# US 2013/0092867 A1 · Method for producing sintered rare-earth magnet, sintered rare-earth magnet, and material for same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0092867 A1
- Document ID: US20130092867A1
- Status: Published application
- Kind: A1
- Application number: 13/511,465
- Filed: 2010-11-18
- Published: 2013-04-18
- Earliest claimed: 2009-11-26
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Inventors: Tetsuya Shoji; Noritsugu Sakuma; Hidefumi Kishimoto
- Web page: https://patentgrep.com/patent/US20130092867A1

## CPC

- H01F 1/11: in the form of particles {(for magnetic record carriers G11B5/70626)}
- H01F 1/0572: {with a protective layer}
- H01F 1/0577: {sintered}
- H01F 1/061: {with a protective layer}
- H01F 1/086: {sintered}
- H01F 41/0266: {Moulding; Pressing (H01F41/0273 takes precedence; hard magnetic particles H01F1/06, H01F1/11)}
- B82Y 40/00: Manufacture or treatment of nanostructures
- H01F 1/058: and IVa elements, e.g. Gd2Fe14C
- Y10S 977/838: Magnetic property of nanomaterial
- Y10S 977/90: having step or means utilizing mechanical or thermal property, e.g. pressure, heat
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for producing a sintered rare-earth magnet characterized by sintering a raw material that includes a ribbon-shaped polycrystalline phase with an average grain size of 10 to 200 nm fabricated by rapid solidification of an alloy melt having a rare-earth magnet composition, and a low-melting point phase formed on the surface of the polycrystalline phase and having a melting point lower than the polycrystalline phase.

## Claims

### Claim 1

A method for producing a sintered rare-earth magnet by comprising:
preparing a ribbon composed of a polycrystalline phase including crystal grains with an average grain size of 10 to 200 nm by rapidly solidificating of an alloy melt having a rare-earth magnet composition;
forming a low-melting point phase having a melting point lower than the polycrystalline phase on the surface of the ribbon; and
sintering a raw material composed of the ribbon and the low-melting point phase.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the rapidly solidificating the alloy melt is performed by a single-roll process in which a single roll is used, and the surface of the ribbon on which the low-melting point phase is formed is opposite to a surface in contact with the single roll.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the low-melting point phase is formed on one or both surfaces of the ribbon by an electrodeposition.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the electrodeposition is performed using an organic solvent or ionic liquid as an electrolyte liquid.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the average grain size of the crystal grains contained in the polycrystalline phase is 10 to 50 nm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the sintering of the raw material includes pulverizing the raw material to obtain a powder, and sintering the powder.

### Claim 7 (depends on 1)

A sintered rare-earth magnet being produced using the method according to claim 1.

### Claim 8

A raw material for a sintered rare-earth magnet comprising:
a ribbon composed of a polycrystalline phase including crystal grains with an average grain size of 10 to 200 nm; and
a low-melting point phase formed on the surface of the ribbon and having a melting point lower than the polycrystalline phase.

### Claim 9 (depends on 8)

The raw material according to claim 8, wherein the average grain size of the crystal grains contained in the polycrystalline phase is 10 to 50 nm.