# US 2013/0092453 A1 · Use of tungsten carbide tube rod to hard-face pdc matrix

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0092453 A1
- Document ID: US20130092453A1
- Status: Published application
- Kind: A1
- Application number: 13/649,830
- Filed: 2012-10-11
- Published: 2013-04-18
- Earliest claimed: 2011-10-14
- Assignees: Varel International Ind., L.P.
- Inventors: Charles Daniel Johnson
- Web page: https://patentgrep.com/patent/US20130092453A1

## CPC

- E21B 10/54: the bit being of the rotary drag type, e.g. fork-type bits
- B22F 7/06: of composite workpieces or articles from parts, e.g. to form tipped tools {(B22F7/002 takes precedence)}
- C22C 29/06: based on carbides, but not containing other metal compounds
- C22C 29/08: based on tungsten carbide
- C22C 29/12: based on oxides
- C22C 29/16: based on nitrides {(containing cubic BN or wurtzitic BN and diamond C22C26/00)}
- E21B 17/1085: {Wear protectors; Blast joints; Hard facing}
- C22C 2204/00: End product comprising different layers, coatings or parts of cermet
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A hardfaced infiltrated matrix downhole tool and a method for hardfacing such items. The hardfaced infiltrated matrix downhole tool includes a body, an intermediate base coat coupled to at least a portion of the surface of the body, and a hardfacing material coupled to at least a portion of the intermediate base coat. The body is composed of at least a carbide material and an infiltrating binder material. The intermediate base coat bonds to the surface of the body and to the hardfacing material. The method includes obtaining an infiltrated matrix downhole tool, applying and bonding the intermediate base coat to at least a portion of the surface of the infiltrated matrix downhole tool, and applying and bonding the hardfacing material to at least a portion of the intermediate base coat.

## Claims

### Claim 1

A hardfaced infiltrated matrix downhole tool, comprising:
a body comprising a carbide material and an infiltrating binder material;
an intermediate base coat coupled to at least a portion of the surface of the body; and
a hardfacing material coupled to at least a portion of the intermediate base coat, wherein the intermediate base coat bonds to the body and the hardfacing material.

### Claim 2 (depends on 1)

The hardfaced infiltrated matrix downhole tool of claim 1, wherein the body forms at least a portion of one of an infiltrated matrix drill bit, an infiltrated matrix bi-center bit, an infiltrated matrix core head, an infiltrated matrix reamer, and an infiltrated matrix stabilizer.

### Claim 3 (depends on 1)

The hardfaced infiltrated matrix downhole tool of claim 1, wherein the carbide material is formed using one or more metals selected from a group consisting of titanium, zirconium, halfnium, rutherfordium, vanadium, niobium, tantalum, dubnium, chromium, molybdenum, tungsten, and seaborgium.

### Claim 4 (depends on 1)

The hardfaced infiltrated matrix downhole tool of claim 1, wherein the infiltrating binder material includes at least one of copper, nickel, iron, cobalt, and alloys thereof

### Claim 5 (depends on 1)

The hardfaced infiltrated matrix downhole tool of claim 1, wherein the intermediate base coat bonds to the infiltrating binder material.

### Claim 6 (depends on 1)

The hardfaced infiltrated matrix downhole tool of claim 1, wherein the body further comprises:
one or more blades extending from about one end of the body towards a second end of the body, each blade comprising a leading edge, a trailing edge, and a face extending from the leading edge to the trailing edge; and
at least one cutter mounted on the face of the blade,
wherein the intermediate base coat is coupled to at least portions of the face.

### Claim 7 (depends on 1)

The hardfaced infiltrated matrix downhole tool of claim 1, wherein the body further comprises:
one or more blades extending from about one end of the body towards a second end of the body, each blade comprising a leading edge, a trailing edge, and a face extending from the leading edge to the trailing edge; and
at least one cutter mounted on the face of the blade,
wherein the intermediate base coat is coupled to at least portions of the leading edge.

### Claim 8

A method for hardfacing an infiltrated matrix downhole tool, comprising:
obtaining an infiltrated matrix downhole tool fabricated using at least a carbide material and an infiltrating binder material;
applying an intermediate base coat onto at least a portion of a surface of the infiltrated matrix downhole tool;
bonding the intermediate base coat onto at least a portion of the surface of the infiltrated matrix downhole tool;
applying a hardfacing material onto at least a portion of the intermediate base coat; and
bonding the hardfacing material onto at least a portion of the intermediate base coat.

### Claim 9 (depends on 8)

The method of claim 8, wherein applying an intermediate base coat comprises:
heating at least a portion of the infiltrated matrix downhole tool to a first temperature and forming a heated infiltrated matrix downhole tool;
applying the intermediate base coat onto at least a portion of the heated infiltrated matrix downhole tool; and
allowing the heated infiltrated matrix downhole tool to cool to a second temperature.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first temperature ranges between about 900 degrees Fahrenheit to about 1250 degrees Fahrenheit.

### Claim 11 (depends on 9)

The method of claim 9, wherein the second temperature ranges between about 400 degrees Fahrenheit to about 600 degrees Fahrenheit.

### Claim 12 (depends on 8)

The method of claim 8, wherein the hardfacing material comprises a first phase and a second phase, the second phase being a metal matrix material.

### Claim 13 (depends on 12)

The method of claim 12, wherein applying the hardfacing material comprises:
heating the hardfacing material to an operating temperature, the operating temperature being equal to or greater than the melting temperature of the second phase;
applying the hardfacing material onto at least a portion of the intermediate base coat previously bonded to the infiltrated matrix downhole tool; and
allowing the hardfacing material on the intermediate base coat to cool.

### Claim 14 (depends on 8)

The method of claim 8, wherein the hardfacing material is applied onto the infiltrated matrix downhole tool using a tube rod, the tube rod comprising a first phase and a second phase, the second phase substantially surrounding the first phase and disposed at one end of the tube rod.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first phase comprises at least one of tungsten carbide, titanium carbide, tantalum carbide, titanium diboride, chromium carbide, titanium nitride, aluminum nitride, aluminum oxide, and silicon carbide.

### Claim 16 (depends on 14)

The method of claim 14, wherein the second phase comprises at least one of cobalt, iron, nickel, aluminum, copper, magnesium, titanium, and one or more alloys thereof.

### Claim 17 (depends on 8)

The method of claim 8, wherein the carbide material is formed using one or more metals selected from a group consisting of titanium, zirconium, halfnium, rutherfordium, vanadium, niobium, tantalum, dubnium, chromium, molybdenum, tungsten, and seaborgium.

### Claim 18 (depends on 8)

The method of claim 8, wherein the infiltrating binder material includes at least one of copper, nickel, iron, cobalt, and alloys thereof.

### Claim 19

A hardfaced infiltrated matrix drill bit, comprising:
a bit body fabricated from at least a carbide material and an infiltrating binder material facilitating the bonding of the carbide material;
a shank coupled to the bit body
an intermediate base coat bonded to at least a portion of the surface of the body; and
a hardfacing material bonded to at least a portion of the intermediate base coat,
wherein the intermediate base coat bonds to the body and the hardfacing material.

### Claim 20 (depends on 19)

The hardfaced infiltrated matrix drill bit of claim 19, wherein the bit body further comprises:
one or more blades extending from about one end of the bit body towards the shank, each blade comprising a leading edge, a trailing edge, and a face extending from the leading edge to the trailing edge; and
at least one cutter mounted on the face of the blade,
wherein the intermediate base coat is coupled to at least portions of the face.