a composition comprising at least one propylene-based polymer; at least one of multifunctional acrylates, multifunctional methacrylates, functionalized polybutadiene resins, functionalized cyanurate, and allyl isocyanurate; at least one of hindered phenols, phosphites, and hindered amines; and at least one photoinitiator for UV curing. The propylene-based polymer can include propylene derived units and one or more dienes, and have a triad tacticity of from 50% to 99% and a heat of fusion of less than 80 J/g. The composition can be extruded and crosslinked. The crosslinked composition is particularly useful for making films and fibers.

## Claims

### Claim 1

A method for making a crosslinked composition comprising the steps of:
(a) providing a composition comprising:
(i) from about 60 to about 95 wt % of at least one propylene-based polymer comprising propylene-derived units and one or more dienes, the propylene-based polymer having a triad tacticity of from 50% to 99% and a heat of fusion of less than 80 J/g;
(ii) from about 0.1 to about 15 wt % of at least one of multifunctional acrylates, multifunctional methacrylates, functionalized polybutadiene resins, functionalized cyanurate, and allyl isocyanurate;
(iii) from about 0.1 to about 5 wt % of at least one of hindered phenols, phosphates, and hindered amines; and
(iv) from about 0.1 to about 5 wt % of at least one photoinitiator;
(b) extruding the composition; and
(c) crosslinking the composition.

### Claim 2 (depends on 1)

The method of claim 1, wherein the photoinitiator is an ultraviolet (UV) photoinitiator.

### Claim 3 (depends on 2)

The method of claim 2, wherein the UV photoinitiator is at least one of a benzophenone photoinitiator; a phenylglyoxylate photoinitiator; an alpha hydroxy ketone photoinitiator; a combination of acyl phosphine oxide and an alpha hydroxy ketone photoinitiator; 2,2-aimethoxy-1,2-diphenylethan-1-one; and a combination of oxy-phenyl-acetic acid 2-[2-oxo-2-phenyl-acetoxy-ethoxy]-ethyl ester and oxy-phenyl-acetic acid 2-[2-hydroxy-ethoxy]-ethyl ester.

### Claim 4 (depends on 2)

The method of claim 2, wherein the composition of step (a) comprises from about 1 to about 3 wt % of a UV photoinitiator.

### Claim 5 (depends on 1)

The method of claim 1, wherein the extruded composition is crosslinked by at least one of visible light, ultraviolet radiation, and gamma radiation.

### Claim 6 (depends on 1)

The method of claim 1, wherein the extruded composition is crosslinked using ultraviolet radiation at about 200 to about 350 nm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the crosslinked composition has an Elongation at Break of at least about 700%.

### Claim 8 (depends on 1)

The method of claim 1, wherein the propylene-based polymer comprises from about 5 wt % to about 40 wt % of at least one of ethylene and butene units.

### Claim 9 (depends on 1)

The method of claim 1, wherein the propylene-based polymer of step (a) comprises from about 0.2 to about 4 wt % 5-ethylidene-2-norbornene.

### Claim 10

A method for making a crosslinked composition comprising the steps of:
(a) providing a composition comprising:
(i) at least one propylene-based polymer comprising propylene-derived units and optionally one or more dienes, the propylene-based polymer having a triad tacticity of from 50% to 99% and a heat of fusion of less than 80 J/g;
(ii) from about 0.1 to about 5 wt % of at least one ultraviolet photoinitiator selected from the group consisting of a benzophenone photoinitiator; a phenylglyoxylate photoinitiator; an alpha hydroxy ketone photoinitiator; a combination of acyl phosphine oxide and an alpha hydroxy ketone photoinitiator; 2,2-aimethoxy-1,2-diphenylethan-1-one; and a combination of oxy-phenyl-acetic acid 2-[2-oxo-2-phenyl-acetoxy-ethoxy]-ethyl ester and oxy-phenyl-acetic acid 2-[2-hydroxy-ethoxy]-ethyl ester;
(b) extruding the composition; and
(c) crosslinking the composition using ultraviolet radiation.

### Claim 11 (depends on 10)

The method of claim 10, wherein the propylene-based polymer of step (a) comprises from about 0.1 to about 10 wt % of a diene.

### Claim 12 (depends on 10)

The method of claim 10, wherein the extruded composition is crosslinked using ultraviolet radiation at about 200 to about 350 nm.

### Claim 13 (depends on 10)

The method of claim 10, wherein the crosslinked composition after UV radiation has an Elongation at Break of at least about 700%.

### Claim 14

A method for making a crosslinked composition comprising the steps of:
(a) providing a composition comprising:
(i) from about 60 to about 95 wt % of at least one propylene-based polymer comprising propylene-derived units and one or more dienes, the propylene-based polymer having a triad tacticity of from 50% to 99% and a heat of fusion of less than 80 J/g;
(ii) from about 1 to about 20 wt % of a at least one of a polypropylene homopolymer and polypropylene-ethylene copolymer; and
(iii) from about 0.1 to about 5 wt % of at least one ultraviolet photoinitiator;
(b) extruding the composition; and
(c) crosslinking the composition using ultraviolet radiation.

### Claim 15 (depends on 14)

The method of claim 14, wherein the composition of step (a) further comprises from about 0.1 to about 15 wt % of at least one of multifunctional acrylates, multifunctional methacrylates, functionalized polybutadiene resins, functionalized cyanurate, and allyl isocyanurate.

### Claim 16 (depends on 14)

The method of claim 14, wherein the composition of step (a) further comprises from about 0.1 to about 5 wt % of at least one of hindered phenols, phosphates, and hindered amines.

### Claim 17 (depends on 14)

The method of claim 14, wherein the composition of step (a) comprises from about 1 to about 10 wt % of a polypropylene homopolymer.

### Claim 18 (depends on 14)

The method of claim 14, wherein the composition of step (a) comprises from about 2 to about 7 wt % of a polypropylene-ethylene copolymer, and the polypropylene-ethylene copolymer comprises about 50 wt % to about 70 wt % of ethylene-derived units.

### Claim 19 (depends on 14)

The method of claim 14, wherein the composition of step (a) comprises from about 2 to about 7 wt % of a polypropylene-ethylene copolymer, and the polypropylene-ethylene copolymer comprises about 2 wt % to about 5 wt % of ethylene-derived units.

### Claim 20 (depends on 14)

The method of claim 14, wherein the crosslinked composition after UV radiation has an Elongation at Break of at least about 700%.

### Claim 21 (depends on 1)

An article made from the composition of claim 1.

### Claim 22 (depends on 1)

The method of claim 1, wherein the composition of step (a) is crosslinked after being extruded.

### Claim 23 (depends on 1)

The method of claim 1, wherein the composition of step (a) is crosslinked before being extruded.

### Claim 24 (depends on 1)

The method of claim 1, wherein the composition of step (a) is crosslinked while being extruded.

### Claim 25 (depends on 1)

The method of claim 1, further comprising a step of crosslinking the composition using electron beam radiation at an e-beam dose of about 200 KGy or less before, simultaneously with, or after ultraviolet radiation.