# US 2013/0092297 A1 · Cu-Co-Si System Alloy Sheet and Method for Manufacturing Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0092297 A1
- Document ID: US20130092297A1
- Status: Published application
- Kind: A1
- Application number: 13/581,715
- Filed: 2011-03-24
- Published: 2013-04-18
- Earliest claimed: 2010-06-03
- Assignees: JX Nippon Mining & Metals Corporation
- Inventors: Hiroshi Kuwagaki
- Web page: https://patentgrep.com/patent/US20130092297A1

## CPC

- C22C 9/06: with nickel or cobalt as the next major constituent
- C22F 1/08: of copper or alloys based thereon
- H01B 1/026: {Alloys based on copper}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

The present invention provides a Cu—Co—Si system alloy sheet, being suitable for use in a variety of electronic device components, in particular, having excellent uniform adhesive property for plate. The copper alloy sheet for electronic materials, contains 0.5 to 3.0 mass % Co, 0.1 to 1.0 mass % Si, the balance being Cu and unavoidable impurities, wherein an average grain size in the center part of the sheet thickness is 20 μm or less, and the number of the crystal grain, being tangent to a surface of the sheet and having 45 μm or more of the length of major axis, is 5 or less in the area of 1 mm in a rolling direction.

## Claims

### Claim 1

A copper alloy sheet for electronic materials, containing 0.5 to 3.0 mass % Co, 0.1 to 1.0 mass % Si, the balance being Cu and unavoidable impurities, wherein
an average grain size in the center part of the sheet thickness is 20 μm or less, and
the number of the crystal grain, being tangent to a surface of the sheet and having 45 μm or more of the length of major axis, is 5 or less in the area of 1 mm in a rolling direction.

### Claim 2 (depends on 1)

The copper alloy sheet for electronic materials of claim 1, wherein Cr is furthermore contained in a maximum amount of 0.5 mass %.

### Claim 3 (depends on 1)

The copper alloy for electronic materials of claim 1, wherein a single element or two or more elements selected from Mg, P, As, Sb, Be, B, Mn, Sn, Ti, Zr, Al, Fe, Zn and Ag are furthermore contained in total in a maximum amount of 2.0 mass %.

### Claim 4 (depends on 1)

A method for manufacturing the copper alloy sheet according to claim 1, comprising sequentially conducting:
a step for casting an ingot;
a step for heating the ingot for 1 hour or more at material temperature being 950° C. to 1050° C., thereafter hot rolling the ingot, setting the temperature to 700° C. or more when hot rolling is completed;
a step for conducting an intermediate rolling before a solution treatment, by conducting the last pass at a reduction ratio being 8% or more;
a step for conducting a intermediate solution treatment, by heating at material temperature being 850° C. to 1050° C., for 0.5 minute to 1 hour;
a step for conducting aging, by heating at 400° C. to 600° C.; and
a step for conducting last rolling at a reduction ratio being 10 to 50%.

### Claim 5 (depends on 2)

The copper alloy for electronic materials of claim 2, wherein a single element or two or more elements selected from Mg, P, As, Sb, Be, B, Mn, Sn, Ti, Zr, Al, Fe, Zn and Ag are furthermore contained in total in a maximum amount of 2.0 mass %.

### Claim 6 (depends on 2)

A method for manufacturing the copper alloy sheet according to claim 2, comprising sequentially conducting:
a step for casting an ingot;
a step for heating the ingot for 1 hour or more at material temperature being 950° C. to 1050° C., thereafter hot rolling the ingot, setting the temperature to 700° C. or more when hot rolling is completed;
a step for conducting an intermediate rolling before a solution treatment, by conducting the last pass at a reduction ratio being 8% or more;
a step for conducting a intermediate solution treatment, by heating at material temperature being 850° C. to 1050° C., for 0.5 minute to 1 hour;
a step for conducting aging, by heating at 400° C. to 600° C.; and
a step for conducting last rolling at a reduction ratio being 10 to 50%.