# US 2013/0092953 A1 · Epitaxial substrate and method for manufacturing epitaxial substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0092953 A1
- Document ID: US20130092953A1
- Status: Published application
- Kind: A1
- Application number: 13/705,554
- Filed: 2012-12-05
- Published: 2013-04-18
- Earliest claimed: 2010-06-08
- Assignees: NGK Insulators, Ltd.
- Inventors: Makoto MIYOSHI; Shigeaki SUMIYA; Mikiya ICHIMURA; Sota MAEHARA; Mitsuhiro TANAKA
- Web page: https://patentgrep.com/patent/US20130092953A1

## CPC

- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D 30/4755: {having wide bandgap charge-carrier supplying layers, e.g. modulation doped HEMTs such as n-AlGaAs/GaAs HEMTs}
- H10D 62/221: {of FETs}
- H10D 62/8164: {comprising only semiconductor materials (potential variation in long-range structurally-disordered materials H10D62/8163)}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3216: {Nitrides}
- H10P 14/3252: {Alternating layers, e.g. superlattice}
- H10P 14/3416: {Nitrides}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a crack-free epitaxial substrate having a small amount of warping, in which a silicon substrate is used as a base substrate. The epitaxial substrate includes: a (111) single crystal Si substrate and a buffer layer formed of a plurality of lamination units being continuously laminated. The lamination unit includes: a composition modulation layer formed of a first and a second unit layer having different compositions being alternately and repeatedly laminated such that a compressive strain exists therein; a termination layer formed on an uppermost portion of the composition modulation layer, the termination layer acting to maintain the compressive strain existing in the composition modulation layer; and a strain reinforcing layer formed on the termination layer, the strain reinforcing layer acting to enhance the compressive strain existing in the composition modulation layer.

## Claims

### Claim 1

An epitaxial substrate in which a group of group-III nitride layers are formed on a base substrate made of (111)-oriented single crystal silicon such that a (0001) crystal plane of said group of group-III nitride layers is substantially in parallel with a substrate surface of said base substrate, said epitaxial substrate comprising:
a buffer layer formed of a plurality of lamination units being continuously laminated; and
a crystal layer formed on said buffer layer,
said lamination unit including:
a composition modulation layer formed of a first unit layer and a second unit layer having different compositions being alternately and repeatedly laminated such that a compressive strain exists therein;
a termination layer formed on an uppermost portion of said composition modulation layer, said termination layer acting to maintain said compressive strain existing in said composition modulation layer; and
a strain reinforcing layer formed on said termination layer, said strain reinforcing layer acting to enhance said compressive strain existing in said composition modulation layer.

### Claim 2 (depends on 1)

The epitaxial substrate according to claim 1, wherein
a second group-III nitride of said second unit layer has an in-plane lattice constant, under a strain-free state, greater than that of a first group-III nitride of said first unit layer,
each of said second unit layers is formed so as to be in a coherent state relative to said first unit layer.

### Claim 3 (depends on 2)

The epitaxial substrate according to claim 2, wherein
said termination layer is made of said first group-III nitride and formed with a thickness greater than that of said first unit layer.

### Claim 4 (depends on 3)

The epitaxial substrate according to claim 3, wherein
said strain reinforcing layer includes an intermediate layer that is made of a third group-III nitride and formed so as to be coherent to said termination layer.

### Claim 5

An epitaxial substrate in which a group of group-III nitride layers are formed on a base substrate made of (111)-oriented single crystal silicon such that a (0001) crystal plane of said group of group-III nitride layers is substantially in parallel with a substrate surface of said base substrate, said epitaxial substrate comprising:
a buffer layer formed of a plurality of lamination units being continuously laminated; and
a crystal layer made of a group-III nitride and formed on said buffer layer,
said lamination unit including:
a composition modulation layer formed of a first unit layer and a second unit layer made of group-III nitrides having different compositions being alternately and repeatedly laminated, in which a second group-III nitride of said second unit layer has an in-plane lattice constant, under a strain-free state, greater than that of a first group-III nitride of said first unit layer;
a termination layer formed on an uppermost portion of said composition modulation layer, said termination layer being made of said first group-III nitride and formed with a thickness greater than that of said first unit layer; and
an intermediate layer made of a third group-III nitride, wherein
in said composition modulation layer, said second unit layer is formed so as to be in a coherent state relative to said first unit layer,
said intermediate layer is formed so as to be in a coherent state relative to said termination layer,

### Claim 6 (depends on 1)

The epitaxial substrate according to claim 1, wherein
said first unit layer is made of AlN, and said second unit layer is made of a group-III nitride having a composition of AlxGa1-xN (0≦x≦0.25).

### Claim 7 (depends on 6)

The epitaxial substrate according to claim 6, wherein
said intermediate layer is made of a group-III nitride having a composition of AlyGa1-xN (0≦y≦0.25), and formed with a thickness of 100 nm or more and 500 nm or less.

