# US 2013/0095411 A1 · Fluorine containing ionomer composite with ion exchange function, preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0095411 A1
- Document ID: US20130095411A1
- Status: Published application
- Kind: A1
- Application number: 13/805,329
- Filed: 2010-06-18
- Published: 2013-04-18
- Earliest claimed: 2010-06-18
- Assignees: Shandong Huaxia Shenzhou New Material Co., Ltd.
- Inventors: Yongming Zhang; Junke Tang; Ping Liu; Heng Zhang; Jun Wang
- Web page: https://patentgrep.com/patent/US20130095411A1

## CPC

- H01M 8/1041: Polymer electrolyte composites, mixtures or blends
- B01D 69/1071: {Woven, non-woven or net mesh}
- B01D 69/141: {Heterogeneous membranes, e.g. containing dispersed material; Mixed matrix membranes}
- C08J 5/2281: {fluorine containing heterogeneous membranes}
- D06M 14/28: of macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- H01M 8/1039: halogenated, e.g. sulfonated polyvinylidene fluorides
- H01M 8/106: characterised by the chemical composition of the porous support
- H01M 8/1072: by chemical reactions, e.g. in situ polymerisation or in situ crosslinking
- B01D 71/32: containing fluorine atoms
- B01D 2323/30: Cross-linking
- B01D 2325/42: Ion-exchange membranes
- C08J 2327/18: Homopolymers or copolymers of tetrafluoroethylene
- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- H01M 8/1023: having only carbon, e.g. polyarylenes, polystyrenes or polybutadiene-styrenes
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a composite which is comprised of one or more ion exchange resin(s) and fluorine containing polymer fiber, wherein the fiber and the film-forming resin form a triazine-ring crosslinked structure, so that the film prepared from the composite is of good airtightness and stability, as well as high ion exchange capacity and high conductivity. The preparation method of the composite, the product prepared from this composite and the use thereof are also provided.

## Claims

### Claim at position 1

1-10. (canceled)

### Claim 11

A composite material, wherein:
(a) said composite material is composed of one or more ion exchange resins with ion exchange function and fluorine-containing polymer fiber functioning as reinforcing material;
(b) the surface of said fluorine-containing polymer fiber is graft-modified by nitrile group-containing functional monomer;
(c) at least one of ion exchange resins composing said composite material comprises nitrile group which forms triazine ring cross-linked structure with the nitrile group of the functional monomer grafted in fluorine-containing polymer fiber.

### Claim 12 (depends on 11)

The composite material according to claim 11, wherein said nitrile group-containing functional monomer is one or more combinations of substances shown in the following general formula (I):
said nitrile group-containing ion exchange resin is one or more combinations of resins shown in the following general formulas (II) and/or (III):
wherein e≈1-3; n=0 or 1; m=2-5; x, y=an integer of 3-15;
wherein a, b, c=an integer of 3-15; a′, b′, c′=an integer of 1-3; j=0-3.

### Claim 13 (depends on 12)

The composite material according to claim 12, wherein said composite material may further comprise one or more combinations of resins shown in the following general formulas (IV) and/or (V) and/or (VI):
wherein x=3-15, n=0-2; p=2-5;
wherein c, d=an integer of 3-15; c′, d′=an integer of 1-3;
wherein f, g, h=an integer of 3-15; f′, g′, h′=an integer of 1-3; i=0-3; M, M′=H, K, Na or NH4.

### Claim 14 (depends on 13)

The composite material according to claim 13, wherein the ion exchange capacity of said resin as shown in general formulas (II), (III), (IV), (V) or (VI) is 0.80-1.60 mmol/g; the number average molecular weight is 150,000-450,000.

### Claim 15 (depends on 14)

The composite material according to claim 14, wherein said fluorine-containing polymer fiber is one or more selected from polytetrafluroethylene fiber, polyperfluorinated ethylene propylene fiber, perfluoropropyl vinylether fiber and/or fluorocarbon polymer fiber; the diameter of the fluorine-containing polymer fiber is 0.005 μm-50 μm and the length of the fluorine-containing polymer fiber is 0.05 μm-3 mm; the mass ratio of the fluorine-containing polymer fiber to the ion exchange resin is 0.5-50:100.

### Claim 16 (depends on 15)

The composite material according to claim 15, wherein the diameter of the fluorine-containing polymer fiber is 0.01-20 μm.

### Claim 17 (depends on 15)

The composite material according to claim 15, wherein the mass ration of the fluorine-containing polymer fiber is 0.5-20:100.

