# US 2013/0095603 A1 · Method for the treatment of a metal contact formed on a substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0095603 A1
- Document ID: US20130095603A1
- Status: Published application
- Kind: A1
- Application number: 13/634,498
- Filed: 2011-03-11
- Published: 2013-04-18
- Earliest claimed: 2010-03-12
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Raphaël Cabal
- Web page: https://patentgrep.com/patent/US20130095603A1

## CPC

- H10F 77/211: {for photovoltaic cells}
- H05K 3/12: using {thick film techniques, e.g.} printing techniques to apply the conductive material {or similar techniques for applying conductive paste or ink patterns}
- H05K 3/1291: {Firing or sintering at relative high temperatures for patterns on inorganic boards, e.g. co-firing of circuits on green ceramic sheets}
- H05K 2203/107: Using laser light
- Y02E 10/50: Photovoltaic [PV] energy
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention relates to a method for obtaining a metal contact on a substrate, comprising the following steps: (a) depositing a metal pattern in the form of a paste formed from a mixture of a metal power and a solvent, (b) heating the assembly formed in step (a) in order to evaporate the solvent, and (c) annealing same in order to form a metal contact between the metal pattern and the substrate. The invention is characterised in that it also includes a step (d) in which the metal contact is heated by laser at an energy density of between 0.5 J/cm2 and 15 J/cm2.

## Claims

### Claim 1

A method for obtaining a metal contact on a substrate, comprising the steps of:
(a) depositing a metal pattern in the form of a paste comprising a metal powder and a solvent onto the substrate to form an assembly;
(b) heating the assembly formed in step (a) to evaporate the solvent; and
(c) carrying out an annealing step to form a metal contact between the metal pattern and the substrate, and
(d) heating the metal contact using a laser with an energy density between 0.5 J/cm2 and 15 J/cm2.

### Claim 2 (depends on 1)

The method of claim 1, wherein step (a) comprises a step of screen printing.

### Claim 3 (depends on 1)

The method of claim 1, wherein the metal pattern is at least 1 μm in thickness.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal contact takes the form of a mesh.

### Claim 5 (depends on 1)

The method of claim 1, wherein the metal contact takes the form of a layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the metal contact comprises silver, aluminum, or a silver-aluminum alloy.

### Claim 7 (depends on 1)

The method of claim 1, further comprising a step of depositing a dielectric layer on the substrate before step (a).

### Claim 8 (depends on 1)

The method of claim 1, wherein the laser emits in the infrared range.

### Claim 9 (depends on 1)

The method of claim 1, wherein the laser is a laser-diode-pumped laser, with a peak current drawn by the laser diode is between 20 A and 30 A.

### Claim 10 (depends on 1)

The method of claim 1, wherein the laser emits pulses at a frequency between 30 kHz and 60 kHz.

### Claim 11 (depends on 1)

The method of claim 1, wherein the metal contacts comprise a degree of coverage of an area between two pulses of at least 95%.

### Claim 12 (depends on 1)

The method of claim 1, wherein the laser comprises a scan rate lower than 10 m/s.

### Claim 13 (depends on 1)

The method of claim 1, wherein the laser emits pulses between 1 ns and 1 μs in duration.

### Claim 14 (depends on 1)

The method of claim 1, wherein the laser is a pulsed laser-diode-pumped laser emitting in the infrared range, and said laser is employed under the following conditions:
the frequency of the pulses lies between 40 kHz and 60 kHz;
the degree of coverage of the area of the metal contact between two pulses is 97% or more;
the scan rate of the laser over the area of the metal contact is between 1 m/s and 10 m/s and preferably between 1 m/s and 5 m/s; and
the laser diode draws a peak current of between 25 A and 28 A.

### Claim 15 (depends on 8)

The method of claim 8, wherein the infrared range wavelength is about 1064 nm.

### Claim 16 (depends on 9)

The method of claim 9, wherein the peak current drawn by the laser diode is between 25 A and 28 A.

### Claim 17 (depends on 10)

The method of claim 10, wherein the laser emits pulses at a frequency between 40 kHz and 60 kHz.

### Claim 18 (depends on 11)

The method of claim 11, wherein the degree of coverage is at least 97%.

### Claim 19 (depends on 12)

The method of claim 12, wherein the scan rate is between 1 m/s and 10 m/s.

### Claim 20 (depends on 13)

The method of claim 13, wherein the laser emits pulses between 100 ns and 1 μs.

### Claim 21 (depends on 14)

The method of claim 14, wherein the scan rate is between 1 m/s and 5 m/s.