### Claim 8 (depends on 6)

The epitaxial substrate according to claim 6, wherein
said second unit layer is made of a group-III nitride having a composition of AlxGa1-xN (0.1≦x≦0.25), and said intermediate layer is made of a group-III nitride having a composition of AlyGa1-yN (0.1≦y≦0.25).

### Claim 9 (depends on 8)

The epitaxial substrate according to claim 8, wherein
the composition of said second unit layer is substantially the same as the composition of said intermediate layer.

### Claim 10 (depends on 1)

The epitaxial substrate according to claim 1, further comprising:
a first base layer made of AlN and formed on said base substrate; and
a second base layer made of AlpGa1-pN (0≦p<1) and formed on said first base layer, wherein
said first base layer is a layer with many crystal defects configured of at least one kind from a columnar or granular crystal or domain,
an interface between said first base layer and said second base layer defines a three-dimensional concavo-convex surface,
said buffer layer is formed immediately on said second base layer.

### Claim 11

A method for manufacturing an epitaxial substrate for use in a semiconductor device, said epitaxial substrate having a group of group-III nitride layers formed on a base substrate made of (111)-oriented single crystal silicon such that a (0001) crystal plane of said group of group-III nitride layers is substantially in parallel with a substrate surface of said base substrate, said method comprising:
a buffer layer formation step for forming a buffer layer; and
a crystal layer formation step for forming a crystal layer above said buffer layer, said crystal layer being made of a group-III nitride, wherein
in said buffer layer formation step, a lamination unit formation step is continuously repeated a plurality of times, said lamination unit formation step including:
a composition modulation layer formation step for forming a composition modulation layer by alternately and repeatedly laminating a first unit layer and a second unit layer made of group-Ill nitrides having different compositions;
a termination layer formation step for forming a termination layer on an uppermost portion of said composition modulation layer; and
an intermediate layer formation step for forming an intermediate layer on said termination layer,
in said composition modulation layer formation step, said composition modulation layer is formed such that:
a second group-III nitride of said second unit layer has an in-plane lattice constant, under a strain-free state, greater than that of a first group-III nitride of said first unit layer; and
each of said second unit layers is in a coherent state relative to said first unit layer,
in said termination layer formation step, said termination layer is made of said first group-III nitride and formed with a thickness greater than that of said first unit layer,
in said intermediate layer formation step, said intermediate layer is made of a third group-III nitride and formed so as to be in a coherent state relative to said termination layer.

### Claim 12 (depends on 11)

The method for manufacturing the epitaxial substrate according to claim 11 wherein
said first unit layer is made of lN, and said second unit layer is made of a group-III nitride having a composition of AlxGa1-xN (0≦x≦0.25).

### Claim 13 (depends on 12)

The method for manufacturing the epitaxial substrate according to claim 12, wherein
said intermediate layer is made of a group-III nitride having a composition of AlyGa1-yN (0≦y≦0.25), and formed with a thickness of 100 nm or more and 500 nm or less.

### Claim 14 (depends on 12)

The method for manufacturing the epitaxial substrate according to claim 12, wherein
said second unit layer is made of a group-III nitride having a composition of AlxGa1-xN (0.1<x<0.25), and said intermediate layer is made of a group-III nitride having a composition of AlyGa1-yN (0.1≦y≦0.25).

### Claim 15 (depends on 14)

The method for manufacturing the epitaxial substrate according to claim 14, wherein
the composition of said second unit layer is substantially the same as the composition of said intermediate layer.

### Claim 16 (depends on 11)

The method for manufacturing the epitaxial substrate according to claim 11, further comprising:
a first base layer formation step for forming a first base layer on said base substrate, said first base layer being made of AlN; and
a second base layer formation step for forming a second base layer on said first base layer, said second base layer being made of AlpGa1-pN (0≦p<1), wherein
in said first base layer formation step, said first base layer is formed as a layer with many crystal defects configured of at least one kind from a columnar or granular crystal or domain, such that a surface thereof is a three-dimensional concavo-convex surface,
in said buffer layer formation step, said buffer layer is formed immediately on said second base layer.

### Claim 17 (depends on 5)

The epitaxial substrate according to claim 5, wherein
said first unit layer is made of AlN, and said second unit layer is made of a group-III nitride having a composition of AlxGa1-xN (0≦x≦0.25).

### Claim 18 (depends on 17)

The epitaxial substrate according to claim 17, wherein
said intermediate layer is made of a group-III nitride having a composition of AlyGa1-yN (0≦y≦0.25), and formed with a thickness of 100 nm or more and 500 nm or less.

### Claim 19 (depends on 17)

The epitaxial substrate according to claim 17, wherein
said second unit layer is made of a group-III nitride having a composition of AlxGa1-xN (0.1≦x≦0.25), and said intermediate layer is made of a group-III nitride having a composition of AlyGa1-yN (0.1≦y≦0.25).

### Claim 20 (depends on 19)

The epitaxial substrate according to claim 19, wherein
the composition of said second unit layer is substantially the same as the composition of said intermediate layer.