Preparation process of transition metal boride and uses thereof
AssigneeShenzhen Sunxing Light Alloys Materials Co., Ltd.
InventorsXuemin CHEN, Jun YANG, Zhihong LI, Weiping WU
Life of this patent
Estimating the term…
Loading patent…
AssigneeShenzhen Sunxing Light Alloys Materials Co., Ltd.
InventorsXuemin CHEN, Jun YANG, Zhihong LI, Weiping WU
Estimating the term…
The invention provides a preparation process of transition metal boride, comprising the following steps: A) aluminum is put in a reactor, inert gas is fed into the reactor after evacuation, the reactor is heated up to 700 to 800° C. and then added with dry potassium fluoborate or sodium fluoborate, monomer boron and cryolite are generated by rapid stirring and reaction for 4 to 6 hours, and the molten liquid at the upper layer is sucked out and the monomer boron is obtained by means of separation; and B) the obtained monomer boron is added with transition metal for reaction at the temperature from 1800 to 2200° C. in order to generate corresponding transition metal boride.
A preparation process of transition metal boride, characterized in that:
Dependencies are inferred from the claim text.