### Claim 18 (depends on 15)

The composite material according to claim 15, wherein said composite material comprises a high valence metal compound, through which part of acidic exchange groups in the ion exchange resin form physical bonds in between and part of high valence metal compounds which are also catalysts of forming triazine ring cross-linked structure form complexing bond with the trizaine ring.

### Claim 19 (depends on 18)

The composite material according to claim 18, wherein said high valence metal compound forming physical bonds is one or more combinations selected from compounds of the following elements: W, Zr, Ir, Y, Mn, Ru, Ce, V, Zn, Ti and La.

### Claim 20 (depends on 19)

The composite material according to claim 19, wherein said high valence metal ion compound is one selected from nitrate, sulfate, carbonate, phosphate, acetate of such metal elements in the highest and intermediate valence state or double salts thereof; or one or more selected from cyclodextrin, crown ether, acetylacetone, nitrogen-containing crown ether or nitrogen-containing heterocycle, EDTA, DMF or DMSO complex of such metal elements in the highest and intermediate valence state; or selected from hydroxide of such metal elements in the highest and intermediate valence state; or selected from oxide, with perovskite structure, of such metal elements in the highest and intermediate valence state, including compounds of CexTi(1-x)O2 (x=0.25-0.4), Ca0.6La0.27TiO3, La(1-y)CeyMnO3 (y=0.1-0.4) and La0.7Ce0.15Ca0.15MO3.

### Claim 21 (depends on 18)

The composite material according to claim 18, wherein the added amount of said high valence metal compound is 0.0001-5 wt % of resin.

### Claim 22 (depends on 21)

The composite material according to claim 21, wherein the added amount of said high valence metal compound is 0.001-1 wt % of resin.

### Claim 23 (depends on 18)

A method for preparing said composite material according to any one of claim 18, wherein the method comprises the following steps: adding trace strong protonic acid and/or Lewis acid into the composite material as catalyst to allow the nitrile group of at least one nitrile group-containing ion exchange resin to form triazine ring cross-linked structure with the nitrile group in a functional monomer grafted in fluorine-containing polymer fiber.

### Claim 24 (depends on 23)

The method for preparing said composite material according to claim 23, wherein said protonic acid is selected from H2SO4, CF3SO3H, or H3PO4; said Lewis acid is selected from ZnCl2, FeCl3, AlCl3, organotin, organic antimony, or organic tellurium.

### Claim 25 (depends on 23)

The method for preparing said composite material according to claim 23, wherein the added amount of said Lewis acid and/or protonic acid is usually 0.1%-1% of resin weight.

### Claim 26 (depends on 23)

The method for preparing said composite material according to claim 23, wherein the method comprises the following steps:
(1) mixing a solution of the high valence metal compound and an acid crosslinking catalyst with a dispersed solution of the ion exchange resin as well as nitrile group-grafted fiber, followed by forming wet membrane on a plate after pouring, tape casting, screen-printing process, spraying or impregnating process;
(2) subjecting the wet membrane to heat treatment at 30-300° C. to obtain a composite material with triazine ring cross-linked structure;
the solvent used in the processes of solution pouring, tape casting, screen-printing, spraying impregnating and the like is one or more selected from dimethylformamide, dimethylacetamide, methylformamide, dimethyl sulfoxide, N-methyl pyrrolidone, hexamethyl phosphoric acid amide, acetone, water, ethanol, methanol, propanol, isopropanol, glycol and/or glycerol;
preparation conditions include: the concentration of resin dispersed solution is 1-80%, the temperature for heat treatment is 30-300° C., the time for heat treatment is 1-600 minutes;
wherein the amount of the high valence metal compound to be added is 0.0001-5 wt % of weight of resin.

### Claim 27 (depends on 26)

The method for preparing said composite material according to claim 26, wherein the preparation conditions include: the concentration of resin dispersed solution is 5-40%, the temperature for heat treatment is 120-250° C., the time for heat treatment is 5-200 minutes.

### Claim 28 (depends on 26)

The method of preparing said composite material according to claim 26, wherein the amount of the high valence metal compound to be added is 0.001-1 wt % of resin; the acid crosslinking catalyst is Lewis acid and/or protonic acid and the amount to be added is 0.1-1 wt % of resin weight.

### Claim 29 (depends on 11)

An ion exchange membrane made from said composite material according to claim 11.

### Claim 30 (depends on 11)

A use of said composite material according to claim 11 in manufacturing the ion exchange membrane in fuel cells.