# US 2013/0094083 A1 · Pressure-sensitive adhesive layer for optical film, pressure-sensitive adhesive optical film, and image display

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0094083 A1
- Document ID: US20130094083A1
- Status: Published application
- Kind: A1
- Application number: 13/703,714
- Filed: 2011-06-17
- Published: 2013-04-18
- Earliest claimed: 2010-06-28
- Assignees: Nitto Denko Corporation
- Inventors: Takaaki Ishii; Kunihiro Inui; Toshitsugu Hosokawa; Masayuki Satake
- Web page: https://patentgrep.com/patent/US20130094083A1

## CPC

- C09J 133/12: Homopolymers or copolymers of methyl methacrylate
- C09J 133/04: Homopolymers or copolymers of esters {(C09J143/04 takes precedence)}
- G02B 5/30: Polarising elements (light-modulating devices with active elements G02F1/00)
- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- G02F 1/133528: {Polarisers}
- G02F 2202/28: Adhesive materials or arrangements
- Y10T 428/2835: including moisture or waterproof component
- Y10T 428/2848: Three or more layers
- Y10T 428/2891: including addition polymer from alpha-beta unsaturated carboxylic acid [e.g., acrylic acid, methacrylic acid, etc.] Or derivative thereof
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The pressure-sensitive adhesive layer for an optical film having good heat and moisture durability is formed by a process of applying an aqueous dispersion-type pressure-sensitive adhesive containing an emulsion of a (meth)acryl-based polymer obtained by subjecting a monomer mixture containing at least one of an alkyl (meth)acrylate (a1) with an alkyl group of 1 to 3 carbon atoms and an alkoxysilyl group-containing monomer (a2), and an alkyl (meth)acrylate (b) with an alkyl group of 4 to 14 carbon atoms to emulsion polymerization in water in the presence of a radical polymerization initiator and a reactive surfactant having a radically-polymerizable functional group; and then drying the emulsion, wherein a content of the reactive surfactant is 0.3 to 3 parts by weight based on 100 parts by weight of the monomer mixture, and has a saturated water absorption of 1.2 to 3.2% by weight at 50° C. and 90% R.H.

## Claims

### Claim 1

A pressure-sensitive adhesive layer for an optical film, which is formed by a process comprising:
applying an aqueous dispersion-type pressure-sensitive adhesive containing an emulsion of a (meth)acryl-based polymer obtained by subjecting a monomer mixture containing
at least one of an alkyl (meth)acrylate (a1) with an alkyl group of 1 to 3 carbon atoms and an alkoxysilyl group-containing monomer (a2), and
an alkyl (meth)acrylate (b) with an alkyl group of 4 to 14 carbon atoms to emulsion polymerization in water in the presence of a radical polymerization initiator and a reactive surfactant having a radically-polymerizable functional group; and then drying the emulsion,
wherein a content of the reactive surfactant is 0.3 to 3 parts by weight based on 100 parts by weight of the monomer mixture, and
the pressure-sensitive adhesive layer has a saturated water absorption of 1.2 to 3.2% by weight at 50° C. and 90% R.H.

### Claim 2 (depends on 1)

The pressure-sensitive adhesive layer for an optical film according to claim 1, wherein the content of the reactive surfactant is 0.3 to less than 2 parts by weight based on 100 parts by weight of the monomer mixture.

### Claim 3 (depends on 1)

The pressure-sensitive adhesive layer for an optical film according to claim 1, wherein the monomer mixture contains 0.1 to 40% by weight of the alkyl (meth)acrylate (a1) with an alkyl group of 1 to 3 carbon atoms and 50 to 99.9% by weight of the alkyl (meth)acrylate (b) with an alkyl group of 4 to 14 carbon atoms based on the total amount of the monomer mixture.

### Claim 4 (depends on 1)

The pressure-sensitive adhesive layer for an optical film according to claim 1, wherein the monomer mixture contains 0.001 to 1% by weight of the alkoxysilyl group-containing monomer (a2) and 89 to 99.999% by weight of the alkyl (meth)acrylate (b) with an alkyl group of 4 to 14 carbon atoms based on the total amount of the monomer mixture.

### Claim 5 (depends on 1)

The pressure-sensitive adhesive layer for an optical film according to claim 1, wherein the monomer mixture contains 0.1 to 40% by weight of the alkyl (meth)acrylate (a1) with an alkyl group of 1 to 3 carbon atoms, 0.001 to 1% by weight of the alkoxysilyl group-containing monomer (a2), and 89 to 99.999% by weight of the alkyl (meth)acrylate (b) with an alkyl group of 4 to 14 carbon atoms based on the total amount of the monomer mixture.

### Claim 6 (depends on 1)

The pressure-sensitive adhesive layer for an optical film according to claim 1, wherein the monomer mixture contains 0.1 to 10% by weight of a carboxyl group-containing monomer (c) based on the total amount of the monomer mixture.

### Claim 7 (depends on 1)

The pressure-sensitive adhesive layer for an optical film according to claim 1, which has an elongation percentage (L60) of 200% or less in an environment at 60° C. and 7% R.H. and a ratio {(L60−90)/(L60)} of at least 1.5, wherein {(L60−90)/(L60)} is the ratio of an elongation percentage (L60−90) in an environment at 60° C. and 90% R.H. to the elongation percentage (L60) in an environment at 60° C. and 7% R.H., and the elongation percentage is determined from the following equation: elongation percentage (%)={(L1−L0)/L0}×100 by a process comprising forming the pressure-sensitive adhesive layer into a cylindrical test piece with a cross section of 4.6 mm2 and a length of 30 mm, allowing the test piece to stand in an environment at 60° C. and 7% R.H. or at 60° C. and 90% R.H. for 1 hour, then measuring the length L0 (mm) of the test piece, then suspending the test piece in an environment at 60° C. and 7% R.H. or at 60° C. and 90% R.H. for 2 hours, while fixing one end of the test piece and attaching a 12 g weight to the other end of the test piece, and then measuring the length L1 (mm) of the test piece.

### Claim 8 (depends on 1)

A pressure-sensitive adhesive optical film, comprising an optical film and the pressure-sensitive adhesive layer for an optical film according to claim 1 placed on at least one side of the optical film.

### Claim 9 (depends on 8)

The pressure-sensitive adhesive optical film according to claim 8, wherein the optical film, on which the pressure-sensitive adhesive layer is placed, has a moisture permeability of 1,000 g/m2 per 24 hours at 80° C. and 90% R.H. or less.

### Claim 10 (depends on 8)

The pressure-sensitive adhesive optical film according to claim 8, wherein the optical film is a polarizing plate comprising a polarizer and a transparent protective film provided on at least one side of the polarizer.

### Claim 11 (depends on 8)

An image display comprising at least one piece of the pressure-sensitive adhesive optical film according to claim 8.